    • 2. 发明公开
    • PROPYLENE-BASED RESIN FOAM PARTICLE AND FOAM PARTICLE MOLDED BODY
    • PROPYLENBASIERTE HARZSCHAUMPARTIKELFORMKÖRPERAUS SCHAUMPARTIKEL
    • EP3095811A1
    • 2016-11-23
    • EP14879190.8
    • 2014-12-24
    • JSP CORPORATION
    • ONO, MichitoshiKITAHARA, TaizoTSURUGAI, Kazuo
    • C08J9/16
    • The present invention is concerned with expanded propylene resin beads including a core layer being in a foamed state and constituted of a propylene-based resin composition (a) and a cover layer constituted of an olefin-based resin (b), the propylene-based resin composition (a) satisfying the following (i) and (ii), and the olefin-based resin (b) satisfying the following (iii) or (iv).
      (i) A mixture of 75% by weight to 98% by weight of a propylene-based resin (a1) having a melting point of 100°C to 140°C and 25% by weight to 2% by weight of a propylene-based resin (a2) having a melting point of 140°C to 165°C.
      (ii) A difference between the melting point of the resin (a2) and the melting point of the resin (a1) is 15°C or more.
      (iii) A crystalline olefin-based resin having a melting point TmB that is lower than a melting point TmA of the composition (a) and having a relation of 0°C
      (iv) A non-crystalline olefin-based resin having a softening point TsB that is lower than TmA and having a relation of 0°C
    • 本发明涉及包括发泡状态的芯层和由丙烯类树脂组合物(a)构成的发泡丙烯树脂珠和由烯烃类树脂(b)构成的覆盖层,丙烯类 满足以下(i)和(ii)的树脂组合物(a)和满足以下(iii)或(iv)的烯烃类树脂(b)。 (i)75重量%〜98重量%的熔点为100〜140℃的丙烯系树脂(a1)和25重量%〜2重量%的丙烯 - (a2),熔点为140℃〜165℃。 (ii)树脂(a2)的熔点和树脂(a1)的熔点之间的差为15℃以上。 (iii)具有低于组合物(a)的熔点TmA的熔点TmB并且具有0℃<[TmA-TmB]‰80℃的结晶烯烃类树脂。 (iv)软化点TsB低于TmA并具有0℃<[TmA-TsB]‰100℃的非结晶烯烃类树脂。
    • 4. 发明公开
    • PROPYLENE RESIN FOAMED PARTICLE AND FOAMED PARTICLE MOLDED BODY
    • 丙烯树脂泡沫颗粒和泡沫颗粒模塑体
    • EP3309197A1
    • 2018-04-18
    • EP16824474.7
    • 2016-07-13
    • JSP Corporation
    • KITAHARA, TaizoONO, MichitoshiTSURUGAI, Kazuo
    • C08J9/18
    • C08J9/232C08J9/18C08J2323/10C08K5/0066C08K5/01C08K5/02C08K5/136C08L2205/025
    • The present invention is concerned with expanded propylene resin beads including a core layer being in a foamed state, having a tubular shape, and being constituted of a propylene-based resin composition (a) satisfying the following (i) and (ii) and a cover layer being constituted of an olefin-based resin (b) satisfying the following (iii) or (iv).
      (i) A mixture of 75% by weight to 98% by weight of a propylene-based resin (a1) having a melting point of 100°C to 140°C and 25% by weight to 2% by weight of a propylene-based resin (a2) having a melting point of 140°C to 165°C.
      (ii) A difference between the melting point of the resin (a2) and the melting point of the resin (a1) is 15°C or more.
      (iii) A crystalline olefin-based resin having a melting point TmB that is lower than a melting point TmA of the composition (a) and having a relation of 0°C
      (iv) A non-crystalline olefin-based resin having a softening point TsB that is lower than TmA and having a relation of 0°C
    • 本发明涉及一种发泡丙烯类树脂珠,该发泡丙烯类树脂珠包含发泡状的芯层,该芯层呈管状,并且由满足以下(i)和(ii)的丙烯类树脂组合物(a)和 覆盖层由满足以下(iii)或(iv)的烯烃类树脂(b)构成。 (i)将75重量%〜98重量%的熔点为100℃〜140℃的丙烯系树脂(a1)和25重量%〜2重量%的丙烯系树脂 (a2),熔点为140℃〜165℃。 (ii)树脂(a2)的熔点与树脂(a1)的熔点之差为15℃以上。 (iii)熔点TmB低于组合物(a)的熔点TmA且具有0℃<[TmA-TmB]≤80℃的关系的结晶烯烃基树脂。 (iv)软化点TsB低于TmA且具有0℃<[TmA-TsB]≤100℃的关系的非晶性烯烃类树脂。