    • 2. 发明公开
    • 다층구조 전도사로 이루어진 전도성 직물의 염색가공방법
    • 具有多层导电纱线的导电纺织品染色工艺
    • KR1020110031664A
    • 2011-03-29
    • KR1020090089007
    • 2009-09-21
    • (주)삼광염직다이텍연구원경북대학교 산학협력단
    • 전준형김은철이봉환김미경최우혁김태경
    • D06P1/38D06P3/80
    • D06P1/38D06P3/80
    • PURPOSE: A method for dyeing fabric containing multi-layered conductive yarn covered with nylon and cotton fiber is provided to ensure excellent color fastness and shape stability. CONSTITUTION: A method for dyeing conductive fabric containing multi-layered conductive yarn comprises: a step of mixing 8-10 g/L of hydrogen peroxide, 3-5 g/L of stabilizing agent, 2-4 g/L of refining agent, 1-3 g/L of NaOH, and remaining amount of water to prepare a refining/bleaching agent; a step of refining/bleaching using the refining/bleaching agent at 80-85°C for 30-40 minutes and drying at room temperature; a step of preparing dyeing solution containing 2-13% of o.w.f, 40-60 g/L of Na_2SO_4, 15-20 g/L of Na_2CO_3, and remaining amount of water and dyeing at 40-80°C for 60-90 minutes; and a step of soaping at 60-70°C for 20-30 minutes.
    • 目的:提供用尼龙和棉纤维覆盖的含有多层导电丝的织物染色方法,以确保优异的色牢度和形状稳定性。 构成:含有多层导电丝的导电性织物的染色方法包括:将8-10g / L过氧化氢,3-5g / L稳定剂,2-4g / L澄清剂, 1-3g / L NaOH和剩余量的水以制备精制/漂白剂; 使用精制/漂白剂在80-85℃下精制/漂白30-40分钟并在室温下干燥的步骤; 制备含有2-13%的owf,40-60g / L的Na 2 SO 4,15-20g / L的Na 2 CO 3的染色溶液和剩余量的水并在40-80℃下染色60-90分钟的步骤 ; 和在60-70℃下皂化20-30分钟的步骤。
    • 6. 发明公开
    • 전도성 직물의 동색성향상염색방법
    • 导电纺织品的水平染色工艺
    • KR1020130034938A
    • 2013-04-08
    • KR1020110099116
    • 2011-09-29
    • (주)삼광염직
    • 안병준김은철이봉환윤석환김미경
    • D06P3/84D06P1/38D06P1/32
    • D06P1/38D06P1/39D06P3/82
    • PURPOSE: A homochromatic dyeing method of a conductive fabric is provided to maintain shape stability and electric property of the conductive fabric, and to enhance homochromatism and color formation. CONSTITUTION: A homochromatic dyeing method of a conductive fabric comprises: a step of pretreating a fabric containing a multilayer conductive yarn and a wool yarn in a refining and bleaching solution at 70-80 deg. C for 30-60 minutes; a step of dyeing the conductive fabric in a dyeing solution at pH 7-8 and at 90-100 deg. C for 30-60 minutes; a step of washing the conductive fabric with warm water at 60-70 deg. C for 5-10 minutes; and a step of washing the conductive fabric with cold water at 30-40 deg. C for 5-10 minutes.
    • 目的:提供导电织物的同色染色方法,以保持导电织物的形状稳定性和电性能,并增强均匀性和色彩形成。 构成:导电织物的同色染色方法包括:在70-80度的精炼和漂白溶液中预处理含有多层导电纱线和羊毛纱线的织物的步骤。 C为30-60分钟; 在pH7-8和90-100度的染色溶液中染色导电织物的步骤。 C为30-60分钟; 用60-70度的温水洗涤导电织物的步骤。 C 5-10分钟; 以及用30-40℃的冷水洗涤导电织物的步骤。 C 5-10分钟。