热词
    • 4. 发明申请
    • SILICA CONTAINER AND METHOD FOR PRODUCING THE SAME
    • 二氧化硅容器及其制造方法
    • US20110272322A1
    • 2011-11-10
    • US13145063
    • 2010-10-19
    • Shigeru YamagataTomomi Usui
    • Shigeru YamagataTomomi Usui
    • B65D85/00C03B19/06C03B19/09C03B20/00
    • B65D13/02C03B19/095C03B2201/54C03C3/06C03C2201/54C30B15/10C30B29/06C30B35/002Y02P40/57
    • The present invention is a method for producing a silica container having a substrate containing gaseous bubbles in its outer peripheral part and an inner layer comprised of a transparent silica glass formed on an inner surface of the substrate, wherein a powdered raw material for forming a substrate containing Li, Na, and K with the total concentration of 50 or less ppm by weight and a powdered raw material for forming an inner layer containing Ca, Sr, and Ba with the total concentration of 50 to 2000 ppm by weight are prepared; a preliminarily molded substrate is formed in a frame; a preliminarily molded inner layer is formed on an inner surface of the preliminarily molded substrate; and the preliminarily molded substrate and molded inner layer are heated from inside thereof by a discharge-heat melting method under a gas atmosphere containing a hydrogen gas or a helium gas or a gas mixture thereof with the ratio of more than 10% by volume thereby making an outer peripheral part of the preliminarily molded substrate to a sintered body and an inner peripheral part of the preliminarily molded substrate and the preliminarily molded inner layer to a fused glass body. With this, a method for producing a silica container, producible with a low cost and having a high durability and dimensional precision, and a container of this sort can be provided.
    • 本发明是一种生产二氧化硅容器的方法,该二氧化硅容器具有在其外周部分含有气泡的基底和由形成在基材的内表面上的透明石英玻璃构成的内层,其中形成基材的粉末原料 含有总浓度为50以下的Li,Na和K,并且制备总重量为50〜2000ppm的含有Ca,Sr,Ba的内层的粉末状原料。 在框架中形成预成型基板; 在预成型基板的内表面上形成预成型内层, 并且通过放电加热熔融法在含有大于10体积%的氢气或氦气或其气体混合物的气体气氛下从其内部加热预成型基板和模制内层,从而使 将预成型基板的外周部分与烧结体和预成型基板的内周部分和预成型的内层部分连接到熔融玻璃体。 由此,可以提供一种生产低成本,高耐久性和尺寸精度的二氧化硅容器的制造方法和这种容器。
    • 6. 发明申请
    • SILICA CONTAINER AND METHOD FOR PRODUCING THE SAME
    • 二氧化硅容器及其制造方法
    • US20110240663A1
    • 2011-10-06
    • US13131987
    • 2010-06-25
    • Shigeru YamagataTomomi Usui
    • Shigeru YamagataTomomi Usui
    • B65D6/00C03B19/09B32B1/02
    • C03B19/095C03B2201/07C03B2201/075C03B2201/32C30B15/10C30B29/06C30B35/002Y10T428/131Y10T428/1317Y10T428/2982
    • A method for producing a silica container having a rotational symmetry is provided. The method includes, forming a preliminarily molded article by feeding a powdered substrate's raw material to an inner wall of an outer frame having aspiration holes with rotating the frame, and forming a silica substrate. The preliminarily molded article is aspirated from an outer peripheral side with controlling a humidity inside the outer frame by ventilating gases present in the outer frame with charging from inside the preliminarily molded article a gas mixture comprised of an O2 gas and an inert gas and made below a prescribed dew-point temperature by dehumidification, and at the same time heated from inside the preliminarily molded article by a discharge-heat melting method with carbon electrodes, thereby making an outer peripheral part of the preliminarily molded article to a sintered body while an inner peripheral part to a fused glass body.
    • 提供了具有旋转对称性的二氧化硅容器的制造方法。 该方法包括:通过将粉末状基材的原料供给到具有旋转框架的抽吸孔的外框架的内壁,形成二氧化硅基板来形成预成型品。 从外周侧抽吸预成型品,通过从外部框架内部充填从O 2气体和惰性气体构成的气体混合物从外部框架内的气体通风来控制外框内的湿度, 通过除湿规定的露点温度,同时用碳电极通过放电加热熔融法从预成型体内部加热,由此使预成型品的外周部分成为烧结体,而内部 周边部分为熔融玻璃体。
    • 7. 发明授权
    • Silica container and method for producing the same
    • 二氧化硅容器及其制造方法
    • US08733127B2
    • 2014-05-27
    • US13123629
    • 2010-06-01
    • Shigeru YamagataTomomi Usui
    • Shigeru YamagataTomomi Usui
    • C03B19/09
    • C03B19/09C03B19/095Y02P40/57
    • A method for producing a silica container, the method including forming a preliminarily molded silica substrate to an intended shape by feeding a powdered substrate's raw material (silica particles) to an inner wall of a carbon-made outer frame having aspiration holes with rotating the outer frame, and forming the silica substrate wherein the preliminarily molded substrate is degassed by aspiration from its outer peripheral side with charging from an inner peripheral side of the preliminarily molded silica substrate a reducing gas containing more than 10% by volume of an H2 gas, and at the same time heated from inside the preliminarily molded silica substrate by a discharge-heat melting method with carbon electrodes, thereby making an outer peripheral part of the preliminarily molded silica substrate to a sintered body while an inner peripheral part of the preliminarily molded silica substrate to a fused glass body.
    • 一种二氧化硅容器的制造方法,其特征在于,通过将粉末状基材的原料(二氧化硅粒子)供给到具有抽吸孔的碳制外框的内壁,将预成型的二氧化硅基板形成为预定形状, 框架,并且形成二氧化硅基板,其中通过从预先模塑的二氧化硅基板的内周侧充填含有超过10体积%的H 2气体的还原气体,从其外周侧抽吸预先模塑的基板被脱气,以及 同时用碳电极通过放电加热熔化法从预成型二氧化硅基板内部加热,从而将预先成型的二氧化硅基板的外周部分制成烧结体,而预成型二氧化硅基板的内周部分 到熔融玻璃体。
    • 9. 发明申请
    • SILICA CONTAINER FOR PULLING SINGLE CRYSTAL SILICON AND METHOD FOR PRODUCING THE SAME
    • 用于拉伸单晶硅的硅砂容器及其制造方法
    • US20140041575A1
    • 2014-02-13
    • US14112190
    • 2013-01-22
    • Shigeru Yamagata
    • Shigeru Yamagata
    • C30B15/10
    • C30B15/10C03B19/095C03B2201/03C30B29/06C30B35/002Y02P40/57Y10T117/1032
    • The present invention is directed to a silica container for pulling single crystal silicon, the silica container including a straight body portion, a curved portion, and a bottom portion, wherein the outside of the silica container is made of opaque silica glass containing gaseous bubbles, the inside of the silica container is made of transparent silica glass containing substantially no gaseous bubble, and, on the inner surface of the bottom portion, a silica glass layer containing the OH group in a concentration of more than 300 ppm by mass but 3000 ppm by mass or less, the silica glass layer having a thickness of 20 μm or more but 1000 μm or less, is formed. As a result, a low-cost silica container for pulling single crystal silicon, the silica container that can reduce cavity defects called voids and pinholes in pulled single crystal silicon, is provided.
    • 本发明涉及一种用于拉取单晶硅的二氧化硅容器,该二氧化硅容器包括直体部分,弯曲部分和底部部分,其中二氧化硅容器的外部由含有气泡的不透明二氧化硅玻璃制成, 二氧化硅容器的内部由基本上不含气泡的透明石英玻璃制成,并且在底部的内表面上含有浓度大于300质量ppm但为3000ppm的OH基的二氧化硅玻璃层 以下,形成厚度为20μm以上且1000μm以下的石英玻璃层。 结果,提供了一种用于拉制单晶硅的低成本二氧化硅容器,可以减少被拉制的单晶硅中称为空洞和针孔的空洞缺陷的二氧化硅容器。