    • 1. 发明专利
    • Support device of cylindrical member, method of manufacturing the cylindrical member, and plate material
    • 圆柱形构件的支撑装置,制造圆柱形构件的方法和板材料
    • JP2013173186A
    • 2013-09-05
    • JP2013012646
    • 2013-01-25
    • Honda Motor Co Ltd本田技研工業株式会社
    • MITA KAZUYUKIKIMURA TAKEHISAHIGUCHI AKINORINAKAJIMA KATSUYUKIITO MASAMI
    • B23K37/053B23K9/025
    • PROBLEM TO BE SOLVED: To provide a support device of a cylindrical member which can adequately weld both end parts of a plate material.SOLUTION: A support device of the cylindrical member 4 supports the cylindrical member 4, which is manufactured by curving the plate material and welding both end parts 1a, 1b, so as to clip from both end part sides by two pressing members 3, 3'. Cutout parts 2 are formed on both end parts of side edges of the plate material 1, and an end part side of the cutout part 2 becomes a cutout part side inclined surface 2a which inclines so as to be closer to the end parts 1a, 1b gradually toward an outside. Projection parts 5 corresponding to the cutout parts 2 are formed on the pressing members 3, 3', and the projection part includes a projection part side inclined surface 5a inclined by corresponding to the cutout part side inclined surface 2a. The plate material 1 is clipped by the pressing members 3, 3'. Force in a clipping direction of the pressing members 3, 3' is converted into force in an approaching direction of both end parts 1a, 1b of the plate material 1 when the projection part side inclined surface 5a abuts on the cutout part side inclined surface 2a.
    • 要解决的问题:提供一种圆柱形构件的支撑装置,其可以适当地焊接板材的两个端部部分。解决方案:圆柱形构件4的支撑装置支撑圆柱形构件4,其通过弯曲板材制造 并且焊接两个端部1a,1b,以便通过两个按压部件3,3'从两个端部侧夹持。 切割部分2形成在板材1的侧边缘的两个端部,并且切口部分2的端部侧成为倾斜以更靠近端部1a,1b的切口部分侧倾斜面2a 逐渐走向外面。 对应于切口部分2的投影部分5形成在按压部件3,3'上,并且突出部分包括相应于切口部分侧倾斜面2a倾斜的突出部分侧倾斜面5a。 板材1被按压部件3,3'夹住。 当突起部分侧倾斜表面5a抵接在切口部分侧倾斜表面2a上时,按压部件3,3'的夹紧方向的力沿着板材1的两个端部1a,1b的接近方向转换 。
    • 2. 发明专利
    • Correction device of engine valve
    • 发动机阀校正装置
    • JP2013160181A
    • 2013-08-19
    • JP2012024329
    • 2012-02-07
    • Honda Motor Co Ltd本田技研工業株式会社
    • SUGITA MASAYAKIMURA TAKEHISAMABUCHI NATSUHIKOKINOSHITA KATSUMISAITO YUJI
    • F01L3/24
    • PROBLEM TO BE SOLVED: To provide an inexpensive correction device of an engine valve, capable of easily correcting a stem part and an umbrella-like part of the engine valve.SOLUTION: In an umbrella correction die 20 for correcting an umbrella-like part of an engine valve, a biting part 22 and a relief part 23 are provided in addition to a correction part 21. The umbrella correction die 20 is rotated less than one revolution with the engine valve set in the relief part 23. In short, the engine valve is corrected in the biting part 22, the correction part 21 and the relief part 23 in this order. The biting part corrects the tilted umbrella-like part. Consequently, an inexpensive correction device of the engine valve is provided, which can easily correct a stem part and the umbrella-like part of the engine valve.
    • 要解决的问题:提供一种便宜的发动机气门校正装置,能够容易地校正发动机气门的杆部和伞状部分。解决方案:在用于校正伞形部分的伞形部分的伞式校正模具20中, 除了校正部件21之外,还设置有发动机气门,咬入部22和凸出部23.伞修正模20与设置在凸出部23中的发动机气门旋转小于1转。简而言之,发动机 在咬合部22,校正部21和浮雕部23中依次修正阀。 咬合部分纠正倾斜的伞状部分。 因此,提供了一种廉价的发动机阀的校正装置,其可以容易地校正发动机气门的杆部和伞状部分。
    • 4. 发明专利
    • Manufacturing method of metal ring and device therefor
    • 金属环的制造方法及其器件
    • JP2014100720A
    • 2014-06-05
    • JP2012253210
    • 2012-11-19
    • Honda Motor Co Ltd本田技研工業株式会社
    • NAKAJIMA KATSUYUKIHIGUCHI AKINORIMITA KAZUYUKIKIMURA TAKEHISA
    • B23K26/38B23K26/08B23K26/10B23K26/16
    • PROBLEM TO BE SOLVED: To remove spatters generated in a step for irradiating a metal cylindrical workpiece (drum) with laser light so as to be cut in a round sliced shape, from a holding member for holding the cylindrical workpiece.SOLUTION: A metal ring manufacturing device 10 has a holding tool 16 in which a longitudinal direction passage 76 and a circumferential direction passage 78 are formed on the side wall. When a cylindrical workpiece W held on the side wall is cut, molten scattering objects entering the circumferential direction passage 78 or spatters formed by solidifying the molten scattering objects are removed by a fluid (for example, compressed air) supplied into the circumferential direction passage 78. Namely, the holding tool 16 is cleaned by the fluid.
    • 要解决的问题:从用于保持圆柱形工件的保持构件中去除用于用激光照射金属圆柱形工件(鼓)以从圆形切割形状切割的步骤中产生的飞溅物。解决方案:金属环 制造装置10具有保持工具16,其中在侧壁上形成有纵向通道76和周向通道78。 当保持在侧壁上的圆柱形工件W被切割时,通过供给到圆周方向通道78的流体(例如,压缩空气)去除进入圆周方向通道78的熔融散射物体或通过固化熔融散射物体形成的飞溅物 即,保持工具16被流体清洗。
    • 6. 发明专利
    • Method and apparatus for manufacturing metal ring
    • 用于制造金属环的方法和装置
    • JP2014024093A
    • 2014-02-06
    • JP2012166447
    • 2012-07-27
    • Honda Motor Co Ltd本田技研工業株式会社
    • MITA KAZUYUKIHIGUCHI AKINORIKIMURA TAKEHISANAKAJIMA KATSUYUKI
    • B21D53/16B21D3/14
    • PROBLEM TO BE SOLVED: To efficiently obtain a high-precision metal ring by correcting a drum to have a nearly true circular shape and smoothly inserting a work holding member into the drum.SOLUTION: A method for manufacturing a metal ring includes the steps of: determining, when a minimum clearance L between an outer peripheral surface 16a of a diameter-reduced work holding member 16 and an inner peripheral surface 12a of a drum 12 is provided over the whole circumference of the drum 12, the minimum diameter Ra of an inscribed circle inscribed in the drum 12; determining correction load enabling the drum 12 to be corrected so as to have a shape having an inscribed circle with the minimum diameter Ra or greater (a nearly true circular shape); and correcting the drum 12 by application of the correction load via correction members 20 and 22.
    • 要解决的问题:为了有效地获得高精度的金属环,通过校正滚筒以具有几乎真实的圆形并将工件保持构件平滑地插入滚筒中。解决方案:一种用于制造金属环的方法包括以下步骤: 确定当直径减小的工件保持构件16的外周表面16a和滚筒12的内周表面12a之间的最小间隙L设置在滚筒12的整个圆周上时,刻划的最小直径Ra 圆圈刻在滚筒12中; 确定校正负载,使得滚筒12被校正成具有具有最小直径Ra或更大的内接圆的形状(几乎是真实的圆形); 以及通过经由校正构件20和22施加校正载荷来校正滚筒12。
    • 8. 发明专利
    • Brush and method for manufacturing the same
    • BRUSH及其制造方法
    • JP2013031537A
    • 2013-02-14
    • JP2011168845
    • 2011-08-01
    • State Kogyo Kkステイト工業株式会社Honda Motor Co Ltd本田技研工業株式会社
    • NAKANE TOSHIHARUYAGASAKI TORUKIMURA TAKEHISAAOYAMA HIDEAKIMITA KAZUYUKI
    • A46D3/06
    • PROBLEM TO BE SOLVED: To provide a brush for disusing a cap-like supporting member which supports bristle materials to reduce frequency of exchange capable of manufacturing in a short period of time compared with the conventional brushes, and to provide a method for manufacturing the brush.SOLUTION: The method for manufacturing the brush which is detachably attached to a mounting part of a brush device includes the steps of: manufacturing brush body for manufacturing a brush body 10 to form a fusion part 12 integrally fused by dissolving bristle materials 11 into proximal ends of a bundle made of a plurality of bristle materials 11 made of resins; manufacturing engaging body for manufacturing an engaging body 20 made of resins engaged with the mounting part of the brush device; and joining for fusing the fusion part 12 of the brush body 10 and the engaging body 20.
    • 要解决的问题:提供一种用于排除支撑刷毛材料的帽状支撑构件的刷子,以减少与常规刷子相比在短时间内制造的交换频率,并且提供一种用于 制造刷子。 解决方案:可拆卸地附接到刷装置的安装部分的刷子的制造方法包括以下步骤:制造用于制造刷体10的刷体,以形成通过溶解刷毛材料11而整体熔合的熔化部分12 由多个由树脂制成的刷毛材料11制成的束的近端; 制造用于制造由与刷装置的安装部分接合的树脂制成的接合体20的接合体; 以及用于熔合刷体10和接合体20的熔融部分12的接合。版权所有(C)2013,JPO&INPIT
    • 9. 发明专利
    • Brush grinding device
    • 刷磨机
    • JP2012218080A
    • 2012-11-12
    • JP2011083491
    • 2011-04-05
    • Honda Motor Co Ltd本田技研工業株式会社
    • KIMURA TAKEHISAYAGASAKI TORUAOYAMA HIDEAKIMITA KAZUYUKI
    • B24B29/00B24D13/14
    • PROBLEM TO BE SOLVED: To provide a brush grinding device capable of not only preventing degradation of a binding force at a tip end due to self-wear of a grinding brush, but also preventing degradation of elasticity to perform grinding work, even if an initial full length dimension of the grinding brush is relatively long.SOLUTION: A brush housing member 5 is provided, which houses the brush while covering an outer circumference of the grinding brush 3 to regulate deflection and projects the tip end of the grinding brush 3. A brush holder 2 and the grinding brush 3 in the brush housing member 5 are coupled with a brush shaft 4. A binding force varying means 8 is provided, which varies the binding force to the grinding brush 3 by scaling a diameter of a lower-end opening of the brush housing member 5. When binding of the grinding brush 3 by the binding force varying means 8 is released, the grinding brush 3 is pushed out of the brush housing member 5 by the brush shaft 4.
    • 要解决的问题:提供一种刷磨装置,其不仅能够防止由于研磨刷的自磨损导致的尖端的结合力的劣化,而且能够防止弹性降低,进行磨削加工,甚至 如果研磨刷的初始全长尺寸相对较长。 解决方案:设置电刷容纳构件5,其容纳电刷,同时覆盖研磨刷3的外周,以调节偏转并使研磨刷3的尖端突出。电刷架2和研磨刷3 在电刷容纳构件5中与刷轴4联接。提供了结合力改变装置8,其通过缩放电刷容纳构件5的下端开口的直径来改变与研磨刷3的结合力。 当解除了通过结合力改变装置8将研磨刷3粘合时,磨刷3被刷轴4从刷子壳体5推出。(C)2013,JPO&INPIT
    • 10. 发明专利
    • Perimeter correcting method for plastically deformable ring
    • JP2004017071A
    • 2004-01-22
    • JP2002173343
    • 2002-06-13
    • Honda Motor Co Ltd本田技研工業株式会社
    • NAGAO YUICHITAKAHASHI TOMOJIKIMURA TAKEHISATAKENAKA OSAMU
    • B21D1/10B21D53/14
    • PROBLEM TO BE SOLVED: To provide a perimeter correcting method which can reduce a variation in the perimeter after the correction.
      SOLUTION: This perimeter correcting method includes a first step of correcting the perimeter of a first group of rings based on an initial elongation level and then measuring the perimeters as the first corrected perimeter, determining the average of the perimeters as a first average, determining the difference of the average from a desired perimeter to provide a first perimeter difference, and adding the correction level based on the first perimeter difference to the initial elongation level to determine a first correction elongation level, and a second step of correcting the perimeter of a second group of rings based on the first correcting elongation level, determining second corrected perimeters on the assumption that the perimeter has been corrected based on the initial elongation level, determining the average of the perimeters as a second average, determining the average of the first and second averages to provide a total average, determining the difference of the total average from the desired perimeter to provide a second perimeter difference, and adding the correction level based on the second perimeter difference to the initial elongation level to provide a second correction elongation level. The second average is obtained by subtracting the correction level based on the first perimeter difference from the average of corrected perimeters of the second group of rings which have been corrected based on the first corrected elongation level. The second step is repeated.
      COPYRIGHT: (C)2004,JPO