    • 8. 发明申请
    • SPUNBOND FIBERS AND FABRICS FROM POLYOLEFIN BLENDS
    • SPUNBOND纤维和织物从聚烯烃混合物
    • WO2008091432A2
    • 2008-07-31
    • PCT/US2007/084646
    • 2007-11-14
    • ExxonMobil Chemical Patents Inc.KACKER, SmitaCHENG, Chia, Yung
    • KACKER, SmitaCHENG, Chia, Yung
    • D01F6/46C08L23/10C08L2203/12C08L2205/02D04H3/16Y10T442/681C08L2666/06
    • The invention described relates to a polyolefm blend composition suitable for spunbond fiber or filament compositions, and to fabric compositions and composite constructions therefrom, said blend comprising a) from 60-98 wt% of at least one random propylene copolymer having a comonomer content of from 8 to 25 wt% and a crystalline melting point (Tm) as determined by differential scanning calorimetry (DSC) of from about 4O°C to about 110°C; and b) from 2-40 wt% of at least one substantially isotactic polypropylene homopolymer or copolymer comprising one or more C 2 and/or C 4 -C 8 comonomer, having a crystalline melting point (Tm) as determined by DSC greater than or equal to 12O°C. The blends of the present invention typically have a melt flow rate (MFR) of from 100 g/10min to about 500 g/10min.
    • 所描述的本发明涉及适用于纺粘纤维或长丝组合物的聚烯烃共混物组合物,以及由其组成的织物组合物和复合结构,所述共混物包含a)60-98重量%的至少一种无规丙烯共聚物,其共聚单体含量为 8〜25重量%,通过差示扫描量热法(DSC)测定的约40℃〜约110℃的结晶熔点(Tm) 和b)2-40重量%的至少一种基本上全同立构的聚丙烯均聚物或共聚物,其包含一个或多个C 2和/或C 4 -C 8 具有通过DSC测定的结晶熔点(Tm)大于或等于120℃的共聚单体。 本发明的共混物通常具有100g / 10min至约500g / 10min的熔体流动速率(MFR)。