热词
    • 3. 发明专利
    • CONTINUOUS CASTING ROLL EXCELLENT IN COOLING CAPACITY
    • JPH11314144A
    • 1999-11-16
    • JP11973998
    • 1998-04-28
    • NIPPON STEEL CORP
    • ONO KEIICHIROISHIMORI YUICHIICHIKI MASAO
    • B22D11/128
    • PROBLEM TO BE SOLVED: To prevent the lowering of cooling capacity by inserting a rectangular corrosion-resistant metallic plate having specific dimensions so as to be shiftable, into a cooling hole in the axial center of a roll so as to scrape away the stuck and grown scale on the center hole surface at the time of using the roll. SOLUTION: In the cooling hole 2, the metallic plate 3 of any one of an austenitic stainless steel, copper or copper alloy and lead or lead alloy, is inserted. At the time of substituting (t) for the thickness, (w) for the width of the metallic plate 3 and D for the diameter of the cooling hole 2, the dimensions of the metallic plate are made be in the range of w=(0.17-0.92)D, t=(0.05-0.15)D and the metallic plate has the width smaller than the diameter of the cooling hole 2 and larger than the hole diameter of rotary joint adapters 5 on both sides of the roll 1 and the length suitably shorter than the distance between both surfaces of the rotary joint adapters. In this way, the metallic plate 3 is turned over accompanied with the slow rotation of the roll 1 to scrape away the scale stuck on the surface of the cooling hole 2 and tending to grow with the collision and the slippage to the surface of the cooling hole 2.
    • 4. 发明专利
    • UNIVERSAL SHAFT JOINT IN MOLTEN METAL
    • JPH07138722A
    • 1995-05-30
    • JP29045893
    • 1993-11-19
    • NIPPON STEEL CORPNTN TOYO BEARING CO LTD
    • ONO KEIICHIROTSUYUKI AKIRA
    • F16D3/16C23C2/00C23C2/40
    • PURPOSE:To greatly prolong the service life of the universal shaft joint of a clutch type by forming only the meshed parts, etc., for transmitting torque of the pawls and grooves formed on the joint body from a corrosion resistant and wear resistant alloy. CONSTITUTION:The in-bath universal shaft joint for driving the support roll of a continuous galvanizing device is composed of a pawl side shaft 8 having plural pieces of joint pawls 9 radially overhanging at equal intervals at the shaft end and a joint outside cylinder 10 having grooves to be meshed with these pawls 9 at the shaft end. At this time, the pawl side shaft 8 and the joint outside cylinder 10 are formed from an alloy consisting of SUS 410. High- hardness liners 12, 13, 14, 15 consisting of any of ceramics, cermet or corrosion resistant and wear resistant alloy having a required thickness are mounted only at the meshing parts A-1, A-2 for transmitting the torque of the pawls 9 and the grooves and the central joint side end face contact parts B-1, B-2 of the pawl side shaft 8 and the joint outside cylinder. As a result, the life of the universal shaft joint is greatly prolonged and the chatter marks of the steel sheet surface are drastically decreased.
    • 8. 发明专利
    • CONTINUOUS CASTING ROLL EXCELLENT IN COOLING POWER
    • JP2000107843A
    • 2000-04-18
    • JP28228698
    • 1998-10-05
    • NIPPON STEEL CORP
    • ONO KEIICHIROISHIMORI YUICHIMIYAMOTO YASUNORIICHIKI MASAO
    • B22D11/128
    • PROBLEM TO BE SOLVED: To prevent the sticking of scale on a cooling hole by arranging a clamper to a pipe for cooling water, fitting stainless steel-made rings to the clamper, sizing the diameter of the ring to the intermediate size between the outer diameter of the pipe and the diameter of the cooling hole and disposing stainless steel round bars in a space formed with the adjacent rings, the outer diameter of the pipe and the inner wall of the cooling hole. SOLUTION: The clamper 4 projecting to the diameter direction is arranged to the pipe 3 in the inner part of the cooling hole 2 in the continuous casting roll. To the clamper 4, the rings 7-1, 7-2, 7-3 are welded and fixed. The stainless steel round bars 8 are disposed in the spaces between the adjacent rings 7-1 and 7-2 and between the adjacent rings 7-2 and 7-3. The diameter of the stainless steel round bar 8 is sized to >1/2 of the gap size between the outer surface of the pipe 3 and the inner wall of the cooling hole 2 in the continuous casting roll. Applying of knurling or rough shot blasting on the outer cylindrical surface of the stainless steel round bar 8, is desirable because of the improvement of the effect for peeling out the scale.
    • 9. 发明专利
    • CONTINUOUS CASTING ROLL
    • JPH11267807A
    • 1999-10-05
    • JP7100198
    • 1998-03-19
    • NIPPON STEEL CORP
    • ISHIMORI YUICHIONO KEIICHIRO
    • B22D11/128
    • PROBLEM TO BE SOLVED: To prevent the development of a crack which arises from the continuos casting roll surface, in almost parallel to the perimeter direction, and progresses from the surface to the inside. SOLUTION: The particle with the curvature in the crack progress direction for preventing the progress of the crack is placed in concentric circular state in the roll cross section at a certain depth from a roll surface where breakage does not happen even if the crack develops and also placed so that crack progress from any position may reach the particle. Further, the combination of the particle and the peripheral material should be the combination of the particle and the peripheral material, in which the crack does not develop continuously from the peripheral material to the particle. By this, breakage trouble of the continuous casting roll by the progress of the crack is solved, and an exchange period for the crack repair is drastically improved, and the productivity of the continuous casting equipment can be improved.