会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明专利
    • Method for manufacturing optical fiber
    • 制造光纤的方法
    • JP2005181414A
    • 2005-07-07
    • JP2003418251
    • 2003-12-16
    • Hitachi Cable Ltd日立電線株式会社
    • NISHIO TOMOYUKIMURAKAMI KAZUYATAN KOTARO
    • G02B6/00C03B37/014C03C25/00
    • C03B2201/22C03B2203/23
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing an optical fiber which has excellent fiber characteristics and long-term reliability as a single-mode optical fiber and which can be manufactured at low cost. SOLUTION: The method for manufacturing an optical fiber having a core 21 and a clad part composed of a first clad 22 in the inner layer side and a second clad 23 in the outer layer side, both surrounding the core 21 includes steps of: forming an optical fiber preform while controlling the relative index difference Δ 12 % of the first clad 22 with respect to the second clad 23 to be in the range of -0.1≤Δ 12 COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:提供一种光纤的制造方法,其具有优异的纤维特性和作为单模光纤的长期可靠性,并且可以以低成本制造。 解决方案:包括芯21和由内层侧的第一包层22和外层侧的第二包层23构成的​​包含芯21的光纤的方法,包括芯21包括以下步骤: :将第一包层22相对于第二包层23的相对折射率差ΔSSB> 12 的百分比形成在-0.1≤ΔS12 / SB> <0; 将预成型件拉制成光纤; 并将所获得的光纤保持在重氢气氛中一段预定的时间。 版权所有(C)2005,JPO&NCIPI
    • 3. 发明专利
    • Optical connector
    • 光学连接器
    • JP2008164795A
    • 2008-07-17
    • JP2006352553
    • 2006-12-27
    • Hitachi Cable Ltd日立電線株式会社
    • SUZUKI KANAKOKATO YOSHIHISASHIINA NORIBUMIOSONO KAZUMASANISHIO TOMOYUKI
    • G02B6/36G02B6/38
    • G02B6/3846G02B6/255G02B6/382
    • PROBLEM TO BE SOLVED: To provide an optical connector that suppresses an increase in transmission loss in a connection part, even if connecting holey fibers and that has small change over time in return loss.
      SOLUTION: The optical connector 1 is equipped with a ferrule 3 and a V groove substrate 5 connected to the ferrule 3 and is designed to butt-connect one optical fiber 11 to the other optical fiber 51 in the V groove 8 on the V groove substrate 5, wherein the other optical fiber 51 is connected through a cross-linking-hardening refractive index matching agent r provided on the end face of the one optical fiber 11, and spaces 9, 9 for making the stress imposed on the cross-linking-hardening refractive index matching agent r are provided in the V groove 8 relax.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:即使连接多孔纤维并且在回波损耗中随时间变化小的方式提供抑制连接部分中的传输损耗增加的光连接器。 解决方案:光连接器1配备有与套圈3连接的套圈3和V槽基板5,并被设计成将一根光纤11与V槽8中的另一根光纤51对接 V槽基板5,其中,另一个光纤51通过设置在一个光纤11的端面上的交联硬化折射率匹配剂r和用于施加在十字形上的应力的空间9,9连接 连接硬化型折射率匹配剂r设置在V形槽8中。 版权所有(C)2008,JPO&INPIT
    • 5. 发明专利
    • Mechanical splice
    • 机械系
    • JP2008070545A
    • 2008-03-27
    • JP2006248263
    • 2006-09-13
    • Hitachi Cable Ltd日立電線株式会社
    • NAMEKAWA YOSHIKAZUNAKATANI YOSHIHIROOSONO KAZUMASANISHIO TOMOYUKIKATO YOSHIHISASUZUKI KANAKO
    • G02B6/24
    • PROBLEM TO BE SOLVED: To provide a mechanical splice to be used for splicing of holey fibers.
      SOLUTION: The mechanical splice 1 includes: a V groove substrate 6 that has a V groove 10 for holding and aligning optical fibers 4h, 5 to be spliced by butting them against each other; a pressing substrate 7 that presses the optical fibers 4h, 5 held on the V groove 10; and a clamp spring 8 for clamping the optical fibers 4h, 5 by holding the V groove substrate 6 and the holding substrate 7. In this mechanical splice 1, an optical waveguide member 2 with a hardenable refractive index matching material 3 deposited on one end or both end faces is incorporated in the V groove 10 of the V groove substrate 6.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供用于多孔纤维的拼接的机械接头。 解决方案:机械接头1包括:V槽基板6,其具有V槽10,用于保持和对准通过将它们彼此接合而被接合的光纤4h,5; 压入保持在V槽10上的光纤4h,5的按压基板7; 以及用于通过保持V槽基板6和保持基板7来夹持光纤4h,5的夹紧弹簧8。在该机械接头1中,具有在一端上沉积的具有可硬化折射率匹配材料3的光波导部件2 两个端面被并入V槽基板6的V形槽10中。版权所有(C)2008,JPO&INPIT
    • 7. 发明专利
    • Optical fiber drawing furnace and method of drawing optical fiber
    • 光纤绘图炉和绘制光纤的方法
    • JP2006240930A
    • 2006-09-14
    • JP2005060385
    • 2005-03-04
    • Hitachi Cable Ltd日立電線株式会社
    • SHIROSAWA TATSUYANISHIO TOMOYUKIKUROSAWA YOSHINORI
    • C03B37/029G02B6/00
    • C03B37/029C03B2205/82C03B2205/83
    • PROBLEM TO BE SOLVED: To provide an optical fiber preform, optical fiber, furnace tube and an optical fiber drawing furnace free from the deposition of dust on an exhaust path. SOLUTION: The optical fiber drawing furnace 10 is used for drawing the optical fiber preform P heated and melted in a core 13 while purging the inside of the core 13 with inert gases G1, G2 and is provided with the furnace tube 11 forming the core 13, an inner furnace tube 12 provided in the lower part of the furnace tube 11 and an exhaust path-forming member 20 provided to close the gap between the furnace tube 11 and the inner furnace tube 12 and composed of a heat insulating material. The exhaust path-forming member 20 has the exhaust path 23 for exhausting the inert gases G1, G2 after purging the inside of the core 13 to the outside. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种光纤预制棒,光纤,炉管和光纤拉丝炉,不会在排气路径上沉积灰尘。 解决方案:光纤拉丝炉10用于拉伸在芯13中加热和熔化的光纤预制棒P,同时用惰性气体G1,G2清洗芯13的内部,并且设置有形成 芯13,设置在炉管11的下部的内炉管12和排气路形成构件20,其设置成封闭炉管11和内炉管12之间的间隙,并由绝热材料 。 排气路径形成构件20具有用于在将芯13的内部清除到外部之后排出惰性气体G1,G2的排气路径23。 版权所有(C)2006,JPO&NCIPI
    • 9. 发明专利
    • Manufacturing method and manufacturing apparatus for glass preform
    • 玻璃预制件的制造方法和制造设备
    • JP2003081642A
    • 2003-03-19
    • JP2001269033
    • 2001-09-05
    • Hitachi Cable Ltd日立電線株式会社
    • NISHIO TOMOYUKI
    • G02B6/00C03B8/04C03B37/014
    • C03B37/01446C03B37/0146
    • PROBLEM TO BE SOLVED: To perform dewatering and a heat treatment for transparent glass formation without giving rise to a fluctuation in the external diameter of a glass preform in its longitudinal direction. SOLUTION: The method of manufacturing the glass preform to form the dense transparent glass preform of high purity by subjecting the porous glass preform 2 in a heating furnace 8 while hanging the porous glass preform in a furnace tube 3 and downwardly moving the glass preform under rotation, in which a front end position 14 of the transparent glass preform 12 after the heat treatment is detected on an outlet side below the heating furnace 8 and the front end moving speed of the transparent glass preform 12 is calculated in accordance with this front end position 14, then the output of the heating furnace 8 is so regulated as to eliminate the deviation component between this front end moving speed and the preset feed speed of the transparent glass preform 12.
    • 要解决的问题:为了进行透明玻璃的脱水和热处理而不会引起玻璃预成型件在其纵向上的外径的波动。 解决方案:制造玻璃预成型件以通过将多孔玻璃预制件2放置在加热炉8中同时将多孔玻璃预制件悬挂在炉管3中并向下移动玻璃预成型件旋转的方法来制造玻璃预成型件以形成高纯度的致密透明玻璃预制件 其中,在加热炉8的出口侧检测到热处理后的透明玻璃预成型体12的前端位置14,并根据该前端位置计算出透明玻璃预成型体12的前端移动速度 如图14所示,加热炉8的输出被调整为消除了该前端移动速度与透明玻璃预制件12的预设进给速度之间的偏差分量。