    • 9. 发明公开
    • PROPYLENE RESIN FOAM PARTICLES AND FOAM PARTICLE MOLDED ARTICLE
    • 丙烯树脂泡沫颗粒和泡沫颗粒模塑制品
    • EP3243868A1
    • 2017-11-15
    • EP15876892.9
    • 2015-01-09
    • JSP Corporation
    • OIKAWA, MasaharuKOSHITA, NobumasaTAKAGI, Syouta
    • C08J9/18C08J9/228
    • C08J9/228C08J9/0061C08J9/122C08J9/16C08J9/22C08J9/232C08J2203/06C08J2323/16C08J2423/08C08J2423/16C08L23/16C08L2205/025
    • Provided is an expanded propylene resin bead including a core layer in a foamed state, which includes a propylene-based resin composition (a) satisfying the following (i) and (ii); and a cover layer which includes an olefin-based resin (b) satisfying the following (iii) or (iv):
      (i) the propylene-based resin composition (a) is a mixture of 65% by weight to 98% by weight of a propylene-based resin (a1) having a melting point of 145°C to 165°C and a flexural modulus of 1,200 MPa or more and 35% by weight to 2% by weight of a propylene-based resin (a2) having a melting point of 100°C to 145°C and a flexural modulus of 800 MPa to 1,200 MPa;
      (ii) a difference in a melting point between the resin (a1) and the resin (a2) is 5°C to 25°C;
      (iii) the olefin-based resin (b) is a crystalline olefin-based resin having a melting point (TmB) that is lower than a melting point (TmA) of the composition (a) and being in a relation of (0°C
      (iv) the olefin-based resin (b) is a non-crystalline olefin-based resin having a softening point (TsB) that is lower than the TmA and being in a relation of (0°C
    • 提供一种包含发泡状态的芯层的丙烯系树脂发泡粒子,其含有满足下述(i)和(ii)的丙烯系树脂组合物(a)。 (iii)或(iv)的烯烃系树脂(b)的覆盖层:(i)丙烯系树脂组合物(a)为65重量%〜98重量% 的熔点为145℃〜165℃,弯曲弹性模量为1200MPa以上且35重量%〜2重量%的丙烯类树脂(a2)的丙烯类树脂(a1) 熔点为100℃至145℃,挠曲模量为800MPa至1200MPa; (ii)树脂(a1)和树脂(a2)的熔点差为5℃〜25℃, (iii)烯烃类树脂(b)为结晶性烯烃类树脂,其熔点(TmB)低于组合物(a)的熔点(TmA),且为(0° C <[TmA-TmB]≤80°C); (iv)烯烃类树脂(b)为软化点(TsB)低于TmA且处于(0℃<[TmA-TsB]的关系的非结晶烯烃类树脂, ≤100°C)。