    • STEEL PIPE EXCELLENT IN DEFORMATION CHARACTERISTICS AND METHOD OF PRODUCING THE SAME
    • 钢管在变形特性方面表现出色,其生产方法也是如此
    • US20100119860A1
    • 2010-05-13
    • US12452765
    • 2008-07-22
    • Asahi HitoshiTetsuo IshitsukaMotofumi KoyubaToshiyuki Ogata
    • Asahi HitoshiTetsuo IshitsukaMotofumi KoyubaToshiyuki Ogata
    • B32B1/08C22C38/58C22C38/42C22C38/54C21D9/08C22C38/04
    • C22C38/04C21D8/105C21D9/08Y10T428/12292
    • The invention provides a steel pipe excellent in deformation characteristics, most notably a steel pipe for expandable-pipe oil well and a low-yield-ratio line pipe, and a method of producing the same without conducting water cooling requiring large-scale heat treatment equipment, namely a method of producing a steel pipe excellent in deformation characteristics whose microstructure is a two-phase structure including a martensite-austenite constituent at an area fraction of 2 to 10% and a soft phase, which method comprises: heating at Ac1+10° C. to Ac1+60° C. and thereafter cooling a precursor steel pipe which contains, in mass %, C: 0.04 to 0.10% and Mn: 1.00 to 2.50%, is limited to Si: 0.80% or less, P: 0.03% or less, S: 0.01% or less, Al: 0.10% or less and N: 0.01% or less, further contains one or more of Ni: 1.00% or less, Mo: 0.60% or less, Cr: 1.00% or less and Cu: 1.00% or less, where content of Mn and content of one or more of Cr, Ni, Mo and Cu satisfy Mn+Cr+Ni+2Mo+Cu≧2.00, and a balance of iron and unavoidable impurities.
    • 本发明提供一种变形特性优异的钢管,特别是可膨胀管油管用钢管和低屈服比管线管,以及不进行需要大型热处理设备的水冷却的制造方法 即具有优异的变形特性的钢管的制造方法,其特征在于微结构为包含2〜10%面积分数的马氏体 - 奥氏体组分和软相的两相组织,该方法包括:在Ac1 + 10 ℃至Ac1 + 60℃,然后将质量%C:0.04〜0.10%,Mn:1.00〜2.50%的前体钢管冷却至Si:0.80%以下,P: 0.03%以下,S:0.01%以下,Al:0.10%以下,N:0.01%以下,还含有Ni:1.00%以下,Mo:0.60%以下,Cr:1.00% 以下,Cu:1.00%以下,其中,Cr,Ni,Mo,Cu中的一种以上的Mn含量满足Mn + Cr + Ni + 2Mo +Cu≥2.00, 和铁和不可避免的杂质的平衡。
    • 6. 发明授权
    • Steel pipe excellent in deformation characteristics and method of producing the same
    • 变形特性优良的钢管及其制造方法
    • US08920583B2
    • 2014-12-30
    • US12452765
    • 2008-07-22
    • Hitoshi AsahiTetsuo IshitsukaMotofumi KoyubaToshiyuki Ogata
    • Hitoshi AsahiTetsuo IshitsukaMotofumi KoyubaToshiyuki Ogata
    • B32B1/08C22C38/58C22C38/42C22C38/54C22C38/04C21D9/08C21D8/10
    • C22C38/04C21D8/105C21D9/08Y10T428/12292
    • The invention provides a steel pipe excellent in deformation characteristics, most notably a steel pipe for expandable-pipe oil well and a low-yield-ratio line pipe, and a method of producing the same without conducting water cooling requiring large-scale heat treatment equipment, namely a method of producing a steel pipe excellent in deformation characteristics whose microstructure is a two-phase structure including a martensite-austenite constituent at an area fraction of 2 to 10% and a soft phase, which method comprises: heating at Ac1+10° C. to Ac1+60° C. and thereafter cooling a precursor steel pipe which contains, in mass %, C: 0.04 to 0.10% and Mn: 1.00 to 2.50%, is limited to Si: 0.80% or less, P: 0.03% or less, S: 0.01% or less, Al: 0.10% or less and N: 0.01% or less, further contains one or more of Ni: 1.00% or less, Mo: 0.60% or less, Cr: 1.00% or less and Cu: 1.00% or less, where content of Mn and content of one or more of Cr, Ni, Mo and Cu satisfy Mn+Cr+Ni+2Mo+Cu≧2.00, and a balance of iron and unavoidable impurities.
    • 本发明提供一种变形特性优异的钢管,特别是可膨胀管油管用钢管和低屈服比管线管,以及不进行需要大型热处理设备的水冷却的制造方法 即具有优异的变形特性的钢管的制造方法,其特征在于微结构为包含2〜10%面积分数的马氏体 - 奥氏体组分和软相的两相组织,该方法包括:在Ac1 + 10 ℃至Ac1 + 60℃,然后将质量%C:0.04〜0.10%,Mn:1.00〜2.50%的前体钢管冷却至Si:0.80%以下,P: 0.03%以下,S:0.01%以下,Al:0.10%以下,N:0.01%以下,还含有Ni:1.00%以下,Mo:0.60%以下,Cr:1.00% 以下,Cu:1.00%以下,其中,Cr,Ni,Mo,Cu中的一种以上的Mn含量满足Mn + Cr + Ni + 2Mo +Cu≥2.00, 和铁和不可避免的杂质的平衡。