会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 7. 发明申请
    • POLYMERIZATION PROCESS PROVIDING POLYETHYLENE OF ENHANCED OPTICAL PROPERTIES
    • 提供增强光学性能的聚乙烯的聚合方法
    • WO2008137413A1
    • 2008-11-13
    • PCT/US2008/061883
    • 2008-04-30
    • FINA TECHNOLOGY, INC.GEUNTHER, GerhardGRAY, StevenCOFFY, Tim
    • GEUNTHER, GerhardGRAY, StevenCOFFY, Tim
    • C08F110/02
    • C08F10/00C08F210/16C08F4/69C08F2/14C08F210/14C08F2500/12
    • A process for the polymerization of ethylene to provide an ethylene polymer of reduced Yellowness Index. A feed stream, comprising an inert hydrocarbon diluent containing ethylene in a minor amount, is supplied to a polymerization reactor. A chromium-based polymerization catalyst and a triethylboron co-catalyst are incorporated into the feed stream within the reactor. The polymerization catalyst will normally be used in an amount within the range of 0.008-0.1 wt. % of the diluent in the feed stream and the triethylboron co-catalyst is incorporated in an amount within the range of 0.1-50 ppm of the diluent. The polymer fluff from the reactor is heated to a temperature sufficient to melt the fluff which is then extruded to produce a polymer product. The Yellowness Index after high temperature aging is at least 5% less than the corresponding Yellowness Index of a corresponding polymer product produced without the triethylboron co- catalyst.
    • 一种聚合乙烯以提供降低黄度指数的乙烯聚合物的方法。 将包含少量乙烯的惰性烃稀释剂的进料流供给到聚合反应器中。 将铬基聚合催化剂和三乙基硼助催化剂并入反应器内的进料流中。 聚合催化剂通常的用量范围为0.008-0.1wt。 进料流和三乙基硼助催化剂中稀释剂的%的掺入量在稀释剂的0.1-50ppm的范围内。 将来自反应器的聚合物绒毛加热到足以熔化绒毛的温度,然后将其挤出以产生聚合物产物。 高温老化后的黄度指数比相应的不含三乙基硼助催化剂的聚合物产物的黄度指数小至少5%。