    • Fire-resistant steel material superior in HAZ toughness of welded joint and method of production of same
    • 焊接接头HAZ韧性优良的耐火钢材料及其制造方法
    • US08323561B2
    • 2012-12-04
    • US12224253
    • 2007-09-20
    • Yasushi HasegawaSuguru YoshidaYoshiyuki Watanabe
    • Yasushi HasegawaSuguru YoshidaYoshiyuki Watanabe
    • C22C38/22C21D8/00C22C38/00
    • C21D8/021C21D1/54C21D6/002C21D9/46C21D9/50C21D2211/005C22C38/001C22C38/02C22C38/04C22C38/24
    • The present invention provides a fire-resistant steel material superior in HAZ toughness of a welded joint which is high in high temperature yield strength at an envisioned fire temperature of 700 to 800° C. and is free of embrittlement of the welded joint even if exposed at this envisioned fire temperature and a method of production of the same, that is, a fire-resistant steel material of a composition containing, by mass %, C: 0.005% to less than 0.03%, Si: 0.01 to 0.50%, Mn: 0.05 to 0.40%, Cr: 1.50 to 5.00%, V: 0.05 to 0.50%, and N: 0.001 to 0.005% and restricted in contents of Ni, Cu, Mo, B, P, S, and O obtained by heating a steel slab to 1150 to 1300° C., then hot working or hot rolling the slab to an end temperature of 880 degrees or more, acceleratedly cooling the worked or rolled steel material under conditions of a cooling rate at a position of the slowest cooling rate of at least 2° C./sec or more, stopping this accelerated cooling at a temperature region where the surface temperature of the steel material becomes 350 to 600° C., and then allowing the material to cool.
    • 本发明提供一种在700-800℃的预期的火焰温度下,在高温屈服强度高的焊接接头的HAZ韧性优异的耐火钢材料,即使暴露于焊接接头也不会发生脆化 在这种预想的耐火温度及其制造方法中,即,以质量%计含有C:0.005〜小于0.03%的Si:0.01〜0.50%的组成的耐火钢材,Mn:0.01〜 :0.05〜0.40%,Cr:1.50〜5.00%,V:0.05〜0.50%,N:0.001〜0.005%,通过加热得到的Ni,Cu,Mo,B,P,S, 钢板坯坯为1150〜1300℃,然后热轧或热轧板坯至880度以上的终止温度,在冷却速度最慢的位置的条件下,对加工后的钢材进行加速冷却 至少2℃/ sec以上,在表面的温度区域停止加速冷却 钢材的温度变为350〜600℃,然后使材料冷却。
    • 6. 发明申请
    • Fire-Resistant Steel Material Superior in Haz Toughness of Welded Joint and Method of Production of Same
    • 焊接接头耐火韧性优良的耐火钢材料及其生产方法
    • US20090053097A1
    • 2009-02-26
    • US12224253
    • 2007-09-20
    • Yasushi HasegawaSuguru YoshidaYoshiyuki Watannabe
    • Yasushi HasegawaSuguru YoshidaYoshiyuki Watannabe
    • C22C38/22C22C38/00C21D8/00
    • C21D8/021C21D1/54C21D6/002C21D9/46C21D9/50C21D2211/005C22C38/001C22C38/02C22C38/04C22C38/24
    • The present invention provides a fire-resistant steel material superior in HAZ toughness of a welded joint which is high in high temperature yield strength at an envisioned fire temperature of 700 to 800° C. and is free of embrittlement of the welded joint even if exposed at this envisioned fire temperature and a method of production of the same, that is, a fire-resistant steel material of a composition containing, by mass %, C: 0.005% to less than 0.03%, Si: 0.01 to 0.50%, Mn: 0.05 to 0.40%, Cr: 1.50 to 5.00%, V: 0.05 to 0.50%, and N: 0.001 to 0.005% and restricted in contents of Ni, Cu, Mo, B, P, S, and O obtained by heating a steel slab to 1150 to 1300° C., then hot working or hot rolling the slab to an end temperature of 880 degrees or more, acceleratedly cooling the worked or rolled steel material under conditions of a cooling rate at a position of the slowest cooling rate of at least 2° C./sec or more, stopping this accelerated cooling at a temperature region where the surface temperature of the steel material becomes 350 to 600° C., and then allowing the material to cool.
    • 本发明提供一种在700-800℃的预期的火焰温度下,在高温屈服强度高的焊接接头的HAZ韧性优异的耐火钢材料,即使暴露于焊接接头也不会发生脆化 在这种预想的耐火温度及其制造方法中,即,以质量%计含有C:0.005〜小于0.03%的Si:0.01〜0.50%的组成的耐火钢材,Mn:0.01〜 :0.05〜0.40%,Cr:1.50〜5.00%,V:0.05〜0.50%,N:0.001〜0.005%,通过加热得到的Ni,Cu,Mo,B,P,S, 钢板坯坯为1150〜1300℃,然后热轧或热轧板坯至880度以上的终止温度,在冷却速度最慢的位置的条件下,对加工后的钢材进行加速冷却 至少2℃/ sec以上,在表面的温度区域停止加速冷却 钢材的温度变为350〜600℃,然后使材料冷却。
    • 8. 发明申请
    • Automobile-Use High Pressure Fuel Injection Accumulator-Distributor and Method of Production of the Same
    • 汽车用高压燃油喷射蓄能器 - 分配器及其生产方法
    • US20100095934A1
    • 2010-04-22
    • US11989844
    • 2006-07-31
    • Yasushi HasegawaRyuichi HonmaYutaka Takagi
    • Yasushi HasegawaRyuichi HonmaYutaka Takagi
    • F02M63/00F02M61/14
    • F02M55/025F02M55/005F02M2200/803F02M2200/8053F02M2200/8084
    • An automobile-use high pressure fuel injection accumulator-distributor comprised of a body of an automobile-use high pressure fuel injection accumulator-distributor to which pipe attachment holders for attaching fuel distribution pipes for distributing fuel to injection nozzles at an equal pressure are joined by liquid phase diffusion bonding etc., wherein each holder is comprised of a tube part at the pipe side and a partial cone-shaped skirt at the end of the rail body side, each holder skirt has a shape spreading in a partial cone shape toward the joint face end with an angle from the holder tube part side face of 10° or more in a range of a length of 2 mm or more in the holder axial direction at the outer circumference of the end of the holder at the joint face side, the rail body has holder joint position determining guide grooves at its holder joint positions, each guide groove is comprised of a groove inner circumferential wall of a size enabling engagement with a holder joint inner circumference, a groove bottom forming a joint face with the holder, and a groove outer circumferential wall of a partial cone shape bulging out to the inner side parallel to the holder skirt from the groove bottom toward the holder side at a depth of 2 mm or more, and a metal ring is plastically deformed and press-fit into a clearance of 0.5 mm or more between each holder skirt and the groove outer circumferential wall and parallel to the joint face.
    • 一种汽车用高压燃料喷射蓄能器 - 分配器,由汽车用高压燃料喷射蓄能器 - 分配器的主体组成,用于将用于将燃料分配到等压喷嘴的燃料分配管的管附接保持器连接到其上 液相扩散接合等,其中每个保持器由在管侧的管部分和在轨道体侧的端部处的部分锥形裙部组成,每个保持器裙部具有朝向 在保持器轴向方向上,在保持器的端部的外周的接合面侧,在保持器管部侧面10°以上的长度为2mm以上的范围内, 轨道体在其保持器接合位置处具有保持器关节位置确定引导槽,每个引导槽由具有能够与保持器接合部配合的尺寸的槽内周壁 内圆周,形成与保持器的接合面的槽底部,以及从凹槽底部向保持器侧平行于保持器裙部的内侧凸出的部分锥形的凹槽外周壁以2mm的深度 以上,并且金属环塑性变形并且压配合在每个保持器裙部和槽外周壁之间并平行于接合面的0.5mm以上的间隙。