    • 6. 发明申请
    • METHODS FOR PRODUCTION OF ZINC OXIDE ELECTRODES FOR ALKALINE BATTERIES
    • 用于生产碱性电池用氧化锌电极的方法
    • WO02075825A3
    • 2003-05-15
    • PCT/CA0200352
    • 2002-03-15
    • PHILLIPS JEFFREYPOWERGENIX SYSTEMS INC
    • PHILLIPS JEFFREY
    • H01M4/26C01G9/02H01M4/04H01M4/24H01M4/36H01M4/62H01M10/24
    • H01M4/244H01M4/04H01M4/26H01M4/364H01M4/62H01M4/622H01M10/24Y10T29/49115
    • A zinc electrode for use in alkaline batteries comprises a mixture of 0.425 to 1.55 volume parts of zinc oxide with a volume part of a metallic oxide chosen from the group consisting of: calcium oxide, barium oxide, and mixtures thereof, together with hydroxy-ethyl cellulose, an oxide dispersant chosen from the group consisting of: soap derivatives, anionic polyelectrolytes, anionic surfactants, and mixtures thereof, and a binder. The electrode is prepared by mixing zinc oxide with the chosen metallic oxide in an aqueous medium such as water or potassium hydroxide, stirring overnight, filtering and drying the mixture, optionally adding a further small amount of zinc oxide, optionally adding other metallic oxides, and adding hydroxy-ethyl cellulose, an oxide dispersant, and a binder. The aqueous paste os slurry thus formed is placed on a conductive substrate, drawn through a sizing gap, cut and dried, to form low cost pasted zinc oxide electrodes.
    • 用于碱性电池的锌电极包括0.425至1.55体积份量的氧化锌与体积部分金属氧化物的混合物,其选自氧化钙,氧化钡及其混合物,以及羟基乙基 纤维素,选自以下的氧化物分散剂:皂衍生物,阴离子聚电解质,阴离子表面活性剂及其混合物,以及粘合剂。 电极通过在水性介质如水或氢氧化钾中混合氧化锌和选择的金属氧化物,搅拌过夜,过滤并干燥混合物,任选地加入少量氧化锌,任选地加入其它金属氧化物,以及 加入羟乙基纤维素,氧化物分散剂和粘合剂。 将如此形成的水性浆料浆料放置在导电基材上,通过筛分间隙拉伸,切割并干燥,形成低成本的糊化氧化锌电极。
    • 8. 发明申请
    • PASTED NICKEL HYDROXIDE ELECTRODE AND ADDITIVES FOR RECHARGEABLE ALKALINE BATTERIES
    • 补充镍氢氧化物电极和可充电碱性电池的添加剂
    • WO2014110164A1
    • 2014-07-17
    • PCT/US2014/010725
    • 2014-01-08
    • POWERGENIX SYSTEMS, INC.GENG, Mingming
    • GENG, Mingming
    • H01M10/04H01M4/525H01M4/505H01M4/58H01M4/13H01M4/139
    • H01M4/366H01M4/32H01M4/52H01M10/24H01M10/30H01M10/345Y02E60/122
    • A pasted positive nickel hydroxide electrode for use in battery cells (e.g., in nickel zinc cells, and nickel metal hydride cells) includes nickel hydroxide particles, a cobalt metal and/or cobalt compound and a sulfur-containing complexing agent capable of forming a complex with cobalt. The presence of the sulfur-containing complexing agent, such as dialkyldithiocarbamate (e.g., sodium diethyldithiocarbamate) improves lifetime and capacity utilization of the nickel electrode. The resulting pasted nickel hydroxide electrode includes a CoOOH conductive matrix after formation. The surface of the nickel hydroxide particles in the electrode is modified in some embodiments by providing a cobalt-containing coating onto the surface of the nickel hydroxide particles, followed by oxidation with a strong oxidizing agent. The complexing agent can be added before, after, or during the oxidation.
    • 用于电池单元(例如,镍锌电池和镍金属氢化物电池)中的粘贴的正氢氧化镍电极包括氢氧化镍颗粒,钴金属和/或钴化合物和能够形成络合物的含硫络合剂 与钴。 含硫络合剂如二烷基二硫代氨基甲酸钠(例如二乙基二硫代氨基甲酸钠)的存在改善了镍电极的寿命和容量利用。 得到的粘贴氢氧化镍电极在形成后包括CoOOH导电基体。 在一些实施方案中,电极中的氢氧化镍颗粒的表面是通过在氢氧化镍颗粒的表面上提供含钴涂层,然后用强氧化剂氧化来改性的。 络合剂可以在氧化之前,之后或期间加入。