热词
    • 5. 发明申请
    • LASER SCORING OF GLASS SHEETS AT HIGH SPEEDS AND WITH LOW RESIDUAL STRESS
    • 玻璃片的激光切割在高速和低残留应力下
    • WO2009067164A1
    • 2009-05-28
    • PCT/US2008/012770
    • 2008-11-14
    • CORNING INCORPORATEDABRAMOV, Anatoli ASUN, YaweiXU, WeiZHOU, Naiyue
    • ABRAMOV, Anatoli ASUN, YaweiXU, WeiZHOU, Naiyue
    • C03B33/09B23K26/073
    • C03B33/091Y02P40/57
    • Experimental data is presented which shows that laser scoring of glass sheets (112) with existing techniques produces unacceptable levels of residual stress in the separated sheets as the scoring speed is increased. Methods for solving this problem are disclosed which employ elongated and, preferably, asymmetrically-truncated laser beams (13). The methods allow glass sheets (112) to be scored at speeds of 1000mm/s and above with low levels of residual stress, e.g., levels of residual stress which are less than or equal to 500 psi. Such low levels of residual stress translate into low levels of distortion during the manufacture of display panels (e.g., LCD panels) as well as in improved properties of the separated edges. The methods can be used with glasses of various types including glasses having low coefficients of thermal expansion.
    • 实验数据显示,现有技术的玻璃板(112)的激光刻痕在分选片材中随着刻痕速度的提高而产生不可接受的残余应力水平。 公开了解决这个问题的方法,其采用细长的,优选的是非对称截断的激光束(13)。 这些方法允许玻璃板(112)以1000mm / s以上的速度刻痕,残留应力低,例如小于或等于500psi的残余应力水平。 这种低水平的残余应力在显示面板(例如LCD面板)的制造过程中转化为低水平的变形以及分离边缘的改进的性质。 该方法可用于各种类型的眼镜,包括具有低热膨胀系数的眼镜。
    • 7. 发明申请
    • METHOD OF SEPARATING STRENGTHENED GLASS
    • 分离强化玻璃的方法
    • WO2010096316A1
    • 2010-08-26
    • PCT/US2010/023816
    • 2010-02-11
    • CORNING INCORPORATEDABRAMOV, Anatoli AGOMEZ, SinueTSUDA, Sergio
    • ABRAMOV, Anatoli AGOMEZ, SinueTSUDA, Sergio
    • C03B33/09C03B33/02
    • C03B33/091C03B27/0413
    • A method is provided for separating or dividing strengthened glass articles, particularly strengthened glass sheets, into at least two pieces, one of which has a predetermined shape and/or dimension. A flaw is initiated in the glass at a depth that is greater than the depth of the strengthened surface layer of the glass, and a vent extending from the flaw is created at a vent depth that is greater than the depth of and outside the strengthened surface layer to at least partially separate the glass. In one embodiment, the vent is generated by treating the glass with a laser to heat the glass to a temperature in a range from about 50°C below the strain point of the glass up to a temperature between the strain point and the anneal point of the glass. A glass article having at least one strengthened surface and at least one edge having an average edge strength of at least 200 MPa is also described.
    • 提供了一种用于将加强的玻璃制品,特别是加强的玻璃板分离或分成至少两个,其中一个具有预定形状和/或尺寸的方法。 在玻璃中以比玻璃的强化表面层的深度大的深度开始缺陷,并且在比加强表面的深度和深度大的排气深度处产生从缺陷延伸的通气孔 层以至少部分地分离玻璃。 在一个实施例中,通过用激光处理玻璃来产生排气孔,以将玻璃加热到低于玻璃应变点约50℃的范围内的温度,直到应变点和退火点之间的温度 玻璃。 还描述了具有至少一个加强表面和至少一个平均边缘强度至少为200MPa的边缘的玻璃制品。