    • A low-compaction method of making an absorbent cellulosic web includes: forming a nascent web from a papermaking furnish; dewatering the nascent web to a consistency of from about 10 to about 30 percent on a foraminous forming support traveling at a first speed; rush-transferring the web at a consistency of from 10 to about 30 percent to an open texture fabric traveling at a second speed slower than the first speed of the forming support; further dewatering the web on the impression fabric to a consistency of from about 30 to about 60 percent by way of (i) combining the open texture fabric bearing said web with a fluid distribution membrane and an anti-rewet felt as the three pass through a nip into a pressure chamber defined in part by a plurality of nip rolls, the fluid distribution membrane bearing against the side of the open texture fabric away from the web, with the anti-rewet felt bearing against the web, and (ii) applying a pneumatic pressure gradient from the distributor membrane through the web thereby dewatering the web; and drying the web. Preferably the process includes the steps of selecting the papermaking furnish and controlling the process such that the dried web has a void volume fraction of at least 0.7, a hydraulic diameter in the range of from about 3 to about 20 microns and a Wet Springback Ratio of at least about 0.65. Optionally provided is a high solids fabric crepe in a pressure nip.
    • 制造吸收性纤维素网的低压实方法包括:从造纸配料形成新生网; 在初始速度下移动的多孔成形支撑件上将初生纤维网脱水至约10%至约30%的稠度; 以相对于成形支撑件的第一速度慢的第二速度行进的开放纹理织物将幅材以10%至约30%的一致性转移; 通过(i)将带有所述纤维网的开放纹理织物与流体分布膜和防再润湿毡组合在一起,将印模织物上的幅材进一步脱水至约30至约60%的稠度, 夹持在由多个压辊部分限定的压力室中,流体分配膜抵靠打开的织物织物远离纸幅的方向承载,抗再湿润毡轴承抵靠纸幅,并且(ii)施加 从分配器膜通过纤维网的气动压力梯度,从而使幅材脱水; 并干燥网。 优选地,该方法包括选择造纸配料并控制该方法的步骤,使得干燥的幅材具有至少0.7的空隙体积分数,约3至约20微米的水力直径和湿回弹比 至少约0.65。 任选地,在压力压区中提供高固体织物绉纹。