    • 3. 发明专利
    • Melting and refining method and apparatus with electron beam
    • 熔融和精炼方法和装置与电子束
    • JP2003075072A
    • 2003-03-12
    • JP2001261088
    • 2001-08-30
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • NISHIBAYASHI TOSHIKIMORI SUMIOSHIGE TAKASHI
    • F27B14/04F27B14/06F27B14/10F27D11/08
    • PROBLEM TO BE SOLVED: To provide an apparatus and a method for stirring an object for melting and refining applicable to the case where a specimen is non-conductive without influencing an electron beam orbital during melting and refining with electron beam.
      SOLUTION: A melting and refining apparatus with electron beam comprises a vacuum container 20, a vacuum exhaust system 22 for keeping the vacuum container vacuum therein, an electron beam generator 14 for generating electron beam 12 in the vacuum container, a deflection coil 26 for generating a magnetic field 24 for deflecting the orbit of the electron beam, a crucible 18 for containing a specimen melted with the electron beam, a hole 18b penetrating a bottom 18a of the crucible, and a gas introduction nozzle 28 for introducing gas for a specimen in the crucible.
      COPYRIGHT: (C)2003,JPO
    • 要解决的问题:提供一种用于搅拌用于熔化和精炼的物体的装置和方法,其适用于在电子束熔化和精炼期间不影响电子束轨道的情况下的样品不导电的情况。 解决方案:具有电子束的熔化和精炼装置包括真空容器20,用于保持真空容器真空的真空排气系统22,用于在真空容器中产生电子束12的电子束发生器14,用于产生 用于偏转电子束的轨道的磁场24,用于容纳用电子束熔化的试样的坩埚18,穿过坩埚的底部18a的孔18b和用于将样品引入气体的气体引入喷嘴28 坩埚。
    • 6. 发明专利
    • Method for producing rotor for turbine
    • 制造涡轮转子的方法
    • JP2003049223A
    • 2003-02-21
    • JP2001236655
    • 2001-08-03
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • SHIGE TAKASHIFUKUNAGA YOSHIAKIKONISHI SATORU
    • B23K9/23B23K9/00C21D9/28C22C38/00
    • PROBLEM TO BE SOLVED: To provide a method for producing a low-cost rotor for a turbine in which a base metal and a joint does not cause delayed cracks when used, and which has proper toughness and strength by single heat treatment after welding of a rotor material for high temperature use and a rotor material for low temperature use without subjecting the rotor material for high temperature use to build-up welding in advance.
      SOLUTION: The production method is provided with a stage wherein a rotor material for high temperature use consisting of 9% Cr steel and a rotor material for low temperature use consisting of 1% Cr steel are welded by using a 9% Cr based filler metal, and a stage wherein the welded rotor material for high temperature use and rotor material for low temperature use are heat- treated at 625 to 655°C.
      COPYRIGHT: (C)2003,JPO
    • 要解决的问题:提供一种用于制造用于涡轮机的低成本转子的方法,其中贱金属和接头在使用时不会引起延迟的裂纹,并且在焊接之后通过单热处理具有适当的韧性和强度 用于高温使用的转子材料和用于低温使用的转子材料,而不经过转子材料进行高温使用以预先堆积焊接。 解决方案:该制造方法具有这样的阶段,其中使用由9%Cr钢组成的高温用转子材料和由1%Cr钢组成的用于低温用途的转子材料通过使用9%Cr基填料金属焊接, 以及将高温用焊接转子材料和低温用转子材料在625〜655℃进行热处理的阶段。