    • 5. 发明申请
    • Thermoplastic elastomer composition and process for producing the same and pneumatic tire and hose using the same
    • 热塑性弹性体组合物及其制造方法及使用其的充气轮胎和软管
    • US20050103417A1
    • 2005-05-19
    • US11008962
    • 2004-12-13
    • Jiro WatanabeYuichi HaraShigeru YamauchiHideo Nemoto
    • Jiro WatanabeYuichi HaraShigeru YamauchiHideo Nemoto
    • B60C1/00C08L23/02C08L23/28C08L77/00B60C5/12B60C5/14
    • C08L23/02B60C1/00B60C1/0008C08L23/283C08L77/00C08L2312/00Y10T152/10495C08L2666/04C08L2666/20
    • A thermoplastic elastomer composition dynamically vulcanized to a gelation rate of 50 to 95% which is superior in heat resistance and durability while maintaining flexibility and superior in air permeation preventive property which can be efficiently used as, for example, a pneumatic tire as an air permeation preventive layer. In particular, a thermoplastic elastomer composition having a reduced particle size of the domain rubber is produced by a material having a high rubber ratio by mixing a composition (C) mixed under conditions of a ratio of melt viscosities of the rubber composition (A)/resin (B) of 0.8 to 1.2 and the formula (φA/φB)×(ηB/ηA)
    • 一种热塑性弹性体组合物,其动态硫化至50至95%的凝胶化速率,其耐热性和耐久性优异,同时保持柔软性和优异的防透气性,可有效地用作例如充气轮胎作为空气渗透 预防层。 特别地,通过混合在橡胶组合物(A)/(A)的熔体粘度的比例的条件下混合的组合物(C),通过使用具有高橡胶比的材料来制造具有减小的领域橡胶粒径的热塑性弹性体组合物, 树脂(B)为0.8〜1.2,通式(i> i i i i i <<<<<<<<<<<<<<<<<<<<<<<<<<< 橡胶组合物(D)/组合物(C)的熔体粘度比为0.8〜1.2和式(phi / D / C / C)的条件下, /SUB>)x(etaC/etaD)1.0,其中橡胶组合物(A)的体积分数,phi B:树脂(B)的体积分数,ηA:橡胶组合物(A)的熔融粘度,乙烯B:树脂的熔融粘度 (B),化合物(C)的体积分数,橡胶组合物(D)的体积分数,ηC :组合物(C)的熔融粘度,η的熔体粘度:r的熔体粘度 ubber组成(D)。 另外,具有作为分散相的弹性体组合物(A)和热塑性树脂组合物(B)作为基质并具有由至少两种热塑性树脂的共混物组成的热塑性树脂组合物的热塑性弹性体组合物。
    • 10. 发明申请
    • THERMOPLASTIC ELASTOMER COMPOSITION
    • 热塑性弹性体组合物
    • US20120136100A1
    • 2012-05-31
    • US13368539
    • 2012-02-08
    • Yuichi HaraNaoyuki Morooka
    • Yuichi HaraNaoyuki Morooka
    • C08K5/435C08L77/02
    • B60C1/0008C08K5/0016C08K5/435C08L23/28C08L23/283C08L77/02C08L77/06C08L77/10C08L2207/04C08L2312/00C08L2666/20
    • Provided is a thermoplastic elastomer composition, which includes a halogenated isoolefin/para-alkylstyrene copolymer rubber dispersed in a polyamide resin in order to improve the fatigue durability of a polyamide resin, while maintaining high flowability of the polyamide. A thermoplastic elastomer composition comprising a continuous phase composed of a modified polyamide resin (A) and a dispersed phase composed of a halogenated isoolefin/para-alkylstyrene copolymer rubber (B) is provided. The modified polyamide resin (A) is a resin obtained by melt-kneading 100 parts by weight of a polyamide resin (C) with not less than 0.05 part by weight and less than 3 parts by weight a compound (D), such as a monofunctional epoxy compound, capable of binding to a terminal amino group of the polyamide resin at a temperature not lower than the melting point of the polyamide resin (C). The composition can be used as an inner liner of a pneumatic tire.
    • 提供一种热塑性弹性体组合物,其包含分散在聚酰胺树脂中的卤化异烯烃/对烷基苯乙烯共聚物橡胶,以提高聚酰胺树脂的疲劳耐久性,同时保持聚酰胺的高流动性。 提供了包含由改性聚酰胺树脂(A)构成的连续相和由卤代异烯烃/对烷基苯乙烯共聚物橡胶(B)组成的分散相的热塑性弹性体组合物。 改性聚酰胺树脂(A)是通过将100重量份的聚酰胺树脂(C)以0.05重量份以上且小于3重量份的化合物(D),如 能够在不低于聚酰胺树脂(C)的熔点的温度下与聚酰胺树脂的末端氨基结合的单官能环氧化合物。 组合物可以用作充气轮胎的内衬。