    • 1. 发明授权
    • Elastomeric polymer blends and processes for their production
    • 弹性聚合物共混物及其生产方法
    • US08247495B2
    • 2012-08-21
    • US13015364
    • 2011-01-27
    • Rainer KolbJohn W. ChuGabor KissRobert P. Reynolds, Jr.Jean-Roch SchauderThomas T. Sun
    • Rainer KolbJohn W. ChuGabor KissRobert P. Reynolds, Jr.Jean-Roch SchauderThomas T. Sun
    • C08F8/00C08L23/04C08L23/10
    • C08L23/142C08L2205/02C08L2314/06C08L2666/06
    • Elastomeric polymer blends and processes for their production are described. Specifically, the polymer blends comprise a first polymer and a second polymer, where the first polymer comprises from about 70 wt % to about 90 wt % units derived from propylene and from about 10 wt % to about 30 wt % units derived from ethylene and/or a C4-C10 alpha-olefin, and the second polymer comprises from about 88 wt % to about 98 wt % units derived from propylene and from about 2 wt % to about 12 wt % units derived from ethylene and/or a C4-C10 alpha-olefin. The elastomeric polymer blends are further characterized by having two or more of the following properties: an overall propylene content of between about 75 wt % and about 90 wt %, a melting point between about 110° C. and about 145° C., a Vicat softening point greater than about 45° C., a tensile stress at 300% strain of less than about 500 psi (3447 kPa), as determined by a stress strain test according to ASTM D412, or an average maximum force for pellet separation of less than about 10 N in an accelerated storage stability test. The polymer blends are produced in a dual reactor process, in which the first polymer and the second polymer are prepared using differing catalyst systems.
    • 描述了弹性聚合物共混物及其生产方法。 具体地,聚合物共混物包含第一聚合物和第二聚合物,其中第一聚合物包含约70重量%至约90重量%的衍生自丙烯的单元和约10重量%至约30重量%的衍生自乙烯和/ 或C 4 -C 10α-烯烃,并且第二聚合物包含衍生自丙烯的约88重量%至约98重量%的单元和衍生自乙烯和/或C 4 -C 10的约2重量%至约12重量%的单元 α-烯烃。 弹性体聚合物共混物的进一步特征在于具有两种或更多种以下性能:总丙烯含量为约75重量%至约90重量%,熔点为约110℃至约145℃, 维卡软化点大于约45℃,通过根据ASTM D412的应力应变测试确定的小于约500psi(3447kPa)的300%应变下的拉伸应力或丸粒分离的平均最大力 在加速储存稳定性试验中小于约10N。 聚合物共混物在双重反应器方法中制备,其中使用不同的催化剂体系制备第一聚合物和第二聚合物。
    • 2. 发明申请
    • Elastomeric Polymer Blends and Processes for Their Production
    • 弹性体聚合物共混物及其制备方法
    • US20110207888A1
    • 2011-08-25
    • US13015364
    • 2011-01-27
    • Rainer KolbJohn W. ChuGabor KissRobert P. Reynolds, JR.Jean-Roch SchauderThomas T. Sun
    • Rainer KolbJohn W. ChuGabor KissRobert P. Reynolds, JR.Jean-Roch SchauderThomas T. Sun
    • C08L23/14C08J5/00
    • C08L23/142C08L2205/02C08L2314/06C08L2666/06
    • Elastomeric polymer blends and processes for their production are described. Specifically, the polymer blends comprise a first polymer and a second polymer, where the first polymer comprises from about 70 wt % to about 90 wt % units derived from propylene and from about 10 wt % to about 30 wt % units derived from ethylene and/or a C4-C10 alpha-olefin, and the second polymer comprises from about 88 wt % to about 98 wt % units derived from propylene and from about 2 wt % to about 12 wt % units derived from ethylene and/or a C4-C10 alpha-olefin. The elastomeric polymer blends are further characterized by having two or more of the following properties: an overall propylene content of between about 75 wt % and about 90 wt %, a melting point between about 110° C. and about 145° C., a Vicat softening point greater than about 45° C., a tensile stress at 300% strain of less than about 500 psi (3447 kPa), as determined by a stress strain test according to ASTM D412, or an average maximum force for pellet separation of less than about 10 N in an accelerated storage stability test. The polymer blends are produced in a dual reactor process, in which the first polymer and the second polymer are prepared using differing catalyst systems.
    • 描述了弹性聚合物共混物及其生产方法。 具体地,聚合物共混物包含第一聚合物和第二聚合物,其中第一聚合物包含约70重量%至约90重量%的衍生自丙烯的单元和约10重量%至约30重量%的衍生自乙烯和/ 或C 4 -C 10α-烯烃,并且第二聚合物包含衍生自丙烯的约88重量%至约98重量%的单元和衍生自乙烯和/或C 4 -C 10的约2重量%至约12重量%的单元 α-烯烃。 弹性体聚合物共混物的进一步特征在于具有两种或更多种以下性能:总丙烯含量为约75重量%至约90重量%,熔点为约110℃至约145℃, 维卡软化点大于约45℃,通过根据ASTM D412的应力应变测试确定的小于约500psi(3447kPa)的300%应变下的拉伸应力或丸粒分离的平均最大力 在加速储存稳定性试验中小于约10N。 聚合物共混物在双重反应器方法中制备,其中使用不同的催化剂体系制备第一聚合物和第二聚合物。