会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 4. 发明申请
    • FLUXLESS BRAZING METHOD
    • 无流体钎焊法
    • WO2017080771A1
    • 2017-05-18
    • PCT/EP2016/075155
    • 2016-10-20
    • ALERIS ROLLED PRODUCTS GERMANY GMBH
    • SCHLEGEL, ArneJACOBY, BerndKIRKHAM, Steven
    • B23K1/00B23K1/012B23K1/20B23K35/28B23K35/38B23K35/02B23K101/14B23K103/10B23K101/10
    • B23K1/0012B23K1/012B23K1/20B23K35/0238B23K35/286B23K35/383B23K2201/10B23K2201/14
    • The invention relates to a method of manufacturing a heat exchanger, joined by brazing in a controlled atmosphere brazing process, comprising the steps of: (a)providing of the components to be brazed together of which at least one is made from an aluminium alloy brazing sheet product comprising of a core alloy clad on one or both sides with a Al-Si alloy brazingfiller material, the Al- Si alloy brazing filler material has been pre-treated by means of etching with an alkaline or acidic etchant, and wherein the Al-Si alloy brazing filler material has the following composition, consisting of, in wt.%: Si 5% to 15%, Mg 0.10% to 3%, Fe up to 0.8%, Cu up to 0.3%, Mn up to 0.8%, Zn up to 0.25%, Ti up to 0.3%, balance aluminium, (b)assembling the components into an assembly, (c)brazing the assembly without applying brazing flux onto the assembly components, and brazing the whole assembly in a dry inert gas atmosphere at a brazing temperature, and wherein the oxygen content of the dry inert gas atmosphere is less than 35 ppm, and cooling of the brazed assembly.
    • 本发明涉及一种制造热交换器的方法,所述热交换器通过在受控气氛钎焊工艺中钎焊而连接,所述方法包括以下步骤:(a)提供待钎焊在一起的部件,其至少部分地 一种由铝合金钎焊片材产品制成,所述铝合金钎焊片材产品包括在一侧或两侧包覆有铝硅合金钎焊填充材料的芯合金,所述铝硅合金钎焊填充材料已通过碱性蚀刻进行预处理 或酸性蚀刻剂,并且其中所述Al-Si合金钎焊填充材料具有以下组成,其包含以重量%计:Si 5%至15%,Mg 0.10%至3%,Fe最高达0.8%,Cu最高至 0.3%,Mn高达0.8%,Zn高达0.25%,Ti高达0.3%,余量为铝,(b)将组件组装成组件,(c)在不将钎焊剂施加到组件上的情况下硬焊组件, 将整个组件在钎焊温度下在干燥的惰性气体气氛中钎焊,并且其中, 干燥的惰性气体气氛小于35 ppm,并冷却钎焊组件。