    • Polyester type powder coating composition
    • 聚酯型粉末涂料组合物
    • US4180652A
    • 1979-12-25
    • US878445
    • 1978-02-16
    • Sumitaka NogamiYoshio MatsumotoKeiichi WakiTooru Okada
    • Sumitaka NogamiYoshio MatsumotoKeiichi WakiTooru Okada
    • C08G63/21C08G63/50C08G63/553C08G63/66C08G63/682C09D167/00C08G63/76
    • C08G63/682C08G63/21C08G63/50C08G63/553C08G63/66C09D167/00Y10S524/904
    • A novel polyester type powder coating composition which includes a specific self-hardening polyester of air-hardening type comprising as main ester-constituting monomer units, (1) at least one polycarboxylic acid component containing at least 10 mole %, based on the polycarboxylic acid component, of at least one aromatic polycarboxylic acid component (A) and (2) at least one polyhydric alcohol component, having in its main chain at least one terminal blocked with a monofunctional unsaturated alicyclic compound component (B) and having a softening point of 30.degree. to 150.degree. C. This composition is excellent in storage stability and adaptability to either thin coating or thick coating, and when it is applied onto an article to be coated and baked at a temperature of 170.degree. to 230.degree. C. for 5 to 30 minutes, a coating excellent in appearance, mechanical strength, gloss and reflection sharpness can be formed advantageously without generating undesired gases at the baking.
    • 一种新型聚酯型粉末涂料组合物,其包含包含作为主要酯构成单体单元的空气硬化型的特定自硬化聚酯,(1)至少一种含有至少10摩尔%的多元羧酸组分,基于多元羧酸 组分,至少一种芳族多元羧酸组分(A)和(2)至少一种多元醇组分,其主链中至少有一个末端用单官能不饱和脂环族化合物组分(B)封端并具有软化点 30℃至150℃。该组合物的储存稳定性和薄涂层或厚涂层的适应性优异,并且当其施加到待涂覆的制品上并在170℃至230℃的温度下烘烤5次 至30分钟,可以有利地形成外观优异,机械强度,光泽度和反射锐度的涂层,而不会在烘烤时产生不期望的气体。