    • 9. 发明授权
    • Method of making a glass encapsulated diode
    • 制造玻璃封装二极管的方法
    • US4168960A
    • 1979-09-25
    • US897323
    • 1978-04-18
    • Bulent E. Yoldas
    • Bulent E. Yoldas
    • H01L23/04H01L21/56H01L23/051H01L23/29H01L23/31
    • H01L23/3171H01L21/56H01L23/051H01L23/3107H01L2924/0002
    • A glass encapsulated semiconductor diode and a method for glass encapsulation of a fusion to form a semiconductor diode is disclosed. The fusion comprises a body of semiconductor material having a PN junction therein and metal electrodes affixed to opposed major surfaces thereof. The fusion is encircled by a ring-shaped glass member with an inner surface of the ring-shaped glass member fused to an edge surface of the body of semiconductor material to form a protective layer overlying the PN junction. The ring-shaped glass member is formed and fused to the edge of the body of semiconductor material by placing the fushion and a prefabricated glass ring, preferably cut from stress relieved glass tubing, encircling the fusion in a furnace. A weight is applied to the upper surface of the prefabricated glass ring. An atmosphere comprising a predetermined mixture of nitrogen and water vapor is established in the fusion furnace and the temperature of the fusion furnace is increased and decreased in accordance with a predetermined program to cause the prefabricated glass ring to soften and fuse to the edge surface of the body of semiconductor material to form a protective layer, comprising the ring-shaped glass member, overlying the PN junction.
    • 公开了一种玻璃封装的半导体二极管和用于融合以形成半导体二极管的玻璃封装的方法。 熔合物包括其中具有PN结的半导体材料体,并且固定在其相对的主表面上的金属电极。 熔合物被环形玻璃构件环绕,其中环形玻璃构件的内表面与半导体材料的主体的边缘表面融合,以形成覆盖PN结的保护层。 环形玻璃构件通过将缓冲垫和优选从应力释放的玻璃管切割的预制玻璃环环绕在熔炉中而形成并熔合到半导体材料的主体的边缘。 将重量施加到预制玻璃环的上表面。 在熔融炉中建立包含氮和水蒸汽的预定混合气体的气氛,并且根据预定的程序增加和减少熔炉的温度,以使预制的玻璃环软化并熔化到熔融炉的边缘表面 半导体材料体以形成保护层,包括覆盖PN结的环形玻璃构件。
    • 10. 发明授权
    • Economic preparation of alumina suitable for isostatic pressing and
sintering
    • 经济的氧化铝制备适用于等静压和烧结
    • US4357427A
    • 1982-11-02
    • US312575
    • 1981-10-19
    • Shih-Ming HoBulent E. YoldasDouglas M. Mattox
    • Shih-Ming HoBulent E. YoldasDouglas M. Mattox
    • C01F7/00C01F7/02C01F7/36C04B35/115C04B35/44
    • B82Y30/00C01F7/00C01F7/02C01F7/36C04B35/115C01P2004/52C01P2004/62C01P2004/64C01P2006/80
    • Method for preparing finely divided high purity alumina doped with a small predetermined percentage of magnesia. In the preparation, there is first formed a mixed clear solution of aluminum alkoxide and a small amount of magnesium in the form of alkoxide or water soluble magnesium salt. There is then included with the clear solution a substantial excess of water over that required to completely hydrolyze the alkoxide and there is added thereto a small amount of selected acid which is effective to peptize the resulting slurry. The formed milky slurry is then allowed to become fully peptized to form a clear sol. The clear sol is converted to a finely divided and dried powder either by forming the sol into a gel, which is then dried, and mechanically reduced to a powder status or by spray drying the sol at elevated temperatures which produces the dried powder. Thereafter, the finely divided and dried powder is calcined at a temperature of from about 700.degree. C. to about 900.degree. C., with the crystalline structure of the powder predominately being that of a delta alumina. The preparation of this alumina is very economic and the resulting material is suitable for being isostatically pressed into a tubular form and then sintered to translucent tubular form to a density which closely approaches theoretical.
    • 用于制备以预定百分比小的氧化镁掺杂的细分高纯氧化铝的方法。 在制备中,首先形成醇盐和水溶性镁盐形式的醇铝和少量镁的混合澄清溶液。 然后,与透明溶液一起包含相当于完全水解醇盐所需的水相当多的水,并且向其中加入少量选择的酸,其有效地胶化所得浆料。 然后使形成的乳状浆料变得完全胶溶以形成透明溶胶。 通过将溶胶形成凝胶然后将透明溶胶转化成细碎和干燥的粉末,然后干燥,机械还原成粉末状态,或通过在产生干燥粉末的高温下通过喷雾干燥溶胶。 此后,将细粉干燥的粉末在约700℃至约900℃的温度下煅烧,粉末的晶体结构主要为δ氧化铝。 该氧化铝的制备非常经济,所得材料适于均匀地压制成管状,然后烧结成半透明的管形,达到接近理论的密度。