    • PRODUCING METHOD OF POLYMER FILM
    • 聚合物薄膜的生产方法
    • WO2007034973A1
    • 2007-03-29
    • PCT/JP2006/319092
    • 2006-09-20
    • FUJIFILM CorporationTONOHARA, Kouji
    • TONOHARA, Kouji
    • B29C55/08G02B5/30G02F1/1335G02F1/13363B29K1/00B29L7/00B29L11/00
    • B29C41/28B29C47/0021B29C47/8805B29C47/8845B29C55/08B29K2001/00B29K2001/12G02F1/13363G02F2201/50
    • A casting dope (11) prepared from CAP, additive and solvent is cast onto a casting belt (35), peeled and dried to be a primary film (14), and wound to a primary film roll (16). After the storage, the primary film (14) is unwound and fed into a tenter device (18). In the tenter device (18), while the stretch in the widthwise direction is performed, a relaxation of the primary film (14) in the longitudinal direction is made. If an extent percentage of the stretch is less than 70% to the predetermined value, the relation is started. The primary film (14) is fed out as a produced polymer film (22) from the tenter device (18), and the polymer film (22) is wound up to a product film roll (24). On the produced polymer film (22), the in-plane retardation increases and the thickness retardation decreases. Thus the optical properties become preferable.
    • 将由CAP,添加剂和溶剂制备的浇铸液(11)浇铸到铸造带(35)上,剥离并干燥成初级膜(14),并缠绕到初级膜卷(16)上。 储存后,将初级薄膜(14)退绕并进入拉幅机装置(18)。 在拉幅装置(18)中,在进行宽度方向的拉伸的同时,使主膜(14)沿长度方向松弛。 如果拉伸的程度百分比小于预定值的70%,则开始关系。 从拉幅装置(18)将初级薄膜(14)作为生产的聚合物薄膜(22)送出,将聚合物薄膜(22)卷绕到产品薄膜卷(24)上。 在所生产的聚合物膜(22)上,面内延迟增加,厚度延迟减小。 因此,优选光学性质。