    • 6. 发明专利
    • Method of manufacturing optical fiber
    • 制造光纤的方法
    • JP2010155780A
    • 2010-07-15
    • JP2010048758
    • 2010-03-05
    • Mitsubishi Cable Ind Ltd三菱電線工業株式会社
    • YAMAMOTO TETSUYAKIN SEICHINNAGAE NOBUSADAIKEDA YOSHIAKI
    • C03B37/018C03B8/04G02B6/00
    • C03B37/01807C03B2201/32
    • PROBLEM TO BE SOLVED: To provide a method of reducing a loss by contamination of impurities in an optical fiber. SOLUTION: This method of manufacturing an optical fiber includes a base material manufacturing process in which an optical fiber base material is manufactured by MCVD method, and a wiredrawing process in which the optical fiber base material made in the base material manufacturing process is wire-drawn. In the base material manufacturing process, in which Al-doped vitrified SiO 2 is heaped in a quartz tube P by heating by supplying SiCl 4 gas and O 2 gas together with AlCl 3 gas via a piping 61 which is formed with a metal containing iron, the temperature of the piping 61 which supplies AlCl 3 gas is set at a temperature not higher than 215°C. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供通过污染光纤中的杂质来减少损失的方法。 解决方案:这种制造光纤的方法包括其中通过MCVD方法制造光纤基材的基材制造工艺和其中在基材制造过程中制成的光纤基材的拉丝工艺 拉线。 在通过供给SiCl 4 气体和O 2气体的加热在石英管P中堆积Al掺杂的玻璃化SiO 2 SBS的基材制造方法中, / SB>气体与AlCl 3气体通过由含有铁的金属形成的配管61连接,将供给AlCl 3气体的配管61的温度设定为 温度不高于215°C。 版权所有(C)2010,JPO&INPIT
    • 7. 发明专利
    • Method for manufacturing optical fiber preform
    • 制造光纤预制件的方法
    • JP2003054974A
    • 2003-02-26
    • JP2001251825
    • 2001-08-22
    • Mitsubishi Cable Ind Ltd三菱電線工業株式会社
    • ITO HIDEAKIKIN MASATAKANAGAE NOBUSADA
    • G02B6/00C03B37/012
    • C03B37/01211Y02P40/57
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing an optical fiber preform in which the surface of a quartz rod is cleaned and the quartz rod is put in a quartz pipe while keeping the cleaned state. SOLUTION: A quartz rod 2 obtained by drawing a soot sintered compact is inserted in an auxiliary pipe 12 and a quartz pipe 11 while cleaning the surface of the quartz rod 2 by polishing with a flame 21. Flame polishing is gradually carried out from the tip of the quartz rod 2 to be inserted first toward the upper part and the flame-polished part is quickly put in the auxiliary pipe 12 and the quartz pipe 11 as it is. The quartz rod 2 is therefore inserted in the quartz pipe 11 while keeping the cleaned state of the surface and the objective high quality optical fiber preform is obtained.
    • 要解决的问题:提供一种在保持清洁状态的同时清洁石英棒的表面并将石英棒放入石英管中的光纤预制件的制造方法。 解决方案:通过拉制烟灰烧结体获得的石英棒2通过用火焰21进行抛光来清洁石英棒2的表面,同时插入辅助管12和石英管11中。火焰抛光从尖端 将石英棒2首先插入上部并且将火焰抛光部分迅速地放入辅助管12和石英管11中。 因此,石英棒2被插入石英管11中,同时保持表面的清洁状态并获得目标高质量的光纤预制件。