    • 5. 发明专利
    • Invar alloy for shadow mask and production method therefor
    • 用于阴影掩蔽的合金及其生产方法
    • JP2003027188A
    • 2003-01-29
    • JP2001218983
    • 2001-07-19
    • Sumitomo Metal Ind LtdToyo Kohan Co Ltd住友金属工業株式会社東洋鋼鈑株式会社
    • TSUGE SHINJIKITA ISATONISHI TAKAYUKIOKAYAMA HIRONAOFUKUMOTO MASAHIRO
    • C21C7/00C21C7/04C21C7/064C21C7/076C22C38/00C22C38/54H01J29/07
    • Y02P10/242
    • PROBLEM TO BE SOLVED: To provide an inexpensive, high strength invar alloy which has low thermal expansion and excellent hot workability, and is used for a shadow mask of a cathode ray tube, and to provide a production method therefor. SOLUTION: The alloy has a composition which contains one or more kinds of strengthening elements selected from C and Nb, Ni, Co, Al and Ca, and, if required, which further contains B, and in which the contents of Si, Mn, P, S, Mg, Cu, Cr, V, Mo, Ti, N and O are controlled to specified values or lower, in which the content of Mg inclusion is controlled to a specified value or lower, and also, Ca/O is 0.1 to 2.0, or the proportion of Mg, Al and Ca in oxide inclusions is controlled to a specified ratio to allow Ca sulfide to precipitate incidentially to oxide inclusions, and which contains the balance being substantially Fe. In the production of the alloy, the ratio of CaO to Al2 O3 in slag to be used in secondary refining is controlled to 1.4 to 2.2, and the content of SiO2 and the content of MgO in the slag are controlled and then slag refining is performed. Thereafter, a Ca alloy is added thereto by the start of casting.
    • 要解决的问题:提供一种低热膨胀性和优异的热加工性的廉价高强度的非晶合金,并用于阴极射线管的荫罩,并提供其制造方法。 解决方案:该合金具有含有选自C和Nb,Ni,Co,Al和Ca中的一种或多种强化元素的组合物,如果需要,还含有B,其中Si,Mn, P,S,Mg,Cu,Cr,V,Mo,Ti,N和O被控制在规定值以下,Mg含量的含量控制在规定值以下,Ca / O为 0.1〜2.0,或者将氧化物夹杂物中的Mg,Al,Ca的比例控制在规定的比例,使硫化钙与氧化物夹杂物偶然析出,其余量基本上为Fe。 在合金的制造中,用于二次精炼的渣中的CaO与Al 2 O 3的比例控制在1.4〜2.2,控制炉渣中SiO 2含量和MgO含量,进行渣精炼 。 此后,通过开始浇铸加入Ca合金。
    • 7. 发明专利
    • Stainless steel for motorcycle brake disk
    • 摩托车刹车盘不锈钢
    • JP2005054217A
    • 2005-03-03
    • JP2003284476
    • 2003-07-31
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • YAMAGISHI AKIHITOTSUGE SHINJI
    • C22C38/00C22C38/58
    • PROBLEM TO BE SOLVED: To provide stainless steel for an motorcycle brake disk capable of uniformly obtaining a quenching hardness of 31 to 37 by HRC required even in low temperature quenching at 900°C, and further having satisfactory corrosion resistance.
      SOLUTION: The stainless steel for an motorcycle brake disk has a composition comprising 0.030 to 0.060% C, ≤0.5% Si, 0.5 to 2.0% Mn, 11.0 to 14.0% Cr, 0.3 to 4.0% Ni, 0.010 to 0.10% Nb and 0.007 to 0.030% N, and the balance Fe with impurities, and satisfying the inequality (1), and in which the value of Hc defined by the formula (2) is 31 to 37: Mn+4.1Ni≥2.5% (1), and Hc=145C-0.1Cr+0.8Mn+1.8Ni+6.8Nb+120N+26.8 (2); wherein, the atomic symbols in the inequality (1) and the formula (2) denote the content (mass%) of each element comprised in the steel.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:即使在900℃的低温淬火下,也能够通过HRC均匀地获得31〜37的淬火硬度的摩托车制动盘提供不锈钢,并且还具有令人满意的耐腐蚀性。 解决方案:用于摩托车制动盘的不锈钢具有包括0.030至0.060%C,≤0.5%Si,0.5至2.0%Mn,11.0至14.0%Cr,0.3至4.0%Ni,0.010至0.10% Nb和0.007〜0.030%的N,余量为Fe与杂质,满足不等式(1),其中由式(2)定义的Hc的值为31〜37:Mn +4.1Ni≥2.5%( 1),Hc = 145C-0.1Cr + 0.8Mn + 1.8Ni + 6.8Nb + 120N + 26.8(2); 其中,不等式(1)和式(2)中的原子符号表示钢中包含的每种元素的含量(质量%)。 版权所有(C)2005,JPO&NCIPI
    • 8. 发明专利
    • Austenitic stainless steel strip and manufacturing method therefor
    • 奥氏体不锈钢带及其制造方法
    • JP2003328085A
    • 2003-11-19
    • JP2002132196
    • 2002-05-08
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • HATANO MASAHARUTSUGE SHINJIYAMAGISHI AKIHITO
    • B22D11/00B22D11/12B22D11/18C21D9/46C22C38/00C22C38/40C22C38/58
    • PROBLEM TO BE SOLVED: To provide an austenitic stainless steel strip free from uneven brightness, and a manufacturing method for reliably obtaining the steel strip.
      SOLUTION: (1) The austenitic stainless steel strip comprises less than 0.0010% sol.Al or less than 0.0020% sol.Al, 1.1-2.5% Mn, and more than 0.003% but 0.03% or less Ti, and has oxides existing on the surface layer controlled to an average particle diameter of 0.5 μm or less. (2) The method for manufacturing the austenitic stainless steel strip includes a step of continuously casting the molten steel having the above composition into a slab. The method preferably adopts one or more of controlling a range of a surface fluctuation of a bath surface in a mold to ±3 mm or less during continuously casting the steel, removing the slab surface of 1.5 mm or deeper, and controlling a temperature in finish annealing to 1,120°C or higher.
      COPYRIGHT: (C)2004,JPO
    • 要解决的问题:提供一种没有不均匀亮度的奥氏体不锈钢带,以及可靠地获得钢带的制造方法。 (1)奥氏体不锈钢带包括小于0.0010%的sol.Al或小于0.0020%的sol.Al,1.1-2.5%的Mn和大于0.003%但是0.03%或更少的Ti,并且具有 存在于表面层上的氧化物控制在0.5μm以下的平均粒径。 (2)奥氏体系不锈钢带的制造方法包括将具有上述组成的钢水连续铸造成板坯的工序。 该方法优选在连续铸钢期间将模具中的浴表面的表面波动范围控制在±3mm以下的一种或多种,​​去除1.5mm以上的板坯表面,并控制精加工温度 退火至1120℃以上。 版权所有(C)2004,JPO