    • PROCESS FOR PRODUCING POLYPHENYLENE SULFIDE FILAMENT YARNS
    • 生产聚苯硫醚丝线的方法
    • EP1863958A1
    • 2007-12-12
    • EP06723415.3
    • 2006-03-14
    • Diolen Industrial Fibres B.V.
    • KRINS, BastianFEIJEN, Henricus, Hubertus, WilhelminusHEUZEVELDT, PeterVIETH, ChristianELBERT, Rudolf
    • D01F6/76D01D5/088
    • D01F6/765Y10T428/249922
    • The present invention relates to a process for producing a polyphenylene sulfide multifilament yarn, a polyphenylene sulfide multifilament yarn and the use of a polyphenylene sulfide multifilament yarn. The process for producing a polyphenylene sulfide multifilament yarn is characterized in that only after time period between 0,1 sec and 0,3 sec after leaving the spinneret the filaments of the spun yarn are subjected to an active cooling stage. The Polyphenylene sulfide multifilament yam having a filament linear density of 5 dtex to 30 dtex, an overall linear density of 500 dtex to 2500 dtex, a breaking tenacity in the range of 50 cN/tex to 80 cN/tex and an elongation at break of 8% to 16% for a yarn with a breaking tenacity in the range of 60 cN/tex to 80 cN/tex and an elongation at break of 16% to 30% for a yam with a breaking tenacity in the range of 50 cN/tex to 60 cN/tex.
    • 聚苯硫醚复丝纱线,聚苯硫醚复丝纱线以及聚苯硫醚复丝纱线的用途技术领域本发明涉及聚苯硫醚复丝纱线,聚苯硫醚复丝纱线以及聚苯硫醚复丝纱线的用途。 生产聚苯硫醚复丝纱线的方法的特征在于,只有在离开喷丝头后0.1秒和0.3秒之间的时间段之后,细纱的长丝才进入活动冷却阶段。 所述聚苯硫醚复丝纱线具有5dtex至30dtex的丝线密度,500dtex至2500dtex的总线密度,50cN / tex至80cN / tex范围内的断裂强度和 对于断裂强度为60cN / tex至80cN / tex范围内的纱线和断裂伸长率在50cN / tex范围内的纱线具有16%至30%的断裂伸长率的8%至16% tex至60cN / tex。