    • Method for preventing corrosion of cast iron pipe
    • 防止铸钢管腐蚀的方法
    • JP2005342717A
    • 2005-12-15
    • JP2005178068
    • 2005-06-17
    • Dainippon Toryo Co LtdKurimoto Ltd大日本塗料株式会社株式会社栗本鐵工所
    • SAITO MASAHIKODEGUCHI TAKAAKIKAJIWARA YOSHIHISAMICHIURA YOSHISADAYAMADA YOSHIOTAME SHINICHIRO
    • F16L58/08B05D5/00B05D7/14C23C4/08C23C28/00F16L58/10
    • C23C28/00
    • PROBLEM TO BE SOLVED: To provide a method for preventing corrosion of a cast iron pipe by using a coating material which can be coated on the surface of white rust produced in outdoor temporary placing and on white rust produced in steam curing.
      SOLUTION: This method for preventing corrosion of cast iron pipe comprises the steps of (1) thermally spraying zinc, zinc-aluminum pseudoalloy, or zinc-aluminum alloy to form a thermal spray coating layer onto the outer surface of a cast iron pipe, (2) coating an aqueous two-component epoxy emulsion coating material having a solid content of not less than 5% by weight and comprising a first component of an epoxy resin having an epoxy equivalent of 475 to 1,800 and a second component of an amine curing agent having an active hydrogen equivalent (on a solid basis) of 160 to 600 onto the outer surface of the cast iron pipe to form an epoxy resin film, and (3) coating an acrylic emulsion coating material having a solid content of not less than 15% by weight on the epoxy resin film to form an acrylic resin film.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种通过使用可涂覆在户外临时放置产生的白锈表面上的涂层材料和在蒸汽固化中产生的白锈来防止铸铁管的腐蚀的方法。 解决方案:这种防止铸铁管腐蚀的方法包括以下步骤:(1)热喷锌,锌铝合金或锌铝合金,以在铸铁外表面上形成热喷涂层 管,(2)涂布固体含量不小于5重量%的水性双组分环氧乳液涂料,其包含环氧当量为475至1,800的环氧树脂的第一组分和第二组分 具有160至600的活性氢当量(基于固体)的胺固化剂在铸铁管的外表面上形成环氧树脂膜,和(3)涂覆固体含量不高的丙烯酸乳液涂料 在环氧树脂膜上小于15重量%,形成丙烯酸树脂膜。 版权所有(C)2006,JPO&NCIPI
    • 4. 发明专利
    • Corrosion-preventive structure of pipeline
    • 管道腐蚀预防结构
    • JP2014190535A
    • 2014-10-06
    • JP2013069851
    • 2013-03-28
    • Kurimoto Ltd株式会社栗本鐵工所
    • NISHIHARA YOSHIKAZUDEGUCHI TAKAAKIOTSU HIDEKINAKAMOTO KOJIYAMADA YOSHINOBUYAO MASAHIKOSHISHIDO RYO
    • F16L58/10F16L1/024F16L57/00
    • PROBLEM TO BE SOLVED: To provide a corrosion-preventive structure of pipeline which simply improves corrosion-preventive performance of buried pipeline.SOLUTION: A corrosion-preventive structure of pipeline in which an outer circumference of buried metal pipe is covered with polyethylene sleeve, adjacent edge parts of the polyethylene sleeves are overlapped with each other, a rubber band is wound around the outer circumference of overlapped part of the polyethylene sleeve and, thereby, water permeation from the edge part of the polyethylene sleeve is prevented, comprises water-absorbing swelling material disposed between the outer circumference of the pipe and the inner circumference of the rubber band. Thereby, even when water permeation occurs from the edge part of the polyethylene sleeve to the inner side, the water-absorbing swelling material is swollen, therefore, closes an advancing path of water, strengthens the tightening by means of the rubber band, stops the water permeation to the buried pipeline and can prevent corrosion of the pipeline.
    • 要解决的问题:提供简单提高埋管线路防腐蚀性能的管道防腐结构。解决方案:埋管金属管外周覆盖聚乙烯套管的管道防腐结构,相邻 聚乙烯套筒的边缘部分彼此重叠,橡胶带缠绕在聚乙烯套筒的重叠部分的外圆周上,从而防止从聚乙烯套筒的边缘部分渗透水分,包括吸水膨胀 配置在管的外周与橡胶带的内周之间的材料。 因此,即使从聚乙烯套筒的边缘部到内侧发生水渗透,吸水膨胀材料膨胀,因此封闭水的前进路径,通过橡胶带增强紧固,停止 水渗透到埋地管道,可以防止管道腐蚀。
    • 5. 发明专利
    • Coating composition for metallic pipe and metallic pipe coated with the same
    • 用于金属管和金属管的涂层组合物涂覆在其上
    • JP2014185238A
    • 2014-10-02
    • JP2013060903
    • 2013-03-22
    • Kurimoto Ltd株式会社栗本鐵工所
    • YAO MASAHIKODEGUCHI TAKAAKI
    • C09D201/00C09D133/00
    • PROBLEM TO BE SOLVED: To provide a solvent-type coating composition for a metallic pipe with a small environmental load, which can, without adversely affecting various functional demands for coating materials for metallic pipes, inhibit solvent odors and abbreviate drying time; and a metallic pipe coated with the same.SOLUTION: The provided coating composition for water-contacted portions of a metallic pipe includes a resin and a solvent, wherein the solvent does not include, as a main component, a water-insoluble, low-volatility solvent (a), but includes at least 25 wt.% of a water-soluble solvent (b), and includes no water. The coating composition preferably includes at least 3 wt.% of a high-volatility solvent (c). Also provided is a metallic pipe wherein water-contacted portions thereof are coated with the coating composition for water-contacted portions of a metallic pipe.
    • 要解决的问题:为了提供环境负荷小的金属管用溶剂型涂料组合物,可以不影响金属管涂料的各种功能性要求,抑制溶剂气味并缩短干燥时间; 和金属管,其金属管被涂覆。金属管的水接触部分的涂料组合物包括树脂和溶剂,其中溶剂不包括作为主要成分的不溶于水的低分子量水溶液, 挥发性溶剂(a),但包含至少25重量%的水溶性溶剂(b),并且不包括水。 涂料组合物优选包括至少3重量%的高挥发性溶剂(c)。 还提供了金属管,其中与金属管的水接触部分的涂料组合物涂覆有水接触部分。
    • 6. 发明专利
    • Method of coating front and back surfaces
    • 涂覆前表面和背面的方法
    • JP2010253433A
    • 2010-11-11
    • JP2009109135
    • 2009-04-28
    • Kurimoto Ltd株式会社栗本鐵工所
    • DEGUCHI TAKAAKIKACHI SHUNJINAKAMURA KENJISATO TETSUYATANIGUCHI SHINOBUOKAMURA TOSHIMASA
    • B05D3/00B05D7/22
    • PROBLEM TO BE SOLVED: To shorten the entire coating time in a method of coating front and back surfaces and to excellently coat the surface of a lower appropriate temperature. SOLUTION: After coating an inner surface 2 as the back surface of a higher appropriate temperature of the inner and outer surfaces 2 and 3 of a ductile cast iron pipe 1 as an object to be coated at the appropriate temperature of 200°C, the ductile cast iron pipe 1 is forcibly cooled to the lower appropriate temperature by spraying cooling water from cooling water nozzles 6a and 6b and blowing air from an air nozzle 7, and the outer surface 3 as the front surface of the lower appropriate temperature is coated at the appropriate temperature of 70°C. Thus, the interval time from the coating of the inner surface 2 to the coating of the outer surface 3 is shortened, and the entire coating time is shortened. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了缩短涂覆前后表面的方法的整个涂布时间,并且优良地涂覆较低适当温度的表面。 解决方案:在作为被涂物体的球墨铸铁管1的内表面和外表面2和3的较高适当温度的后表面涂覆适当温度为200℃的内表面2之后, 通过从冷却水喷嘴6a和6b喷射冷却水并从空气喷嘴7吹出空气将球墨铸铁管1强制冷却到较低的适当温度,作为适当温度较低的前表面的外表面3为 在适当的温度下涂覆70℃。 因此,从内表面2的涂布到外表面3的涂布的间隔时间缩短,整个涂布时间缩短。 版权所有(C)2011,JPO&INPIT
    • 8. 发明专利
    • Cast iron pipe applied with water-based coating on socket inner face, and method of coating the same
    • 套管内壁涂有水性涂层的铸铁管及其涂覆方法
    • JP2013204689A
    • 2013-10-07
    • JP2012074244
    • 2012-03-28
    • Kurimoto Ltd株式会社栗本鐵工所
    • YAO MASAHIKOHIROHATA SATOKODEGUCHI TAKAAKI
    • F16L58/10B05D7/22B05D7/24F16L57/00
    • PROBLEM TO BE SOLVED: To provide: a cast iron pipe applied with coating on a socket inner face of a tubular body using a water-based paint excellent in adhesion to powder coating applied to a straight tube portion of the tubular body without using a solvent; and a method of coating the cast iron pipe.SOLUTION: A cast iron pipe includes a socket on one end and an insertion port on the other end with a pipe portion therebetween. A coating layer is provided on a socket inner surface. The coating layer includes a coating film provided on the upper surface of the socket inner surface and formed by applying coating with an aqueous paint made of, as solid contents, (A) 1-15 pts.wt. of epoxy ester, (B) 5-30 pts.wt. of acrylic resin emulsion, and (C) 55-94 pts.wt. of acrylic resin dispersion, and containing (D) pigment having pigment volumetric concentration of 35-45%.
    • 要解决的问题:提供一种铸铁管,其使用在不使用溶剂的情况下使用对管状体的直管部分施加的粉末涂料的粘附性优异的水性涂料,在管状体的插座内表面上施加涂层 ; 以及涂覆铸铁管的方法。解决方案:铸铁管包括一端的插座和另一端的插入口,其间具有管部分。 在插座内表面上设置涂层。 涂层包括设置在插座内表面的上表面上的涂膜,通过涂覆由(A)为1-15重量份的固体成分制成的水性涂料而形成。 的环氧酯,(B)5-30重量份 的丙烯酸树脂乳液,(C)55-94重量份 的丙烯酸树脂分散体,并含有颜料体积浓度为35-45%的(D)颜料。
    • 9. 发明专利
    • Powder coating recovery treatment apparatus
    • 粉末涂料回收处理设备
    • JP2008126202A
    • 2008-06-05
    • JP2006317205
    • 2006-11-24
    • Kurimoto Ltd株式会社栗本鐵工所
    • OTSU HIDEKIDEGUCHI TAKAAKI
    • B05C19/06
    • PROBLEM TO BE SOLVED: To provide a powder coating recovery treatment apparatus which enhances the recovery efficiency when the metal powder included in the powder coating is removed.
      SOLUTION: The powder coating recovery treatment apparatus is characterized by incorporating the recovered powder coating W into a fluid tank 20 to maintain a fluid state and arranging a magnet 31 within the fluid tank 20 so that the metal powder included in the recovered powder coating W is removed by adsorbing the same to the magnet 31. A porous plate 22 is installed to the bottom plate of the fluid tank 20. The gas G in a gas reservoir 23 is supplied through the pores 24 of the porous plate 22 and the powder coating W is agitated. The magnet 31 is arranged on the porous plate 22. A lot of the metal powder can be adsorbed to the magnet because the chance of access of the metal powder included in the powder coating W to the magnet 31 is increased by installing the magnet 31 within the fluid tank 20. Therefor, the removal efficiency can be enhanced. Also, the transferring step and transferring working of the powder coating is simplified and the constitution of the apparatus can be simplified because the necessity to provide the removal step and removal device excluding the fluid tank 20 is eliminated.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种除去粉末涂料中包含的金属粉末时提高回收效率的粉末涂料回收处理装置。 解决方案:粉末涂料回收处理装置的特征在于将回收的粉末涂料W并入流体箱20中以保持流体状态,并将磁体31设置在流体箱20内,使得包含在回收粉末中的金属粉末 通过将其吸附到磁体31而除去涂层W.多孔板22安装在流体槽20的底板上。气体储存器23中的气体G通过多孔板22的孔24供给, 粉末涂层W被搅动。 磁体31设置在多孔板22上。由于通过将磁体31安装在磁体31内而使包含在粉末涂层W中的金属粉末进入磁体31的机会增加,所以许多金属粉末可以被吸附到磁体上 流体箱20.因此,可以提高去除效率。 此外,由于不需要提供除了流体箱20之外的除去步骤和除去装置,所以简化了粉末涂层的转印步骤和转印加工,并且可以简化装置的结构。 版权所有(C)2008,JPO&INPIT
    • 10. 发明专利
    • Lining to vessel inside
    • 内装船
    • JP2007289945A
    • 2007-11-08
    • JP2007090021
    • 2007-03-30
    • Kurimoto LtdNippon Oil CorpOhbayashi Corp新日本石油株式会社株式会社大林組株式会社栗本鐵工所
    • TAKEI YOSHIHISAFUKUI MASAOMICHIURA YOSHISADASAITO MASAHIKODEGUCHI TAKAAKIYAMADA YOSHINOBU
    • B05D7/22
    • PROBLEM TO BE SOLVED: To obtain a lining layer to the vessel inside inexpensive, and having acid resistance and abrasion resistance.
      SOLUTION: While moving a rotary Hume pipe 1 in its vessel axis direction, aggregate b and molten sulfur c are supplied to the vessel 1 inside to mix these by the rotation, and the mixture is subjected to lining a to the vessel inside using the molten sulfur c as a binder of the aggregate b. The recycling of sulfur or the like refined by desulfurization of petroleum and natural gas which are not conventionally sufficiently recycled is facilitated. Using the sulfur, a sulfur-possessed acid-resistant and abrasion-resistant vessel 1 of lining to the vessel inside can be obtained at a low cost. If the vessel 1 employs a hardly deformable vessel by strength in a diameter direction such as ductile cast iron and the Hume pipe, due to its resistance to deformation, the above-described performance can be obtained for a long period of time even in sulfur mixture lining a without toughness.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:为了在容器内部获得廉价的并具有耐酸性和耐磨性的内衬层。

      解决方案:在旋转休谟管1沿其容器轴线方向移动时,将聚集体b和熔融硫c供应到容器1内部以通过旋转进行混合,并将混合物经受衬里a到容器内部 使用熔融硫磺作为聚集体b的粘合剂。 通过不常规地充分再循环的石油和天然气的脱硫来精炼的硫等的再循环便利。 使用硫,可以以低成本获得含硫耐酸耐磨损容器1的衬里到容器内部。 如果容器1由于其耐变形性而在诸如球墨铸铁和休斯管之类的直径方向上采用几何变形的容器,所以即使在硫混合物中也可以长期获得上述性能 衬里没有韧性。 版权所有(C)2008,JPO&INPIT