    • 3. 发明授权
    • Nickel crucible for melting analytical sample, method of preparing analytical sample and method of analysis
    • 用于熔化分析样品的镍坩埚,制备分析样品的方法和分析方法
    • US07892843B2
    • 2011-02-22
    • US12278889
    • 2007-02-15
    • Masahiro SakaguchiMitsuru YamaguchiTomio TakahashiKouichi Takemoto
    • Masahiro SakaguchiMitsuru YamaguchiTomio TakahashiKouichi Takemoto
    • G01N33/20B01N3/00G01N1/22
    • G01N1/44B01L3/04B01L2300/12Y10T436/25875
    • A nickel crucible used for melting an analytical sample in the pretreatment of the analytical sample, characterized in that the purity of the nickel crucible is 99.9999 wt % or higher. Also provided is a method of analysis, comprising melting a sample by the use of the nickel crucible for melting having a purity of 99.9999 wt % or higher, and analyzing the melt to thereby obtain an analytical result in which the respective lower limits of determination of Mn, Al, Si, Mg, Pb, Fe, Co, Ti, Cu, Cr, Zr, Mo, and W are Mn: 5 wtppm, Al: 10 wtppm, Si: 10 wtppm, Mg: 5 wtppm, Pb: 5 wtppm, Fe: 5 wtppm, Co: 5 wtppm, Ti: 20 wtppm, Cu: 20 wtppm, Cr: 10 wtppm, Zr: 5 wtppm, Mo: 2 wtppm, and W: 10 wtppm. In light of the recent analytical technology demanded of fast and accurate measurement of high purity materials, high purity analysis is attained through inhibition of mixing of impurities from the crucible.
    • 用于在分析样品的预处理中熔化分析样品的镍坩埚,其特征在于,所述镍坩埚的纯度为99.9999重量%以上。 还提供了一种分析方法,包括通过使用纯度为99.9999重量%以上的熔融用镍坩埚来熔解样品,分析熔融物,得到分析结果,其中, Mn,Al,Si,Mg,Pb,Fe,Co,Ti,Cu,Cr,Zr,Mo和W分别为Mn:5重量ppm,Al:10重量ppm,Si:10重量ppm,Mg:5重量ppm,Pb:5 重量ppm,Fe:5重量ppm,Co:5重量ppm,Ti:20重量ppm,Cu:20重量ppm,Cr:10重量ppm,Zr:5重量ppm,Mo:2重量ppm,W:10重量ppm。 鉴于最近需要快速准确地测量高纯度材料的分析技术,通过抑制来自坩埚的杂质的混合来获得高纯度分析。