热词
    • 3. 发明专利
    • Method for manufacturing optical fiber preform
    • 制造光纤预制件的方法
    • JP2003054974A
    • 2003-02-26
    • JP2001251825
    • 2001-08-22
    • Mitsubishi Cable Ind Ltd三菱電線工業株式会社
    • ITO HIDEAKIKIN MASATAKANAGAE NOBUSADA
    • G02B6/00C03B37/012
    • C03B37/01211Y02P40/57
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing an optical fiber preform in which the surface of a quartz rod is cleaned and the quartz rod is put in a quartz pipe while keeping the cleaned state. SOLUTION: A quartz rod 2 obtained by drawing a soot sintered compact is inserted in an auxiliary pipe 12 and a quartz pipe 11 while cleaning the surface of the quartz rod 2 by polishing with a flame 21. Flame polishing is gradually carried out from the tip of the quartz rod 2 to be inserted first toward the upper part and the flame-polished part is quickly put in the auxiliary pipe 12 and the quartz pipe 11 as it is. The quartz rod 2 is therefore inserted in the quartz pipe 11 while keeping the cleaned state of the surface and the objective high quality optical fiber preform is obtained.
    • 要解决的问题:提供一种在保持清洁状态的同时清洁石英棒的表面并将石英棒放入石英管中的光纤预制件的制造方法。 解决方案:通过拉制烟灰烧结体获得的石英棒2通过用火焰21进行抛光来清洁石英棒2的表面,同时插入辅助管12和石英管11中。火焰抛光从尖端 将石英棒2首先插入上部并且将火焰抛光部分迅速地放入辅助管12和石英管11中。 因此,石英棒2被插入石英管11中,同时保持表面的清洁状态并获得目标高质量的光纤预制件。
    • 7. 发明专利
    • Optical fiber
    • 光纤
    • JP2005148116A
    • 2005-06-09
    • JP2003381002
    • 2003-11-11
    • Mitsubishi Cable Ind Ltd三菱電線工業株式会社
    • OIZUMI SEIROKIN MASATAKAKAWAGISHI MASANORIIMAMURA KAZUOKANEKO TAKASHI
    • G02B6/028G02B6/18
    • PROBLEM TO BE SOLVED: To provide an optical fiber capable of exhibiting superior characteristics (loss characteristic or the like) even if it is bent with a radius of curvature of ≤30 mm. SOLUTION: The optical fiber is provided with a core 2 and a clad 3 in which a refractive index distribution coefficient g is in the range of 1≤g≤3 and in which the refractive index gently varies along the radius direction. The diameter of the core 2 and that of the clad 3 are set at 50 μm and 125 μm respectively. The relative index difference (Δ) between the core 2 and the clad 3 is set at 1.5% COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:即使弯曲曲率半径≤30mm,也能够提供能够表现出优异特性(损耗特性等)的光纤。 解决方案:光纤设置有芯2和折射率分布系数g在1≤g≤3的范围内并且折射率沿着半径方向轻微变化的包层3。 芯2的直径和包层3的直径分别设定为50μm和125μm。 芯2和包层3之间的相对折射率差(Δ)设定为1.5%<Δ<2.3%。 为了减小曲率半径并且保持物理强度,使用了具有≥1.3%的筛选失真特性的光纤。 版权所有(C)2005,JPO&NCIPI