会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明专利
    • Magnetic head
    • 磁头
    • JPS6199913A
    • 1986-05-19
    • JP19487484
    • 1984-09-19
    • Hitachi LtdHitachi Maxell Ltd
    • INAGOYA OSAMUFUJIWARA HIDEOYAMANO MINORUTOTTORI TAKESHIKUMASAKA TAKAYUKIOTOMO MOICHIKUDO SANEHIROMORIKAWA JUICHI
    • G11B5/127G11B5/187G11B5/23G11B5/245G11B5/265G11B5/31
    • G11B5/3103G11B5/127G11B5/1878
    • PURPOSE:To improve the magnetic characteristic by constituting a core base part and a magnetic thin film stuck to its surface so that the minimum value of the sum total of the product of a sectional area except a magnetic gap part of a magnetic path and a saturation magnetic flux density exceeds the product of the magnetic thin film and the saturation magnetic flux density. CONSTITUTION:In a magnetic path except a magnetic gap opposed surface in the first core half body 24, the sum total of the product of a sectional area roughly vertical to the direction of a magnetic flux flowing to the first core base body 30 and a saturation magnetic flux density of the first core base body, and the product of a sectional area roughly vertical to the direction of a magnetic flux flowing to the first magnetic thin film 31 and a saturation magnetic flux density of its first magnetic thin film 31 becomes the smallest at positions of thick lines A, B, C, D and E. In case when sectional areas of parts which have been cut along the thick lines A, B, E, C and D are denoted as S1, S2, S3, S4 and S5, respectively, and a magnetic gap opposed area of the magnetic thin film 31, a saturation magnetic flux density of the first core base body 30, and a saturation magnetic flux density of the magnetic thin film 31 have been defined as S6, B31, and B32, respectively, the core base body 30 and the magnetic thin film 31 are constituted so that the expression is formed (S1+S2+S3)B32+ S4.B31>=S6.B32. In this way, an excellent magnetic characteristic is obtained.
    • 目的:通过构成芯基部和粘附在其表面上的磁性薄膜来提高磁特性,使得除了磁路的磁隙部分以外的截面积和饱和度的乘积的总和的最小值 磁通密度超过磁性薄膜的乘积和饱和磁通密度。 构成:除了第一铁心半体24中的磁隙对置面以外的磁路中,与流过第一铁心基体30的磁通的方向大致垂直的截面积的积的总和和饱和 第一芯基体的磁通密度以及与流过第一磁性薄膜31的磁通方向大致垂直的截面积和其第一磁性薄膜31的饱和磁通密度的乘积成为最小 在粗线A,B,C,D和E的位置处,沿着粗线A,B,E,C和D切割的部分的截面面积被表示为S1,S2,S3,S4和 S5,磁性薄膜31的磁隙对置区域,第一芯基体30的饱和磁通密度和磁性薄膜31的饱和磁通密度定义为S6,B31, 和B32,分别为核心底座 y 30和磁性薄膜31构成为形成表达式(S1 + S2 + S3)B32 + S4.B31> = S6.B32。 以这种方式获得优异的磁特性。
    • 2. 发明专利
    • Magnetic head
    • 磁头
    • JPS6174113A
    • 1986-04-16
    • JP19487684
    • 1984-09-19
    • Hitachi LtdHitachi Maxell Ltd
    • TOTTORI TAKESHIFUJIWARA HIDEOHAYASHI MASASHIUSUI AKIRAKUMASAKA TAKAYUKIOTOMO MOICHIKUDO SANEHIROISHIHARA KIYOSHI
    • G11B5/245G11B5/127G11B5/187G11B5/23G11B5/31
    • G11B5/3103G11B5/1878
    • PURPOSE:To prevent crack and chipping of a core half at manufacture and to ensure excellent magnetic characteristic by forming a very narrow flat part to the tip of a projection of the core half coated with a magnetic film. CONSTITUTION:A flat part 70 having a very narrow width not causing any pseudo magnetic gap, e.g., 15mum or the like is formed at the tip of the projection 29 of the 1st core base 30 to which the 1st magnetic film 31 of a recording/ reproducing head 21 is coated. Then similar flat parts 71, 72, 73 are formed at projections 42, 45 of of an erasure head 22 and a projection 32 of the 2nd core base 33. Thus, crack and chipping at manufacture of the core half are prevented, the number is reduced to 1/3 of that of a conventional head and the excellent magnetic characteristic is ensured.
    • 目的:为了防止制造时半芯片的裂纹和碎裂,并且通过在涂覆有磁性膜的芯部半部的突起的尖端上形成非常窄的扁平部分来确保优异的磁特性。 构成:在第一芯基座30的突起29的顶端处形成具有非常窄的宽度的不产生任何假磁隙(例如15μm等)的平坦部分70,记录/ 再现头21被涂覆。 然后,类似的平面部分71,72,73形成在擦除头22的突起42,45和第二芯基座33的突出部32上。因此,防止在芯部半制造时的裂纹和碎裂,数量是 降低到常规头的1/3,并且确保优异的磁特性。
    • 3. 发明专利
    • Magnetic head
    • 磁头
    • JPS61115204A
    • 1986-06-02
    • JP23596684
    • 1984-11-10
    • Hitachi LtdHitachi Maxell Ltd
    • INAGOYA OSAMUFUJIWARA HIDEOTOTTORI TAKESHIHAYASHI MASASHIOTOMO MOICHIKUMASAKA TAKAYUKIKUDO SANEHIRO
    • G11B5/127G11B5/187H01F10/20
    • G11B5/127G11B5/187
    • PURPOSE:To assure an excellent magnetic characteristic by positioning the sliding surface of a substrate which supports a thin ferromagnetic metallic film toward the (1, 1, 0) face from the single crystal manganese-zinc ferrite face and toward the (2, 1, 1) face from the (1, 1, 1) face respectively within specific angles of inclination. CONSTITUTION:A magnetic head is manufactured by using respectively single crystal manganese-zinc ferrite as the core substrate and an amorphous alloy of cobalt-niobium-zirconium as the thin ferromagnetic metallic film. The magnetic head is brought into contact with a magnetic disk while the disk is kept rotated to maintain the continuous sliding contact between the head and disk. As a result, the head is so formed that the sliding surface of the core substrate is positioned within the range of 0-30 angle of inclination from the (1, 1, 1) face toward the (1, 1, 0) face and within the range of 0-30 angle of inclination from the (1, 1, 1) face toward (2, 1, 1) face, then the core substrate and the thin ferromagnetic metallic film wear approximately at the similar rate and therefore the difference of steps between both is extremely small.
    • 目的:通过将支撑薄铁磁性金属膜的基板的滑动面从单晶锰锌铁氧体磁体朝向(1,1,0)面朝向(2,1, 1)分别在特定倾斜角内从(1,1,1)面朝向。 构成:通过分别使用单晶锰锌铁氧体作为核心基板和钴 - 铌 - 锆的非晶合金作为薄铁磁金属膜来制造磁头。 磁盘与磁盘接触,同时保持磁盘旋转以保持磁头和磁盘之间的连续滑动接触。 结果,头部形成为使得芯基板的滑动面位于从(1,1,1)面朝向(1,1,0)面的0-30°的倾斜角度的范围内,以及 在从(1,1,1)面到(2,1,1)面的0-30°的倾角范围内,芯基板和薄铁磁性金属膜的磨损程度大致相同,因此差异 两者之间的步骤是非常小的。
    • 6. 发明专利
    • Magnetic head
    • 磁头
    • JPS6139907A
    • 1986-02-26
    • JP16026484
    • 1984-08-01
    • Hitachi LtdHitachi Maxell Ltd
    • FUJIWARA HIDEOKUMASAKA TAKAYUKIOTOMO MOICHIYAMASHITA TAKEOKUDO SANEHIRO
    • G11B5/127G11B5/187G11B5/23G11B5/245G11B5/31
    • G11B5/3103G11B5/187G11B5/313
    • PURPOSE:To realize a head having an excellent magnetic characteristic by increasing the total thickness of the magnetic thin film of a core half having a titled base to a gap face to be larger than the width at the tip of a magnetic thin film corresponding to the track width. CONSTITUTION:A side face 7 of two core halves 9, 10 opposing a gap face is tilted to the gap face and the magnetic thin film 4 is formed to the side face 7. Then the total thickness of the magnetic thin film 4, that is, T1+T3, is set to be larger than the width TW at the tip of the magnetic thin film 4 corresponding to the track width. Thus, the magnetic saturation of the magnetic thin film at a part from the magnetic gap before the saturation of a magnetic flux density of the magnetic gap occurred conventionally is avoided and the head with excellent magnetic characteristic enhancing sufficiently the effect of the magnetic thin film is obtained.
    • 目的:通过将具有标称基底的芯半部的磁性薄膜的总厚度增加到间隙面来实现具有优异磁特性的磁头,其大于对应于磁性薄膜的磁性薄膜的尖端处的宽度 轨道宽度。 构成:与间隙面相对的两个半部分9,10的侧面7向间隙面倾斜,并且磁性薄膜4形成在侧面7上。然后,磁性薄膜4的总厚度 ,T1 + T3被设定为大于与磁道宽度对应的磁性薄膜4的前端的宽度TW。 因此,可以避免磁性薄膜在磁饱和之前的磁隙的一部分处的磁饱和发生,磁性薄膜的效果充分提高, 获得。
    • 8. 发明专利
    • Magnetic head
    • 磁头
    • JPS6174118A
    • 1986-04-16
    • JP19487584
    • 1984-09-19
    • Hitachi LtdHitachi Maxell Ltd
    • INAGOYA OSAMUFUJIWARA HIDEOTOTTORI TAKESHIYAMANO MINORUKUMASAKA TAKAYUKIOTOMO MOICHIKUDO SANEHIROMORIKAWA JUICHI
    • G11B5/245G11B5/127G11B5/187G11B5/23G11B5/265G11B5/31
    • G11B5/3103G11B5/1878
    • PURPOSE:To realize a head with excellent high frequency characteristic by selecting an cross angle of both side faces of a projected part of a core base as >=90 deg. so as to make the magnetic thin film thin. CONSTITUTION:A composite magnetic head consists of a recording/reproducing head 21, an erasure head 22 and an intermediate nonmagnetic substance 23. The 1st core half 24 consists of the 1st core base 30 having a projection 29 at the center of opposed side face to the magnetic gap 35 and the 1st magnetic thin film 31. Then a top angle theta2 of the projection 29 is specified in the range between 90 and 150 deg.. The similar structure is applied also to the erasure head 22. Thus, the characteristic of the magnetic thin film is attained sufficiently and chipping is prevented to make the film thickness thin. Thus, the magnetic loss based on eddy currents is suppressed to obtain a head with excellent high frequency characteristic.
    • 目的:通过选择核心基底的突出部分的两个侧面的横角为> = 90度,实现具有优异的高频特性的头部。 从而使磁性薄膜变薄。 构成:复合磁头由记录/再现头21,擦除头22和中间非磁性物质23组成。第一芯半部24由第一芯基座30组成,第一芯基座30具有在相对侧面至 磁隙35和第一磁性薄膜31.然后,凸起29的顶角θ2在90和150度之间的范围内。类似的结构也应用于擦除头22.因此, 充分地获得磁性薄膜,防止了切片,使薄膜变薄。 因此,抑制基于涡电流的磁损耗,以获得具有优异的高频特性的磁头。
    • 9. 发明专利
    • Thin film magnetic head
    • 薄膜磁头
    • JP2004334995A
    • 2004-11-25
    • JP2003130983
    • 2003-05-09
    • Hitachi Ltd株式会社日立製作所
    • OTOMO MOICHIFUKUI HIROSHIYONEKAWA SUNAOMARUYAMA YOJIIWAKURA TADAYUKI
    • G11B5/39
    • G11B5/3916
    • PROBLEM TO BE SOLVED: To provide a thin film magnetic head having small thermal protrusion with respect to the rise of the environmental temperature.
      SOLUTION: A magnetic material having a low thermal expansion coefficient that is equal to or less than 11.5×10
      -6 /K is used for at least one of a bottom section shield or a top section shield. Moreover, a laminated layer film made of a magnetic material having a low thermal expansion coefficient that is equal to or less than 11.5×10
      -6 /K and an 80 wt% NiFe alloy is used for at least the bottom section shield or the top section shield. Thus, a thin film magnetic head, in which noise is made low after recording and thermal protrusion is reduced, is obtained.
      COPYRIGHT: (C)2005,JPO&NCIPI