    • Process for preparing polyimide solution
    • 制备聚酰亚胺溶液的方法
    • US4290936A
    • 1981-09-22
    • US092508
    • 1979-11-08
    • Yoshikazu SasakiHiroshi InoueIchiro SasakiHiroshi ItataniMikito Kashima
    • Yoshikazu SasakiHiroshi InoueIchiro SasakiHiroshi ItataniMikito Kashima
    • C08G73/10C08K5/13
    • C08G73/1028
    • A polyimide solution is prepared by a process wherein a tetracarboxylic acid ingredient containing at least about 80% by mole of 3,3',4,4'-biphenyltetracarboxylic acid or its functional derivative and an aromatic diamine ingredient containing at least about 50% by mole of 4,4'-diaminodiphenyl ether are polymerized at from about 100.degree. to 300.degree. C. in phenol or a halogenated phenolic compound; the amount of the acid and diamine ingredients being approximately equimolar to each other; whereby polymerization of the tetracarboxylic acid ingredient and the aromatic diamine ingredient is effected while being accompanied by imidation. Preferably, the polymerization accompanied by imidation is effected in a manner such that at least a second half of the polymerization is carried out in a closed reaction system. The resulting polyimide solution is suitable for making therefrom shaped articles, such as films, possessing excellent mechanical properties.
    • 通过以下方法制备聚酰亚胺溶液,其中含有至少约80摩尔%的3,3',4,4'-联苯四羧酸或其官能衍生物的四羧酸成分和包含至少约50%的芳族二胺成分 摩尔的4,4'-二氨基二苯醚在苯酚或卤化酚类化合物中在约100-300℃下聚合; 酸和二胺成分的量彼此近似等摩尔数; 从而在伴随着酰亚胺化的同时进行四羧酸成分和芳香族二胺成分的聚合。 优选地,伴随着酰亚胺化的聚合以这样的方式进行,使得聚合的至少一半在闭合反应体系中进行。 所得到的聚酰亚胺溶液适用于具有优异机械性能的成型制品如膜。
    • 10. 发明申请
    • Solution compositions of block copolyimides comprising pyromellitic dianhydride and process for production thereof
    • 包含1,2,4,5-苯四酸二酐的嵌段共聚酰亚胺的溶液组合物及其制备方法
    • US20060004180A1
    • 2006-01-05
    • US10531165
    • 2003-02-28
    • Hiroshi Itatani
    • Hiroshi Itatani
    • C08G69/08
    • C08G73/1042C08G73/1021C08G73/1032C08L79/08
    • Polyimides consisting of PMDA and an aromatic diamine are normally solvent-insoluble. According to the present invention, they are solubilized in solvents to prepare four-component or higher block copolymers containing BTDA. PMDA is reacted with a certain type of aromatic diamine in a molar ratio of 1:2-1.5 to produce a solvent-soluble oligomer. This is combined with an acid dianhydride and an aromatic diamine to produce a four-component or higher solvent-soluble block copolymer. The molar ratio of the aromatic diamine added with PMDA is 1:2-1.5. A number of solvent-soluble block copolymers containing PMDA can be prepared. Four-component or higher polyimide block copolymers containing PMDA, BTDA, and DAT are prepared by sequential reactions in the presence of a binary catalyst. This made it possible to prepare various polyimides from many inexpensively available materials. Polyimides containing PMDA-BTDA-DAT can be prepared at high performance, in mass and at low cost by using economical direct imidation, and therefore can be widely used in future.
    • 由PMDA和芳族二胺组成的聚酰亚胺通常是溶剂不溶性的。 根据本发明,将它们溶解在溶剂中以制备含有BTDA的四组分或更高的嵌段共聚物。 PMDA与某种类型的芳族二胺以1:2-1.5的摩尔比反应,生成溶剂可溶的低聚物。 将其与酸二酐和芳族二胺组合以产生四组分或更高溶剂可溶性嵌段共聚物。 加入PMDA的芳族二胺的摩尔比为1:2-1.5。 可以制备多种含有PMDA的溶剂可溶性嵌段共聚物。 含有PMDA,BTDA和DAT的四组分或更高级的聚酰亚胺嵌段共聚物通过在二元催化剂存在下的顺序反应来制备。 这使得可以从许多廉价的材料制备各种聚酰亚胺。 含有PMDA-BTDA-DAT的聚酰亚胺可以通过使用经济的直接酰亚胺化以高性能,质量和低成本制备,因此可以在将来被广泛使用。