    • 6. 发明申请
    • ISOCYANATE-EPOXIDE HYBRID RESINS
    • 异氰酸酯 - 环氧树脂混合树脂
    • US20160090436A1
    • 2016-03-31
    • US14890847
    • 2014-05-08
    • BASF SE
    • Frank PRISSOKAndre KAMM
    • C08G18/00
    • C08G18/003C08G18/10C08G18/2063C08G2190/00C09D175/04
    • The present invention relates to a method for producing at least one resin, which comprises mixing at least one polyisocyanate with at least one polyepoxide, the reaction taking place in the presence of a catalyst system based on at least one metal-free Lewis base having at least one nitrogen atom, and also to resins obtainable by a method of the invention, and to the use of a resin obtainable by a method of the invention, or of a resin of the invention, for producing seals, for producing components for rotor blades, boat hulls, or vehicle body parts, or for coatings.
    • 本发明涉及一种生产至少一种树脂的方法,该方法包括将至少一种多异氰酸酯与至少一种聚环氧化物混合,所述反应在基于至少一种不含金属的路易斯碱的催化剂体系的存在下进行,所述催化剂体系具有 至少一个氮原子,以及可通过本发明的方法获得的树脂,以及通过本发明的方法获得的树脂或本发明的树脂用于生产用于生产用于转子叶片的部件的密封件 船体,车身部件或涂料。
    • 10. 发明申请
    • METHOD FOR PREPARING EMULSION RESIN COMPOSITION FOR CATIONIC ELECTRODEPOSITION PAINT
    • 用于阳离子电沉积涂料的乳液树脂组合物的制备方法
    • US20140235756A1
    • 2014-08-21
    • US14345674
    • 2013-02-27
    • NIPPON PAINT CO., LTD.
    • Noriyuki NakazawaMasahiko HaradaYotaro Abe
    • C08L63/00
    • C08L63/00C08G18/003C08G18/2825C08G18/2855C08G18/73C08G18/755C08G18/7664C08G18/7671C08G18/8064C08G18/8074C08G18/8077C08G59/4028C09D5/022C09D5/4438C09D163/00C09D175/04
    • The present invention is to provide a method for preparing an emulsion resin composition for a cationic electrodeposition paint, which prepare a cationic electrodeposition paint composition as reducing time for desolvation time or eliminating desolvation step. The present invention provide a method for preparing an emulsion resin composition for cationic electrodeposition paint, which comprises a cationic resin and a blocked isocyanate curing agent, the method comprises the steps: (1) a step of mixing water and the cationic resin to form a W/O emulsion, (2) a step of mixing the blocked isocyanate curing agent and the W/O emulsion to form a curing agent-containing W/O emulsion, (3) a step of mixing water and the curing agent-containing W/O emulsion to form an O/W emulsion, via a phase inversion point from W/O emulsion to O/W emulsion, wherein the cationic resin comprises a cationic epoxy resin, and a solid concentration by mass XW/O (%) of the curing agent-containing W/O emulsion and a solid content by mass Xtra (%) at the phase inversion point from W/O emulsion to O/W emulsion satisfy a relation of XW/O−Xtra>3%.
    • 本发明提供一种阳离子电沉积涂料乳液树脂组合物的制备方法,其制备阳离子电沉积涂料组合物作为去溶剂化时间的还原时间或消除去溶剂化步骤。 本发明提供一种阳离子电沉积涂料乳液树脂组合物的制备方法,其包含阳离子树脂和封端的异氰酸酯固化剂,该方法包括以下步骤:(1)将水与阳离子树脂混合以形成 W / O乳液,(2)将封端异氰酸酯固化剂和W / O乳液混合以形成含固化剂的W / O乳液的步骤,(3)将水和含固化剂的W / O乳液,通过从W / O乳液到O / W乳液的相转化点形成O / W乳液,其中阳离子树脂包含阳离子环氧树脂,固体质量浓度为XW / O(%) 含W固化剂的W / O乳液,W / O乳液到O / W乳液的相转化点固体含量Xtra(%)满足XW / O-Xtra> 3%的关系。