    • Method for increasing the dry residue in processed cyclone dust
    • 增加加工旋风粉尘中残渣的方法
    • US20040136889A1
    • 2004-07-15
    • US10467905
    • 2003-11-25
    • Hans-Jorg BonathGeorg Bombeck
    • C22B034/10
    • A62D3/33A62D2101/43C22B7/008C22B7/02C22B34/1222Y02P10/23Y02P10/234
    • During processing of cyclone dust (4) resulting from the chlorination of titanium ore, a disposable filter cake (26) having a dry residue of greater than 40% (without inert portions serving as a supporting structure), regardless of whether ilmenite, slag or natural or artificial rutile or mixtures thereof were used as a raw material, is obtained when one or a combination of the following method steps is carried out: before increasing to a pH value ranging from 9 to 12 in a neutralization tank (13), a rapid neutralization step (12) is conducted whereby for all volume elements of the liquid, the same precipitation conditions can be maintained in a pH range of 6 to 9; a (preferably anionic) flocculation aid (22) is added before thickening, and; a (preferably cationic) second flocculation aid is mixed into the slurry after thickening. All measures improve the flocculation and render the processing more economical.
    • 在处理由钛矿石氯化产生的旋风粉尘(4)的过程中,具有大于40%(无惰性部分作为支撑结构)的干燥残余物的一次性滤饼(26),不管钛铁矿,矿渣或 使用天然或人造金红石或其混合物作为原料,当进行以下方法步骤之一或组合时获得:在中和罐(13)中增加至9至12的pH值之前, 进行快速中和步骤(12),对于液体的所有体积元素,相同的沉淀条件可以保持在6至9的pH范围内; 在增稠之前加入(优选阴离子)絮凝助剂(22),和 将(优选阳离子)第二絮凝助剂在增稠后混入浆料中。 所有措施都能改善絮凝,使处理更加经济。