    • 1. 发明授权
    • Process for preparing mica-containing ceramic composite
    • 制备含云母陶瓷复合材料的方法
    • US5180532A
    • 1993-01-19
    • US461911
    • 1990-01-08
    • Tadaki MurakamiTakashi ShirazawaKazuharu Kato
    • Tadaki MurakamiTakashi ShirazawaKazuharu Kato
    • C04B35/16C04B32/00C04B35/18C04B35/645
    • C04B35/18C04B32/00C04B35/645
    • Mica-containing ceramic composite having excellent characteristics such as capability of machining work, a small thermal expansion coefficient, high heat-shock resistant temperature difference as well as high heat deformation temperature, is prepared by: a) preparing powder mixture by blending 20 to 50% by weight of mica powder, 15 to 40% by weight of zinc oxide powder, 10 to 20% by weight of silica powder, 8 to 20% by weight of boric acid powder, and 4 to 20% by weight of cordierite powder; b) heating the powder mixture at a temperature of from 940.degree. C. to 1,050.degree. C. to prepare baked product; c) pulverizing the baked product into very fine powder to thereby obtain a shaping material; d) adding an organic binder to the shaping material to prepare a shaping composition; and e) shaping the shaping composition into a shaped body and heating a shaped body at a temperature ranging from 940.degree. C. to 1,050.degree. C. with simultaneous application of pressure to the shaped body to render the same into a baked body.
    • 通过以下方法制备具有加工性能优异,热膨胀系数小,耐热冲击温差高,热变形温度高等特性的含云母陶瓷复合体,其通过以下方法制备:a)通过混合20〜50 云母粉重量百分数,氧化锌粉末重量为15〜40%,二氧化硅粉末为10〜20重量%,硼酸粉末为8〜20重量%,堇青石粉末为4〜20重量%。 b)在940℃至1050℃的温度下加热粉末混合物以制备烘烤产品; c)将烘焙产品粉碎成非常细的粉末,从而获得成型材料; d)向成型材料中加入有机粘合剂以制备成型组合物; 和e)将成形组合物成形为成形体,并在940℃至1050℃的温度范围内加热成型体,同时向成形体施加压力以使其成为烘烤体。