    • 9. 发明公开
    • PROCESS FOR PRODUCTION OF ALUMINUM ALLOY FORMINGS, ALUMINUM ALLOY FORMINGS AND PRODUCTION SYSTEM
    • VERFAHREN ZUR HERSTELLUNG VON ALUMINIUMLEGIERUNGSFORMLINGEN,ALUMINIUMGELIERUNGSFORMLINGE UND PRODUKTIONSSYSTEM
    • EP2048259A1
    • 2009-04-15
    • EP07792004.9
    • 2007-07-31
    • Showa Denko K.K.
    • OKAMOTO, Yasuo
    • C22F1/043B21J5/00C22C21/02B22D11/00B22D11/18B22D11/20C22F1/00
    • B22D11/045B21J1/02B21J5/00B21K1/18B22D11/003B22D21/007C22C21/02C22F1/00C22F1/043F02F3/0084F05C2201/021
    • The present invention are to provide a method for producing an aluminum-alloy shaped product that exhibits high-temperature mechanical strength superior to that of a conventional aluminum-alloy forged product.
      The present invention provides a method for producing an aluminum-alloy shaped product, comprising a step of forging a continuously cast rod of aluminum-alloy serving as a forging material, in which the aluminum-alloy contains Si in an amount of 10.5 to 13.5 mass %, Cu in an amount of 2.5 to 6 mass %, Mg in an amount of 0.3 to 1.5 mass % and Ni in an amount of 0.8 to 4%, and satisfies a relational expression of "Ni (% by mass) ≥ (-0.68 × Cu(% by mass)+4.2(% by mass)),and heat treatment and heating steps including a step of subjecting the forging material to pre-heat treatment (82), a step (87) of heating the forging material during a course of forging of the forging material and a step of subj ecting an aluminum-alloy shaped product to post-heat treatment (89), said pre-heat treatment(82) including treatment of maintaining the forging material at a temperature of -10 to 480°C for two to six hours.
    • 本发明提供一种铝合金成形品的制造方法,该铝合金成形品的高温机械强度优于常规的铝合金锻造品。 本发明提供一种铝合金成形体的制造方法,其特征在于,包括锻造铝合金的连续铸造棒作为锻造材料的步骤,其中所述铝合金含有10.5〜13.5质量%的Si %,Cu为2.5〜6质量%,Mg为0.3〜1.5质量%,Ni为0.8〜4%,满足“Ni(质量%)‰”( -0.68×Cu(质量%)+4.2(质量%))和包括对锻造材料进行预热处理的步骤(82)的热处理和加热步骤,加热锻造的步骤(87) 锻造材料的锻造过程中的材料以及将铝合金成形体产品进行后热处理的步骤(89),所述预热处理(82)包括将锻造材料保持在温度为 -10至480℃2至6小时。