    • 2. 发明申请
    • VALUE IMPROVEMENT OF CLAYS
    • 粘土价值改进
    • WO1998014401A1
    • 1998-04-09
    • PCT/AU1997000636
    • 1997-09-25
    • MCLAUGHLIN GEOSURVEYS PTY. LIMITEDMCLAUGHLIN, Robert, James
    • MCLAUGHLIN GEOSURVEYS PTY. LIMITED
    • C01F07/46
    • C01F7/765C01B33/187C01F7/20C01F7/26C01P2002/84C01P2006/80
    • A process which allows the conversion of clay minerals of the kalonite group, to a relatively pure form of alumina and silica respectively comprising the steps of: (a) heating the kaolinite group minerals to greater than 500 DEG C, which causes dehydroxylation of the crystallographic lattice and formation of an intermediate meta-kaolin; (b) reacting the intermediate with only one of a selection of reagents including acids, alkalines or metalliferous compounds followed by heating of the mixture to form an aluminium salt in solution and residue of silica; (c) separation of the aluminium salt solution from the residue of silica by filtration and further treatment of the silica residue to produce a relatively pure form of fine particled silica; (d) formation of an alum by addition of ammonium sulphate in solution to the aluminium salt solution and further treatment of the alum to produce a relatively pure form of aluminium hydroxide.
    • 允许将钙蓝矿的粘土矿物转化成相对纯的形式的氧化铝和二氧化硅的方法,分别包括以下步骤:(a)将高岭石矿物质加热到大于500℃,这导致晶体学的脱羟基化 中间体高岭土的晶格和形成; (b)使中间体与选择的试剂(包括酸,碱或含金属化合物)中的一种反应,然后加热混合物以在溶液中形成铝盐,并将二氧化硅残余物反应; (c)通过过滤将铝盐溶液与二氧化硅残余物分离,并进一步处理二氧化硅残余物以产生相对纯的形式的细颗粒二氧化硅; (d)通过在铝盐溶液中加入硫酸铵形成明矾,并进一步处理明矾以产生相对纯的形式的氢氧化铝。
    • 4. 发明申请
    • PROCESS FOR NEUTRALIZING BAUXITE DISSOLUTION RESIDUAL SUBSTANCE AND PROCESS FOR PRODUCING ALUMINUM HYDROXIDE
    • 中和挥发性残留物质的处理方法和生产氢氧化铝的方法
    • WO2009082024A2
    • 2009-07-02
    • PCT/JP2008073903
    • 2008-12-22
    • SHOWA DENKO KKISHIKAWA ISAO
    • ISHIKAWA ISAO
    • C01F7/06B09B3/00C02F11/14
    • C22B21/0015C01F7/066C01F7/26C02F1/66
    • A process for neutralization is provided which can maintain a high solid content of a bauxite dissolution residual substance slurry even after a neutralization treatment is completed and the stabilize pH within a short time of the neutralization treatment. Such a process for neutralizing a bauxite dissolution residual substance containing a desiliconizing product which is generated in the production process of aluminum hydroxide using Bayer process, includes: mixing a bauxite dissolution residual substance or a bauxite dissolution residual substance slurry with sulfuric acid in an amount ranging from 0.6 to 1.2 equivalence to the total amount of sodium contained in the bauxite dissolution residual substance or a bauxite dissolution residual substance slurry, such that the solid content after mixing becomes 400 to 700 g/1 to gelate the mixture, and thereafter obtaining a bauxite dissolution residual substance neutralized slurry.
    • 提供了一种中和方法,其即使在中和处理完成之后也可以保持铝土矿溶解残留物浆料的高固体含量,并且在中和处理的短时间内稳定pH。 这种用于中和使用拜耳法生产的氢氧化铝生产过程中含有脱硅产物的铝土矿溶解残留物质的方法包括:将铝土矿溶解残余物质或铝土矿溶解残渣物质与硫酸混合, 与铝矾土溶解残留物或铝土矿溶解残留物料浆中所含的钠的总量相等的0.6〜1.2,混合后的固体成分为400〜700g / l,使混合物凝胶化,然后得到铝土矿 溶解残留物中和浆液。
    • 5. 发明申请
    • ACID DIGESTION PROCESS FOR TREATING ALUMINA-BEARING ORES TO RECOVER METAL VALUES THEREFROM
    • 用于处理氧化铝轴承的酸消除过程以恢复其金属值
    • WO02090605A8
    • 2004-05-13
    • PCT/US0213960
    • 2002-05-02
    • GOLDENDALE ALUMINUM COMPANY
    • BARNETT ROBERT JMEZNER MICHAEL B
    • C01F7/20C01F7/26C01G23/053C01G49/02C22B3/06C22B3/08C22B21/00C01F7/06C22B3/44
    • C22B3/08C01F7/20C01F7/26C01G23/053C01G49/02C01P2004/61C01P2004/62C01P2006/12C01P2006/80C22B3/06C22B21/0007Y02P10/234
    • A method for processing alumina-bearing ores such as bauxite to recover iron, aluminum, silicon and titanium metal values therefrom the method comprising the steps of adding the alumina-bearing ores to a digester containing an acid to provide a mixture of acid and alumina-bearing ores and heating the mixture to dissolve soluble compounds of at least one of iron, aluminum, silicon and titanium to provide a digest containing dissolved salts of the soluble compounds and to provide a gas component. Thereafter, the digest is treated with water to dissolve water soluble salts therein to provide a slurry comprised of a liquid containing water and the dissolved soluble salts and a solid component comprised of silica. The solid component is separated from the liquid and the pH of the liquid is adjusted to form an aluminate and an iron-containing precipitate. The iron-containing precipitate is separated from the liquid to provide an iron-depleted liquid whose pH is adjusted to precipitate aluminum trihydrate which is separated from the iron-depleted liquid to provide an aluminum trihydrate-depleted liquid. The pH of the aluminum trihydrate-depleted liquid is adjusted to form a precipitate comprised of at least one remaining salt in the aluminum trihydrate-depleted liquid to provide a salt-depleted liquid. The salt precipitate is separated from the salt-depleted liquid thereby recovering the metal values from the alumina-bearing ores.
    • 一种用于处理含铝矿石如铝矾土以回收其中的铁,铝,硅和钛金属值的方法,所述方法包括以下步骤:将含氧化铝的矿石加入到含酸的蒸煮器中以提供酸和氧化铝 - 承载矿石并加热该混合物以溶解铁,铝,硅和钛中的至少一种的可溶性化合物,以提供含有可溶性化合物的溶解盐的消化物并提供气体组分。 此后,用水处理消化物以溶解其中的水溶性盐,以提供由含有水的溶液和溶解的可溶性盐以及由二氧化硅组成的固体组分的浆料。 将固体组分与液体分离,并调节液体的pH以形成铝酸盐和含铁沉淀物。 将含铁沉淀物与液体分离以提供贫铁液体,其pH被调节以沉淀三水合铝,其与贫铁液体分离以提供三水合铝贫液体。 调节三水合铝酸液体的pH以在三水合铝贫液体中形成由至少一种剩余的盐组成的沉淀物以提供贫盐液体。 将盐沉淀物与贫盐液体分离,从而从含氧化铝的矿石中回收金属值。
    • 9. 发明申请
    • СПОСОБ ПЕРЕРАБОТКИ ГЛИНОЗЕМСОДЕРЖАЩЕГО СЫРЬЯ И СПОСОБ ВСКРЫТИЯ ГЛИНОЗЕМСОДЕРЖАЩЕГО СЫРЬЯ ПРИ ЕГО ПЕРЕРАБОТКЕ
    • 加工含氧化铝原料的方法和在加工过程中使含铝的原料破裂的方法
    • WO2016056947A1
    • 2016-04-14
    • PCT/RU2015/000601
    • 2015-09-24
    • ОБЩЕСТВО С ОГРАНИЧЕННОЙ ОТВЕТСТВЕННОСТЬЮ "НЬЮКЕМ ТЕКНОЛОДЖИ"
    • ХАМИЗОВ, Руслан ХажсетовичМОРОШКИНА, Лилия ПетровнаВЛАСОВСКИХ, Наталья СергеевнаХАМИЗОВ, Султан Хажсетович
    • C01F7/26C01F7/30
    • C01F7/26C01F7/30
    • Изобретение относится к химии и металлургии для переработки и вскрытия глиноземсодержащего сырья. Способ переработки осуществляется в виде кругового процесса, содержащего: стадию вскрытия, включающую разложение сырья раствором-реагентом, содержащим гидросульфат аммония и серную кислоту, разделение полученной пульпы с выделением неразложившихся твердых остатков, которые промывают водой, и маточного раствора квасцов, при этом раздельно собирают маточный раствор квасцов и промывные воды; стадию очистки, где промывные воды очищают от железа, объединяют с маточным раствором, охлаждают и отделяют кристаллы алюмоаммонийных квасцов, при этом из маточного раствора выделяют серную кислоту, используемую на стадии вскрытия для раствора-реагента; стадию осаждения гидроксида алюминия из очищенного раствора квасцов с аммиаком; стадию отделения гидроксида алюминия; стадию получения твердого сульфата аммония и стадию его термического разложения на гидросульфат аммония и аммиак, используемые, соответственно, на стадии вскрытия при приготовлении раствора-реагента и на стадии осаждения. Изобретение позволяет перерабатывать любое глиноземсодержащее сырье при невысоких температурах, уменьшить потери реагентов и требуемый объем их восполнения в ходе процесса.
    • 本发明涉及化学和冶金,并且用于加工和分解含氧化铝原料。 进行处理方法为循环过程,其包括:使用含有硫酸氢铵和硫酸的试剂溶液分解原料的分解阶段,并将所得浆液分离,产生未分解的固体残余物,用水漂洗 和明矾母溶液,其中明矾母溶液和漂洗水分开收集; 净化阶段,其中冲洗水被纯化,然后与明矾母溶液组合并冷却,分离出铵明矾的晶体,其中用于分解阶段中的试剂溶液的硫酸被分离出来; 沉淀阶段,其中氢氧化铝从纯化的明矾溶液中用氨沉淀; 用于分离氢氧化铝的分离阶段; 在制备试剂溶液期间和在沉淀阶段分别获得固体硫酸铵的阶段和用于将其热分解成硫酸氢铵和氨的阶段,其可用于分解阶段。 本发明使得可以在低温下处理任何含氧化铝的原料,以减少试剂损失并减少在该过程中需要补充的试剂的体积。