    • 4. 发明申请
    • 変性された酸化ジルコニウム-酸化第二スズ複合体ゾルの製造方法
    • 生产改性氧化锆氧化物复合材料溶胶的方法
    • WO2008007708A1
    • 2008-01-17
    • PCT/JP2007/063823
    • 2007-07-11
    • 日産化学工業株式会社小山 欣也浅田 根子
    • 小山 欣也浅田 根子
    • C01G25/00
    • C01G25/00B82Y30/00C01P2004/64
    • It is intended to provide a stable sol containing zirconium oxide-tin oxide composite colloids to be used for improving the performance such as abrasion resistance, transparency, adhesiveness, water resistance or weather resistance of a dried film obtained by applying a hard coating agent containing colloidal particles to the surface of plastic lens. A production method includes the steps of obtaining a sol containing colloidal particles (A1) in which the surface of particles in a sol containing hydrothermally-processed zirconium oxide-tin oxide composite colloids (A) is coated with amine-containing Sb 2 O 5 colloidal particles; obtaining a sol containing colloids (A2) coated with amine-containing Sb 2 O 5 colloidal particles by performing a hydrothermal treatment at a temperature of from 200 to 350°C; and mixing the sol containing the colloidal particles (A2) and a sol containing tungsten oxide-tin oxide-silicon dioxide composite colloidal particles (B2) and aging the resulting aqueous medium at 20 to 100°C.
    • 旨在提供一种含有氧化锆 - 氧化锡复合胶体的稳定溶胶,用于提高通过涂布含有胶体的硬涂层而得到的干燥膜的耐磨性,透明性,粘合性,耐水性或耐候性等性能 颗粒到塑料透镜的表面。 一种制备方法包括以下步骤:获得含有胶体颗粒(A1)的溶胶,其中在含有水热处理的氧化锆 - 氧化锡复合胶体(A)的溶胶中的颗粒表面涂覆有含胺Sb 2 胶体粒子; 5 / 通过在200〜350℃的温度下进行水热处理,得到含有含胺Sb 2 O 5 O 5胶体粒子的含有胶体(A2)的溶胶; 混合含有胶体粒子(A2)的溶胶和含有氧化钨 - 氧化锡 - 二氧化硅复合胶体粒子(B2)的溶胶,并使所得水性介质在20〜100℃下老化。
    • 7. 发明申请
    • プラスチックレンズの製造方法
    • 生产塑料镜片的方法
    • WO2005088352A1
    • 2005-09-22
    • PCT/JP2005/004079
    • 2005-03-09
    • HOYA株式会社小島 博小山 欣也浅田 根子
    • 小島 博小山 欣也浅田 根子
    • G02B1/10
    • C08J7/047C08J2483/00C08K3/22C09D183/04C08L2666/54
    • A method for producing a plastic lens which comprises applying a coating composition comprising (A) modified stannic oxide-zirconium oxide composite colloid particles having a particle diameter of 4.5 to 60 nm which have been formed by coating the surface of nuclei of stannic oxide-zirconium oxide composite colloid particles having a structure wherein colloid particles of stannic oxide obtained by the reaction of metallic tin, an organic acid and hydrogen peroxide and colloid particles of zirconium oxide are bound in a ZrO2/SnO2 ratio of 0.02 to 1.0 based on the weight of these oxides and having a particle diameter of 4 to 50 nm, with colloid particles of tungsten oxide- stannic oxide-silicon dioxide composite having a WO3/SnO2 wt ratio of 0.1 to 100, an SiO2/SnO2 wt ratio of 0.1 to 100, and a particle diameter of 2 to 7 nm, and (B) an organic silicon compound, on a plastic substrate, and then curing the coating composition.
    • 一种塑料透镜的制造方法,其特征在于,涂布涂料组合物,所述涂料组合物包含(A)通过涂覆氧化锡 - 锆的核的表面形成的粒径为4.5〜60nm的改性的氧化锡 - 氧化锆 - 氧化锆复合胶体粒子 氧化物复合胶体颗粒,其具有通过金属锡,有机酸和过氧化氢的反应获得的氧化锡胶体颗粒和氧化锆的胶体颗粒以ZrO 2 / SnO 2比为0.02-1.0的重量结合的结构, 这些氧化物的粒径为4〜50nm,具有WO 3 / SnO 2重量比为0.1〜100,SiO 2 / SnO 2重量比为0.1〜100的氧化钨 - 锡氧化物 - 二氧化硅复合体的胶体粒子,以及 粒径为2〜7nm,(B)有机硅化合物在塑料基材上,然后固化涂料组合物。
    • 8. 发明申请
    • フッ化物コロイド粒子のオルガノゾルおよびその製造方法
    • 氟化物胶体颗粒的有机溶剂及其生产方法
    • WO2008047787A1
    • 2008-04-24
    • PCT/JP2007/070157
    • 2007-10-16
    • 日産化学工業株式会社小山 欣也浅田 根子藤本 修
    • 小山 欣也浅田 根子藤本 修
    • C09C3/08B01J13/00C01F5/28C09C1/02
    • B01J13/00C01F5/28C01P2002/80C01P2004/64C09C3/08Y10S977/773Y10S977/834Y10T428/2991
    • 【課題】フッ化物コロイド粒子を核としてその表面を有機リン化合物により被覆して得られる、表面変性されたフッ化物コロイド粒子のオルガノゾルとその製造方法を提供すること。 【解決手段】フッ化物コロイド粒子を核としてその表面を下記の一般式(1)、(2)及び(3)で表される有機リン化合物からなる群より選ばれる少なくとも1種の有機リン化合物により被覆して得られる、表面変性されたフッ化物コロイド粒子のオルガノゾル。  (R-O) n P(=O)(OM) 3-n  (1)  (R-O) n P(OM) 3-n  (2) (R) n P(=O)(OM) 3-n  (3) 但し、Rは置換又は未置換のアルキル基、アルケニル基又はアリール基を表し、Mは水素原子、アルカリ金属又はNZ 4 (Zは水素原子又はアルキル基を表す。)を表し、そしてnは1又は2の整数を表す。
    • 本发明提供一种表面改性氟化物胶体颗粒的有机溶胶,其通过用有机磷化合物涂布含有氟化物胶体颗粒的芯的表面而制备,并且还提供了制备该有机溶胶的方法。 解决问题的手段通过将包含氟化物胶体颗粒的芯的表面与至少一种选自以下的有机磷化合物的有机磷化合物进行涂布而制造的表面改性氟化物胶体粒子的有机溶胶 式(1),(2)和(3)。 (RO)P(= O)(OM)3-n(1)(RO)n P(OM) 3-n(2)(R)n P(= O)(OM)3-n(3)其中R表示取代或未取代的烷基 ,烯基或芳基; M表示氢原子,碱金属或NZ 4(其中Z表示氢原子或烷基); n表示1或2的整数。