热词
    • 1. 发明申请
    • TRANSPARENT CONDUCTOR AND TOUCH PANEL
    • 透明导体和触控面板
    • US20150205409A1
    • 2015-07-23
    • US14600746
    • 2015-01-20
    • TDK CORPORATION
    • Hiroshi SHINGAIMinoru FUJITAMasahiro OISHI
    • G06F3/044G06F1/16
    • G06F3/044C23C14/08C23C14/3414G06F1/16
    • The transparent conductor includes a transparent substrate, a first metal oxide layer, a metal layer, and a second metal oxide layer laminated. At least one of the first and the second metal oxide layers contains four components of Al2O3, ZnO, SnO2, and Ga2O3. X, Y, and Z are within a region surrounded by line segments between point a, point b, point c, point d, point e, and point f, in terms of (X, Y, Z) coordinates shown in a ternary diagram in FIG. 2, or on the line segments where X is a total molar ratio of the Al2O3 and the ZnO, Y is a molar ratio of the SnO2, and Z is a molar ratio of the Ga2O3, relative to the total amount of the four components. A molar ratio of the Al2O3 relative to the total amount of the four components is 1.5 to 3.5% by mole.
    • 透明导体包括层叠的透明基板,第一金属氧化物层,金属层和第二金属氧化物层。 第一和第二金属氧化物层中的至少一个包含Al 2 O 3,ZnO,SnO 2和Ga 2 O 3的四种成分。 X,Y,Z分别位于由点(a,b,点c,点d,点e,点f)之间的线段包围的区域内, 在图中。 2,或在X是Al 2 O 3和ZnO的总摩尔比的线段上,Y是SnO 2的摩尔比,Z是相对于四种组分的总量的Ga 2 O 3的摩尔比。 Al 2 O 3相对于四种成分的总量的摩尔比为1.5〜3.5摩尔%。