    • PROCESS FOR PRODUCING POLY(1,4-CYCLOHEXYLENEDIMETHYLENE 1,4-CYCLOHEXANEDICARBOXYLATE) AND THE REACTOR GRADE POLYESTER THEREFROM
    • 制备聚(1,4-环己基亚乙基亚甲基1,4-环己烷二羧酸酯)的方法及其反应物级分聚酯
    • WO0231020A2
    • 2002-04-18
    • PCT/US0131194
    • 2001-10-04
    • EASTMAN CHEM CO
    • QUILLEN DONNA RICE
    • C08G63/199C08G63/78C08G63/82
    • C08G63/82C08G63/199C08G63/78
    • In a process for producing a reactor grade polyester, a poly(1,4-cyclohexylenedimethylene 1,4-cyclohexanedicarboxylate) has a reduced amount of isomerization of the trans-isomer to the cis-isomer of 1,4-dimethylcyclohexanedicarboxylate and an increased polymerization rate by the addition of a phosphorus-containing compound to the reaction process. In step (a) of the process, a diacid comprising at least 80 mole percent 1,4-cyclohexanedicarboxylic acid or an ester derivative of the diacid comprising at least 80 mole percent 1,4-dimethylcyclohexanedicarboxylate is reacted with a glycol comprising at least 80 mole percent 1,4-cyclohexanedimethanol at a temperature sufficient to effect esterification for the diacid or transesterification for the ester derivative. In step (b), the product of step (a) is subjected to temperature and pressures in the presence of a suitable catalyst to effect polycondensation. Phosphorus in an amount of 1 to 800 ppm is added in the form of a phosphorus-containing compound during the process.
    • 在制备反应器级聚酯的方法中,聚(1,4-环己烯二亚甲基1,4-环己烷二羧酸酯)具有减少的反式异构体向1,4-二甲基环己烷二羧酸酯的顺式异构体的量和增加的聚合 通过向反应过程中加入含磷化合物的速率。 在该方法的步骤(a)中,将包含至少80摩尔%1,4-环己烷二羧酸的二酸或包含至少80摩尔%1,4-二甲基环己烷二羧酸酯的二酸的酯衍生物与包含至少80 摩尔百分比的1,4-环己烷二甲醇在足以实现酯衍生物的二酸或酯交换的酯化反应的温度下进行。 在步骤(b)中,步骤(a)的产物在合适的催化剂存在下进行温度和压力以进行缩聚反应。 在该过程中以含磷化合物的形式加入1至800ppm的量的磷。
    • 10. 发明申请
    • ALUMINUM/ALKALINE OR ALKALI/TITANIUM CONTAINING POLYESTERS HAVING IMPROVED REHEAT, COLOR AND CLARITY
    • 含有改进的再利用,颜色和澄清的聚酯的铝/碱性或碱性/碱金属
    • WO2007035250A2
    • 2007-03-29
    • PCT/US2006034543
    • 2006-09-06
    • EASTMAN CHEM CO
    • QUILLEN DONNA RICEARMENTROUT RODNEY SCOTTJERNIGAN MARY THERESESTAFFORD STEVEN LEEXIA ZHIYONG
    • B32B27/08C08K3/22C08K3/38
    • C08G63/83B29C47/0004B29C47/0016B29C47/0021C08G63/183C08G63/84Y10T428/1352Y10T428/1355Y10T428/139Y10T428/1397
    • A polyester composition containing: a) aluminum atoms; and b) alkaline earth atoms or alkali metal atoms or alkali compound residues such as lithium atoms; and c) particles comprising titanium, zirconium, vanadium, niobium, hafnium, tantalum, chromium, tungsten, molybdenum, iron, or nickel atoms or combinations thereof, where the particles improve the reheat rate of the polyester composition. The polyester polymer compositions may also contain phosphorus catalyst deactivators/stabilizers. The polyester compositions and the articles made from the compositions such as bottle preforms and stretch blow molded bottles have improved reheat rate while maintaining low haze, high L*, a b* below 3, and have low levels of acetaldehyde. In the process for making the polyester polymer, the polymer melt is polycondensed in the presence of a) and b), with the particles c) added in a melt phase process or added to the polymer in an injection molding machine or extruder. The polyester polymer composition can be made to high IV from the melt phase while avoiding solid state polymerization.
    • 一种聚酯组合物,其含有:a)铝原子; 和b)碱土金属原子或碱金属原子或碱金属化合物残基如锂原子; 和c)包含钛,锆,钒,铌,铪,钽,铬,钨,钼,铁或镍原子或其组合的颗粒,其中颗粒改善了聚酯组合物的再热速率。 聚酯聚合物组合物还可以含有磷催化剂失活剂/稳定剂。 聚酯组合物和由组合物如瓶坯和拉伸吹塑成型瓶制成的制品具有改善的再加热速率,同时保持低雾度,高L *,低于3的b *,并且具有低水平的乙醛。 在制备聚酯聚合物的过程中,聚合物熔体在a)和b)存在下缩聚,颗粒c)以熔融相方式加入,或者在注射成型机或挤出机中加入到聚合物中。 聚酯聚合物组合物可以从熔融相制成高IV,同时避免固态聚合。