热词
    • 5. 发明申请
    • COATED OPTICAL FIBER AND ADIATION CURABLE RESIN COMPOSITION
    • 包覆光纤和安装可固化树脂组合物
    • WO0177040A3
    • 2002-03-28
    • PCT/NL0100278
    • 2001-04-05
    • DSM NVBISHOP TIMOTHY EDWARDSNOWWITHE PAUL EUGENE
    • BISHOP TIMOTHY EDWARDSNOWWITHE PAUL EUGENE
    • G02B6/44C03C25/10C03C25/24C08F2/50C08F220/32C08F220/34C09D4/00C09D4/06
    • C09D4/06C03C25/106C03C25/1065C08F2/50C08F220/32C08F2220/346C09D4/00C08F290/14C08F290/06C08F2220/1875
    • The present invention relates to a coated optical fiber comprising a glass optical fiber with a single protective coating or a combination of an inner and an outer primary coating applied thereon and optionally with a colored coating subsequently applied thereon wherein the inner primary coating or at least a portion of the single coating is prepared from a radiation curable composition, which when applied as a capillary film having a thickness which is chosen as to fulfill the Lambert-Beer law, and cured with a 100W medium pressure mercury lamp, has a percentage reacted double bond unsaturation of at least about 54% after exposure to a dose of about 4.4 mJ/cm or wherein the outer primary coating is prepared from a radiation curable composition, which when applied as a capillary film having a thickness which is chosen as to fulfill the Lambert-Beer law, and cured with a 100W medium pressure mercury lamp, has a percentage reacted double bond unsaturation of at least about 56% after exposure to a dose of about 4.4 mJ/cm . The invention further relates to a radiation curable composition comprising a photoinitiator package of at least two free radical photoinitiators and having a relatively high cure speed.
    • 本发明涉及一种涂覆光纤,其包括具有单一保护涂层的玻璃光纤或其上施加有内部和外部初级涂层的组合,并且可选地随后涂覆有着色涂层,其中所述内部初级涂层或至少一个 单一涂层的一部分由可辐射固化组合物制备,当被用作具有选择满足朗伯 - 比尔定律的厚度并用100W中压汞灯固化的毛细管膜时,其具有反应双重百分比 在暴露于约4.4mJ / cm 2的剂量之后,键不饱和度为至少约54%,或者其中外部初级涂层由可辐射固化组合物制备,当被用作毛细管膜时,其厚度选择为 为了实现朗伯 - 比尔定律,用100W中压汞灯固化,反应后的双键不饱和度百分比至少约为56% 暴露于约4.4mJ / cm 2的剂量。 本发明还涉及包含至少两种自由基光引发剂的光引发剂包并且具有相对较高固化速度的可辐射固化组合物。