    • Synthesis and use of ZSM-12
    • ZSM-12的合成与应用
    • US20110034749A1
    • 2011-02-10
    • US12850060
    • 2010-08-04
    • Wenyih Frank LaiJeffrey T. ElksRobert E. Kay
    • Wenyih Frank LaiJeffrey T. ElksRobert E. Kay
    • C07C15/08C01B39/04C01B39/42
    • B01J29/7034C01B39/42C07C6/126C07C2529/70C10G45/64C10G2300/1096C10G2400/30Y02P20/52C07C15/08
    • A process is described for synthesizing a porous, crystalline material having the framework structure of ZSM-12 of the formula: (n)YO2:X2O3 wherein X is a trivalent element, Y is a tetravalent element and n is between about 80 and about 250. In the process, a mixture capable of forming said material is prepared comprising sources of alkali or alkaline earth metal (M), an oxide of trivalent element (X), an oxide of tetravalent element (Y), hydroxyl ions (OFF), water and tetraethylammonium cations (R), wherein said mixture has a composition, in terms of mole ratios, within the following ranges: YO2/X2O3=100 to 300; H2O/YO2=5 to 15; OH−/YO2=0.10 to 0.30; M/YO2=0.05 to 0.30; and R/YO2=0.10 to 0.20. The mixture is reacted at a temperature of at least about 300° F. (149° C.) for a time of less than about 50 hours to form crystals of the crystalline material and the crystalline material is then recovered.
    • 描述了一种用于合成具有下式的ZSM-12的骨架结构的多孔结晶材料的方法:(n)YO 2:X 2 O 3其中X是三价元素,Y是四价元素,n在约80和约250之间 在该方法中,制备能够形成所述材料的混合物,其包含碱金属或碱土金属(M),三价元素(X)的氧化物,四价元素(Y)的氧化物,羟基离子(OFF), 水和四乙基铵阳离子(R),其中所述混合物的摩尔比为组成,在以下范围内:YO 2 / X 2 O 3 = 100至300; H2O / YO2 = 5〜15; OH- / YO 2 = 0.10〜0.30; M / YO2 = 0.05〜0.30; R / YO2 = 0.10〜0.20。 混合物在至少约300°F(149℃)的温度下反应约少于约50小时,形成晶体,然后回收结晶物质。