热词
    • 41. 发明专利
    • Composite material for brazing, and brazed product using the same
    • 用于制动的复合材料和使用其的BRAZED产品
    • JP2006334602A
    • 2006-12-14
    • JP2005158864
    • 2005-05-31
    • Hitachi Cable Ltd日立電線株式会社
    • KUROKI KAZUMAKURODA HIROMITSUSAGAWA HIDEYUKIHORII FUMIOSAKUYAMA NOBUHITO
    • B23K35/14B23K35/30C22C30/00H01M8/06
    • Y02E60/50
    • PROBLEM TO BE SOLVED: To provide a composite material for brazing having excellent heat resistance, oxidation resistance, high temperature resistance and corrosion resistance, and having satisfactory brazing workability, and to provide a brazed product using the same. SOLUTION: The composite material 10 for brazing is characterized in that the surface of a base material 11 composed of an Ni-containing alloy is integrally provided with a brazing filler metal layer with a multilayer structure in which each Fe or Fe alloy layer 12, each Ti or Ti alloy layer 13 and each Ni or Ni alloy layer 14 are laminated, and the ratio between the weight W1 of the Ni component comprised in the brazing filler metal layer and the total W2 of the weight of the Ni component and the Ti component, W1/W2 is controlled to 0.58 to 0.66. COPYRIGHT: (C)2007,JPO&INPIT
    • 解决的问题:提供耐热性,耐氧化性,耐高温性和耐腐蚀性优异的钎焊用复合材料,并且具有令人满意的钎焊加工性,并提供使用该复合材料的钎焊制品。 解决方案:用于钎焊的复合材料10的特征在于,由含Ni合金构成的基材11的表面一体地设有具有多层结构的钎料金属层,其中每个Fe或Fe合金层 如图12所示,Ti,Ti合金层13和Ni或Ni合金层14层叠,并且包含在钎料层中的Ni成分的重量W1与Ni成分的重量的总W2的比例 将Ti成分W1 / W2控制为0.58〜0.66。 版权所有(C)2007,JPO&INPIT
    • 43. 发明专利
    • Brazing method, filler metal therefor, composite material using the filler metal, and brazed product
    • 填充方法,填充金属,使用填充金属的复合材料和BRAZED产品
    • JP2005186106A
    • 2005-07-14
    • JP2003430329
    • 2003-12-25
    • Hitachi Cable Ltd日立電線株式会社
    • SAGAWA HIDEYUKIKURODA HIROMITSUKUROKI KAZUMASHIRAI SUKAKU
    • F28F21/08B23K1/00B23K1/19B23K1/20B23K35/14B23K35/30B23K35/32C22C9/00C22C14/00C22C19/03
    • PROBLEM TO BE SOLVED: To provide a brazing method that shows a superb flowing characteristic of molten metal and an excellent corrosion resistance in a brazed part, to provide a filler metal for the method and a composite material for brazing using this filler metal, and also to provide a brazed product superior in reliability of the brazed part and inexpensive in the manufacturing cost.
      SOLUTION: This brazing method is for brazing members 31, 32 to be brazed, with a filler metal 10 formed by including in a brazer base material a specific metal for improving the flowing characteristic of molten metal. In brazing the members 31, 32 to be brazed using such filler metal 10, the filler metal 10 is fused and then, with the atmospheric pressure P2 maintained at or below the vapor pressure P
      d1 of the specific metal, the brazing is performed by vaporizing the specific metal from the filler metal 10.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:为了提供一种钎焊方法,其显示熔融金属的极好的流动特性和在钎焊部件中具有优异的耐腐蚀性,以提供该方法的填充金属和使用该填充金属的钎焊复合材料 并且还提供钎焊部件的可靠性优异的钎焊制品,并且制造成本低廉。 解决方案:该钎焊方法是钎焊构件31,32钎焊,其中通过在钎焊基材中包含用于改善熔融金属的流动特性的特定金属形成的填充金属10。 在使用这种填料金属10钎焊待钎焊的构件31,32时,将填充金属10熔化,然后在大气压力P2维持在或低于特定金属的蒸气压P d1 ,通过从填充金属10中蒸发特定金属来进行钎焊。版权所有(C)2005,JPO&NCIPI
    • 44. 发明专利
    • Composite material for brazing, and brazing method using the same
    • 用于制动的复合材料和使用其的制动方法
    • JP2005111548A
    • 2005-04-28
    • JP2003352054
    • 2003-10-10
    • Hitachi Cable Ltd日立電線株式会社
    • KUROKI KAZUMAKURODA HIROMITSUSAGAWA HIDEYUKISHIRAI SUKAKU
    • F28F21/08B23K1/00B23K35/14B23K101/08B23K101/12B23K101/14
    • PROBLEM TO BE SOLVED: To provide a composite material for brazing, with which brazing can be carried out without causing a rise in the fusion temperature of a brazing filler metal, in brazing conducted by two divided heat-treatment steps, and a brazing method using the same.
      SOLUTION: The invented composite material 10 for brazing is used for brazing members to be brazed together and comprises duplex superimposed metal layers made of at least two kinds of metals, of which one is a brazing layer 11 with a low fusing point and the other is a brazing layer 12 with a high fusing point. The brazing layer 11 with a low fusing point is a laminated layer composed of copper or a copper alloy 13 and titanium or a titanium alloy 14. The brazing layer 12 with a high fusing point is a laminated layer composed of nickel or a nickel alloy 15 and titanium or a titanium alloy 16.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:提供一种用于钎焊的复合材料,通过两个分开的热处理步骤进行的钎焊,可以进行钎焊而不引起钎焊料的熔化温度升高,并且 钎焊方法使用相同。 解决方案:本发明的用于钎焊的复合材料10用于被钎焊在一起的钎焊构件,并且包括由至少两种金属制成的双面叠层金属层,其中一个是具有低熔点的钎焊层11, 另一个是具有高熔点的钎焊层12。 具有低熔点的钎焊层11是由铜或铜合金13和钛或钛合金14组成的层压层。具有高熔点的钎焊层12是由镍或镍合金15构成的层压层 和钛或钛合金16.版权所有(C)2005,JPO&NCIPI
    • 45. 发明专利
    • Composite material for brazing and brazed product using the same
    • 使用它的制动和制动产品的复合材料
    • JP2005088071A
    • 2005-04-07
    • JP2003328591
    • 2003-09-19
    • Hitachi Cable Ltd日立電線株式会社
    • SAGAWA HIDEYUKIKURODA HIROMITSUKUROKI KAZUMASHIRAI SUKAKU
    • B23K35/30B23K35/14C22C19/03
    • PROBLEM TO BE SOLVED: To provide a composite material for brazing which has excellent brazing characteristic and excellent heat resistance and corrosion resistance in a brazed portion, and to provide a brazed product which is excellent in reliability of the brazed portions and is low in its manufacturing cost.
      SOLUTION: This composite material 10 for brazing is used to braze members to be brazed to each other, and is composed of a brazing material 15 of a composite layer structure with a Ni layer or a Ni-alloy layer 13 and a Ti layer or a Ti alloy layer 12 overlapped each other. The ratio W1/W2 is 0.60-0.68, wherein W1 denotes the weight of Ni component contained in the brazing material 15, and W2 denotes the total weight of the Ni component and the Ti component.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:提供钎焊部分具有优异的钎焊特性和优异的耐热性和耐腐蚀性的钎焊用复合材料,并且提供钎焊部分的可靠性优异且低的钎焊制品 在制造成本上。 解决方案:用于钎焊的复合材料10用于钎焊彼此钎焊的构件,并且由具有Ni层或Ni合金层13的复合层结构的钎料15和Ti 层或Ti合金层12彼此重叠。 比W1 / W2为0.60-0.68,其中W1表示钎焊材料15中所含的Ni成分的重量,W2表示Ni成分和Ti成分的总重量。 版权所有(C)2005,JPO&NCIPI
    • 47. 发明专利
    • Method of joining soft dilute copper alloy wire to connection terminal
    • 将软钎焊铜合金线连接到终端的方法
    • JP2014102996A
    • 2014-06-05
    • JP2012254427
    • 2012-11-20
    • Hitachi Cable Ltd日立電線株式会社
    • WASHIMI TORUAOYAMA MASAYOSHIKURODA HIROMITSUSAGAWA HIDEYUKIFUJITO KEISUKE
    • H01R4/18C22C9/00C22C9/05C22C9/06C22F1/00C22F1/08H01B1/02H01B5/08H01B7/00H01R13/03
    • PROBLEM TO BE SOLVED: To provide a soft dilute copper alloy wire having high conductivity and a high flex life, which can suppress disconnection during usage in comparison with an oxygen-free copper wire and can be ultrasonically connected to a connection terminal, and a method of joining the soft dilute copper alloy wire to the connection terminal.SOLUTION: The method includes the steps for: manufacturing a soft dilute copper alloy wire 11 by drawing a soft dilute copper alloy material containing an additive element easily bonded to S such as copper, Ti, or the like at a processing degree of 90% or higher and applying annealing to it, and by annealing a roughly drawn wire the average crystal grain size of which is 20 μm or smaller in a surface layer formed from the surface thereof till the depth of 50 μm, and the elongation value of which is 40% or higher while drawing it; manufacturing a cable 10 by making a conductor 12 by stranding a plurality of the copper alloy wires 11 and forming an insulating cover 13 on the periphery of the conductor 12; and ultrasonically joining a connection terminal 20 to the conductor 12 at the terminal of the cable 10.
    • 要解决的问题:提供一种具有高导电性和高挠曲寿命的柔软的稀铜合金丝,与无氧铜线相比可以抑制使用时的断开,并且可以超声波连接到连接端子上 将软弱铜合金线连接到连接端子上。方法:该方法包括以下步骤:通过拉伸含有容易与S结合的添加剂元素的铜的软的稀铜合金材料来制造软的稀铜合金丝11, Ti等等,并且对其进行退火,并且通过将由其表面形成的表面层中的平均晶粒尺寸为20μm或更小的粗拉丝退火直到 深度为50μm,拉伸时的伸长率为40%以上; 通过使多根铜合金线11绞合并在导体12的周围形成绝缘盖13来制造导体12来制造电缆10; 并且在电缆10的端子处将连接端子20超声波连接到导体12。