    • 3. 发明专利
    • PRINTED SEAMLESS CAN AND ITS MANUFACTURE
    • JPH1179174A
    • 1999-03-23
    • JP24435797
    • 1997-09-09
    • KISHIMOTO AKIRA
    • GOTO HIROAKISASAKI HIROSHIMOROFUJI AKIHIKOOTSUKA SHINYAYUGAWA YASUHIRO
    • B65D8/00
    • PROBLEM TO BE SOLVED: To provide a printed seamless can and its manufacture, in which roughness at lap application parts and the distortion of printed images, or the deterioration of gloss, due to steps are eliminated, and which is excellent in the fine appearance of a printed part and in a commodity value in the printed seamless can having a printed ink layer provided on an outer surface thereof and a finish varnish layer provided on the printed ink layer, whose finish varnish layer contains an ultraviolet-curable resin and has, in the circumferential direction of a can body, a single application part and lap application parts at narrow intervals. SOLUTION: This printed seamless can has a printed ink layer 4 provided on an outer surface of the can and a finish varnish layer provided on the printed ink layer 4. The finish varnish layer contains an ultraviolet-curable resin and has, in the circumferential direction of a can body, a single application part and lap application parts at narrow intervals. The degree of surface roughness of the lap application parts of the finish varnish layer is at most 0.3 μm and moreover is controlled to a degree less than double of that of the single application part.
    • 4. 发明专利
    • COATED STRUCTURE
    • JPH10230212A
    • 1998-09-02
    • JP3235997
    • 1997-02-17
    • KISHIMOTO AKIRA
    • GOTO HIROAKISASAKI HIROSHIMOROFUJI AKIHIKOOTSUKA SHINYA
    • B65D1/12B05D5/00B05D5/06B05D7/14B05D7/24
    • PROBLEM TO BE SOLVED: To prevent a coating film from a damage such as peeling by applying a coating material containing resin particulates in a specified wt.% so that a part of the particulates may be embedded in the coating film and remainder may be projected from a surface of the coating film, and curing the coating material by ultraviolet ray. SOLUTION: 2-10wt.% Resin particulates are incorporated in the ultraviolet curing type coating material. Then a part of the particulates is embedded in the coating film and remainder is allowed to protrude from the surface of the coating film and cured by the ultraviolet ray. An average grain size of the resin particulates is kept in 5-15μm, and a smooth part of the cured coating film is kept in 0.5-1 time thickness of the average grain size of the resin particulates. For example, a resin other than resin particulates, reactive diluent, oligomer and monomer are blended and dissolved. Moreover, lubricants, an initiator, sensitizer, titanium oxide and 2-10wt.% resin particulates are added to produce the ultraviolet curing type coating material. The coating film having a coefficient of dynamic friction of about 0.10 is obtained in the case when the coating material is applied and cured by ultraviolet ray and the peeling is prevented and a resistance to scuffing is improved.
    • 6. 发明专利
    • SEAMLESS CAN AND MANUFACTURE THEREOF
    • JPH107122A
    • 1998-01-13
    • JP15828896
    • 1996-06-19
    • KISHIMOTO AKIRA
    • AIZAWA MASANORIGOTO HIROAKISASAKI HIROSHIOTSUKA SHINYA
    • B65D1/16B21D22/30B21D51/26B65D8/16
    • PROBLEM TO BE SOLVED: To improve the impact resistance and the corrosion resistance after a formed can for which a printing and a secondary process have been applied by a method wherein a plurality of oriented crystalization states being shown by specified endothermic peaks in a differential thermal analysis, are imparted to a polyester layer on the internal surface of the can, and a spontaneous stretching property is imparted to a polyester layer straight under the flange part. SOLUTION: A laminate plate 1 wherein at least on the internal surface of a metal plate 2, a biaxially oriented polyester film 3 is laminated by a condition to remain the biaxial orientation, is draw-iron-molded, and is formed into a can body wherein the polyester layer 3 is uniaxially oriented, and a heat treatment is performed by a temperature which is -60 to -5 deg.C of the melting point of the polyester. Then, a printing is applied on the external surface of the can body with an ultra-violet ray hardening type ink, and the ink is hardened by irradiating ultra-voilet rays. Then, the printed can body is secondarily molded, and a post-heat treatment is performed by a temperature which is +100 to 150 deg.C of the glass transition point of the polyester. By this method, three kinds of oriented-crystalization states corresponding with specified three endothermic peaks in a differential thermal analysis, and internally distorted state are realized on the polyester layer 3.