    • METHOD FOR PRODUCING POLYPROPYLENE RESIN FOAM PARTICLES
    • EP4339232A1
    • 2024-03-20
    • EP22875631.8
    • 2022-08-16
    • JSP Corporation
    • HIRA AkinobuNOHARA Tokunobu
    • C08J9/18
    • Provided is a method for producing polypropylene-based resin expanded beads containing a post-consumer recycled material of a polypropylene-based resin foamed molded article containing carbon black in order to enable provision of a black expanded beads molded article excellent in appearance and physical properties using a post-consumer recycled material of a polypropylene-based resin foamed molded article containing carbon black.
      The method for producing polypropylene-based resin expanded beads includes: a mixing step of melt-mixing a polypropylene-based resin having a melt flow rate of 1 g/10 min or more and 15 g/10 min or less at 230°C under a load of 2.16 kg and a polypropylene-based resin recovered materials comprising of a recovered materials of a post-consumer recycled material of a polypropylene-based resin foamed molded article with an extruder to obtain a mixture; an extrusion step; and a foaming step, wherein in the mixture, a blending ratio of the polypropylene-based resin is 30 wt% or more and 90 wt% or less, and a blending ratio of the polypropylene-based resin recovered materials is 10 wt% or more and 70 wt% or less (herein, a total of the polypropylene-based resin and the polypropylene-based resin recovered materials is 100 wt%), the polypropylene-based resin recovered materials contains carbon black, and a content ratio of the carbon black in the polypropylene-based resin recovered materials is 0.5 wt% or more and 5 wt% or less, a melting point of the polypropylene-based resin recovered materials is 135°C or higher and 160°C or lower, a melt flow rate of the polypropylene-based resin recovered materials at 230°C under a load of 2.16 kg is higher than a melt flow rate of the polypropylene-based resin at 230°C under a load of 2.16 kg, and a difference between the melt flow rate of the polypropylene-based resin recovered materials and the melt flow rate of the polypropylene-based resin (melt flow rate of polypropylene-based resin recovered materials - melt flow rate of polypropylene-based resin) is 0.1 g/10 min or more and 12 g/10 min or less.