    • Superabsorbent polymer containing clay, particulate, and method of making same
    • 含有粘土,颗粒的超吸收性聚合物及其制造方法
    • US08222477B2
    • 2012-07-17
    • US12254434
    • 2008-10-20
    • Michael M. AzadScott J. SmithMark JoyGeoffrey Wyatt BlakeMichael S. Jarman
    • Michael M. AzadScott J. SmithMark JoyGeoffrey Wyatt BlakeMichael S. Jarman
    • A61F13/15
    • A61L15/60A61F13/53A61L15/18A61L15/24A61L15/46C08J3/12C08J3/128C08J2300/14Y10T428/2982
    • A process for the preparation of superabsorbent polymer containing clay, the process including the steps of (I) polymerizing a polymerization mixture comprising: (a) one or more ethylenically unsaturated carboxyl-containing monomers, (b) one or more crosslinking agents, (c) optionally one or more comonomers copolymerizable with the carboxyl-containing monomer, (d) neutralizing agent to partially neutralize the polymer to from about 50% to about 99%, by weight, and (e) a polymerization medium, to form a crosslinked partially neutralized hydrogel, (II) admixing a clay with the crosslinked partially neutralized hydrogel to form partially neutralized superabsorbent polymer-clay hydrogel; (III) drying the crosslinked partially neutralized hydrogel at a temperature from about 190° C. to about 210° C. and for a time period of from about 15 minutes to about 120 minutes, and (IV) comminuting the dried partially neutralized superabsorbent polymer-clay hydrogel to particles.
    • 一种制备含有粘土的超吸收聚合物的方法,所述方法包括以下步骤:(I)聚合混合物,其包含:(a)一种或多种烯属不饱和羧酸单体,(b)一种或多种交联剂,(c )任选地一种或多种可与含羧基单体共聚的共聚单体,(d)中和剂以将聚合物部分中和至约50%至约99%(重量),和(e)聚合介质,以形成部分交联 中和的水凝胶,(II)将粘土与交联的部分中和的水凝胶混合以形成部分中和的超吸收聚合物 - 粘土水凝胶; (III)在约190℃至约210℃的温度下干燥交联的部分中和的水凝胶,并且持续约15分钟至约120分钟的时间段,和(IV)粉碎干燥的部分中和的超吸收聚合物 将水凝胶粘贴到颗粒上。
    • 9. 发明申请
    • SUPERABSORBENT POLYMER HAVING INCREASED RATE OF WATER ABSORPTION
    • 具有增加吸水率的超吸收聚合物
    • US20070088093A1
    • 2007-04-19
    • US11610749
    • 2006-12-14
    • Mark JoyWhei-Neen Hsu
    • Mark JoyWhei-Neen Hsu
    • C08J9/30
    • A61L15/60C08L33/10C08L33/08
    • The invention relates to a superabsorbent polymer wherein an increased rate of water absorption is obtained by the addition of an encapsulated blowing agent. The invention relates to a superabsorbent polymer including an encapsulating blowing agent and having a vortex time of 40 seconds or less. In particular, the superabsorbent polymer includes from about 55 to about 99.9 wt. % of polymerizable unsaturated acid group containing monomers; from about 0.001 to about 5.0 wt. % of internal crosslinking agent; wherein the wherein the composition has a degree of neutralization of more than about 20%; and from about 0.05 to about 10.0 wt. % of an encapsulated blowing agent.
    • 本发明涉及一种超吸收性聚合物,其中通过加入包封的发泡剂获得增加吸水率。 本发明涉及一种包含发泡剂的超吸收性聚合物,其旋涡时间为40秒以下。 特别地,超吸收性聚合物包括约55-约99.9wt。 %的含可聚合不饱和酸基团的单体; 约0.001至约5.0wt。 %的内部交联剂; 其中所述组合物具有大于约20%的中和度; 和约0.05至约10.0重量% %的封装发泡剂。