会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 2. 发明授权
    • Composite magnetic member, process for producing the member and electromagnetic valve using the member
    • 复合磁性构件,用于制造构件的方法和使用该构件的电磁阀
    • US06187459B1
    • 2001-02-13
    • US09149082
    • 1998-09-08
    • Yoshitada KatayamaKeizo TakeuchiToshiaki TeradaShinya SugiuraHakaru SasakiTsutomu Inui
    • Yoshitada KatayamaKeizo TakeuchiToshiaki TeradaShinya SugiuraHakaru SasakiTsutomu Inui
    • G11B566
    • H01F1/147B60T8/3615C21D8/12C21D8/1294F15B13/044F16K31/06H01F1/0302H01F1/0306H01F1/047H01F7/081Y10S428/90
    • A metallic member including not more than 0.6% C, 12 to 19% Cr, 6 to 12% Ni, not more than 2% Mn, not more than 2% Mo, not more than 1% Nb and the balance being Fe and inevitable impurities, where Hirayama's equivalent H eq=[Ni %]+1.05 [Mn %]+0.65 [Cr %]+0.35 [Si %]+12.6 [C %] is 20 to 23%; Nickel equivalent Ni eq=[Ni %]+30 [C %]+0.5 [Mn %] is 9 to 12%, and Chromium equivalent Cr eq=[Cr %]+[Mo %]+1.5 [Si %]+0.5 [Nb %] is 16 to 19, wherein % is by weight, is made to have at least one ferromagnetized part having a magnetic flux density B4000 of not less than 0.3T and at least one non-magnetized part having a relative magnetic permeability &mgr; of not more than 1.2 at a temperature of not less than −40° C., as continuously and integrally formed. The non-magnetized part has crystal grain sizes of not more than 30 &mgr;m. The metallic member is subjected to by ferromagnetization and successive local non-magnetization of part or parts of the ferromagnetized member, and the thus obtained composite magnetic member is employed as a support member such as a sleeve in electromagnetic valves.
    • 包含不超过0.6%C,12-19%Cr,6-12%Ni,不大于2%Mn,不超过2%Mo,不大于1%Nb和余量为Fe和不可避免的金属构件 杂质,其中日山的等效H eq = [Ni%] + 1.05 [Mn%] + 0.65 [Cr%] + 0.35 [Si%] + 12.6 [C%]为20〜23%;镍当量Ni eq = [Ni% +30 [C%] +0.5 [Mn%]为9〜12%,铬当量Cr eq = [Cr%] + [Mo%] + 1.5 [Si%] +0.5 [Nb%]为16〜19, %的重量比被制成具有磁通密度B4000至少为0.3T的至少一个铁磁性部分和至少一个在非温度下的相对导磁率μ不大于1.2的非磁化部分 小于-40℃,连续地和一体地形成。 非磁化部件的晶粒尺寸不超过30μm。 金属构件通过铁磁性和铁磁性构件的一部分或多个部分的连续的局部非磁化受到影响,由此获得的复合磁性构件用作诸如电磁阀中的套筒的支撑构件。
    • 4. 发明授权
    • High-strength stainless steel for use as material of fuel injection
nozzle or needle for internal combustion engine, fuel injection nozzle
made of the stainless steel
    • 高强度不锈钢用作燃油喷嘴或内燃机针,不锈钢燃油喷嘴
    • US5492573A
    • 1996-02-20
    • US229005
    • 1994-04-18
    • Katsuaki FukushimaToshio OkunoMasakazu ItoKeizo TakeuchiToshiaki Terada
    • Katsuaki FukushimaToshio OkunoMasakazu ItoKeizo TakeuchiToshiaki Terada
    • C22C38/00C22C38/26C22C38/30F02M61/16F02M61/18C22C38/22
    • F02M61/166C22C38/26C22C38/30
    • A high-strength stainless steel for use as a material of a fuel injection nozzle or a fuel injection needle of an internal combustion engine. The stainless steel is an as annealed martensitic stainless steel which exhibits a hardness not less than HRC 58 after quenching and tempering heat-treatment. The limit swaging ratio of said as annealed martensitic stainless steel is not less than 75%. The hardness of said as annealed martensitic stainless steel is not higher than HB 157. Preferably, the number of carbides having sizes of 0.2 .mu.m or less occupies not more than 50% of the total carbides, and wherein the limit swaging ratio of said as annealed martensitic stainless steel is not less than 75% or the hardness of said as annealed martensitic stainless steel is not higher than HB 157. Preferably, the stainless steel has a chemical composition containing, by weight: 0.4 to 0.6% of C; not more than 0.5% of Si; not more than 0.5% of Mn; 8.0 to 13.0% of Cr; 0.1 to 2.0% of one or both of W and Mo in terms of W/2+Mo; one or both of 0.05 to 1.0% of one or both of Nb and V in terms of Nb/2+V, and 0.2 to 2.0% of Co; and the balance substantially Fe and incidental impurities.
    • 一种高强度不锈钢,用作燃料喷嘴或内燃机的燃料喷射针的材料。 不锈钢是退火马氏体不锈钢,淬火回火热处理后的硬度不低于HRC 58。 所述退火马氏体不锈钢的极限锻压比不小于75%。 所述退火的马氏体系不锈钢的硬度不高于HB157。优选地,尺寸为0.2μm以下的碳化物的数量不超过总碳化物的50%,并且其中所述作为退火的马氏体不锈钢的极限锻造比 退火的马氏体不锈钢不小于75%,或者所述退火的马氏体不锈钢的硬度不高于HB157。优选地,不锈钢具有以重量计含有:C = 0.4-0.6%的化学组成; 不超过0.5%的Si; 不超过0.5%的Mn; 8.0〜13.0%的Cr; 以W / 2 + Mo计,W和Mo中的一种或两种为0.1〜2.0% 以Nb / 2 + V表示的Nb和V中的一种或两种中的一种或两种中的一种或两种,以及Co的0.2〜2.0% 余量基本上是Fe和杂质。