    • Metal thin film dispersing a super-fine diamond particle, a metal material having the metal thin film, and a method for preparing the same
    • 分散超细金刚石颗粒的金属薄膜,具有金属薄膜的金属材料及其制备方法
    • US07201972B2
    • 2007-04-10
    • US10460660
    • 2003-06-13
    • Shigeru ShiozakiMasato SoneHideo YoshidaKiyohito SakonTadamasa Fujimura
    • Shigeru ShiozakiMasato SoneHideo YoshidaKiyohito SakonTadamasa Fujimura
    • B32B5/16B32B5/02B32B15/00C25C5/00
    • C25D15/02Y10T428/12486
    • There is provided a metal thin film comprising a metal plate and a diamond particle dispersed in the metal plate. According to the present invention, the metal thin film has a film thickness of 5 nm to 35000 nm. The diamond particle is dispersed almost homogeneously over the direction of the film thickness of the metal thin film. The metal thin film has the diamond particle at a concentration of 1 to 12%. According to the present invention, based on conversion into an equivalent circle, the diamond particle has a first particle size distribution with respect to a first particle of a first particle size of 16 nm or less, at a first number average existence rate of 50% or more; the diamond particle has a second particle size distribution with respect to a second particle having a second particle size of 50 nm or more, at a second number average existence rate of substantially 0%; and the diamond particle has a third particle size distribution with respect to a third particle having a third particle size of 2 nm or less, at a third number average existence rate of substantially 0%.
    • 提供了金属薄膜,其包括分散在金属板中的金属板和金刚石颗粒。 根据本发明,金属薄膜的膜厚为5nm〜35000nm。 金刚石颗粒在金属薄膜的膜厚方向上几乎均匀地分散。 金属薄膜的浓度为1〜12%的金刚石粒子。 根据本发明,基于转换为等效圆,金刚石颗粒相对于第一粒径为16nm或更小的第一粒子以第一数均分子存在率为50%具有第一粒度分布, 或者更多; 所述金刚石颗粒相对于具有第二粒径为50nm或更大的第二颗粒的​​第二粒度分布,其第二数均分子存在率基本为0%; 并且所述金刚石颗粒相对于第三粒径为2nm以下的第三粒子具有基本上为0%的第三数均分率的第三粒度分布。
    • 2. 发明授权
    • Stable aqueous suspension liquid of finely divided diamond particles, metallic film containing diamond particles and method of producing the same
    • 细碎金刚石颗粒的稳定含水悬浮液,含金刚石颗粒的金属膜及其制造方法
    • US08172916B2
    • 2012-05-08
    • US13046372
    • 2011-03-11
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • B24D3/02C09C1/68C09K3/14B01J3/08C01B31/06
    • C25D15/02Y10S428/935Y10T428/12493Y10T428/12625Y10T428/25
    • An aqueous suspension liquid of finely divided diamond particles comprising 0.05 to 160 parts by weight of a finely divided diamond particles in 1000 parts of water, wherein; (i) the finely divided diamond particles have an element composition consisting mainly of 72 to 89.5% by weight of carbon, 0.8 to 1.5% of hydrogen, 1.5 to 2.5% of nitrogen, and 10.5 to 25.0% of oxygen; (ii) and, almost all of said diamond particles are in the range of 2 mu to 50 nm in diameters thereof (80% or more by number average, 70% or more by weight average), (iii) and, said finely divided diamond particles exhibit a strongest peak of the intensity of the Bragg angle at 43.9° (20±20), strong and characteristic peaks at 73.5° (20±20) and 95° (20±2°), a warped halo at 17′ (20±2′), and no peak at 26.5°, by X-ray diffraction (XRD) spectrum analysis using Cu-Ku radiation when dried, (iv) and, specific surface area of said diamond particles when dry state powder is not smaller than 1.50×105 m2/kg, and substantially all the surface carbon atoms of said particles are bonded with hetero atoms, and the total absorption space of said powder is 0.5 m3/kg or more, when dried. The diamond particles are very active and dispersible in aqueous liquid in stable, and have essentially same mechanical properties as that of usual diamonds.
    • 一种细碎金刚石颗粒的水性悬浮液,其包含0.05至160重量份在1000份水中的细碎金刚石颗粒,其中: (i)细碎金刚石颗粒具有主要由碳原子数为72〜89.5重量%,氢为0.8〜1.5%,氮为1.5〜2.5%,氧为10.5〜25.0%的元素组成。 (ii),并且几乎所有的所述金刚石颗粒的直径在2至50nm的范围内(数均为80%或更多,平均为70%或更多),(iii),并且所述细分 金刚石颗粒在43.9°(20±20)处呈现出最强的布拉格角强度峰值,73.5°(20±20)°和95°(20±2°)处的强特征峰,17' (20±2'),26.5°没有峰,通过干燥后使用Cu-Ku辐射的X射线衍射(XRD)光谱分析,(iv)当干态粉末不是时,所述金刚石颗粒的比表面积 小于1.50×105m2 / kg,并且所述颗粒的基本上所有的表面碳原子与杂原子键合,并且当干燥时,所述粉末的总吸收空间为0.5m 3 / kg以上。 金刚石颗粒在水性液体中是非常活泼和可分散的,并且具有与通常的钻石基本上相同的机械性能。
    • 3. 发明申请
    • STABLE AQUEOUS SUSPENSION LIQUID OF FINELY DIVIDED DIAMOND PARTICLES, METALLIC FILM CONTAINING DIAMOND PARTICLES AND METHOD OF PRODUCING THE SAME
    • 含有金刚石颗粒的金属片状金刚石悬浮液的稳定的悬浮液及其制造方法
    • US20110209642A1
    • 2011-09-01
    • US13046372
    • 2011-03-11
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • C09D1/00B82Y30/00
    • C25D15/02Y10S428/935Y10T428/12493Y10T428/12625Y10T428/25
    • An aqueous suspension liquid of finely divided diamond particles comprising 0.05 to 160 parts by weight of a finely divided diamond particles in 1000 parts of water, wherein; (i) the finely divided diamond particles have an element composition consisting mainly of 72 to 89.5% by weight of carbon, 0.8 to 1.5% of hydrogen, 1.5 to 2.5% of nitrogen, and 10.5 to 25.0% of oxygen; (ii) and, almost all of said diamond particles are in the range of 2 mu to 50 nm in diameters thereof (80% or more by number average, 70% or more by weight average), (iii) and, said finely divided diamond particles exhibit a strongest peak of the intensity of the Bragg angle at 43.9° (20±20), strong and characteristic peaks at 73.5° (20±20) and 95° (20±2°), a warped halo at 17′(20±2′), and no peak at 26.5°, by X-ray diffraction (XRD) spectrum analysis using Cu-Ku radiation when dried, (iv) and, specific surface area of said diamond particles when dry state powder is not smaller than 1.50×105 m2/kg, and substantially all the surface carbon atoms of said particles are bonded with hetero atoms, and the total absorption space of said powder is 0.5 m3/kg or more, when dried. The diamond particles are very active and dispersible in aqueous liquid in stable, and have essentially same mechanical properties as that of usual diamonds.
    • 一种细碎金刚石颗粒的水性悬浮液,其包含0.05至160重量份在1000份水中的细碎金刚石颗粒,其中: (i)细碎金刚石颗粒具有主要由碳原子数为72〜89.5重量%,氢为0.8〜1.5%,氮为1.5〜2.5%,氧为10.5〜25.0%的元素组成。 (ii),并且几乎所有的所述金刚石颗粒的直径在2至50nm的范围内(数均为80%或更多,平均为70%或更多),(iii),并且所述细分 金刚石颗粒在43.9°(20±20)处呈现出最强的布拉格角强度峰值,73.5°(20±20)°和95°(20±2°)处的强特征峰,17' (20±2'),26.5°没有峰,通过干燥后使用Cu-Ku辐射的X射线衍射(XRD)光谱分析,(iv)当干态粉末不是时,所述金刚石颗粒的比表面积 小于1.50×105m2 / kg,并且所述颗粒的基本上所有的表面碳原子与杂原子键合,并且当干燥时,所述粉末的总吸收空间为0.5m 3 / kg以上。 金刚石颗粒在水性液体中是非常活泼和可分散的,并且具有与通常的钻石基本上相同的机械性能。
    • 4. 发明申请
    • Stable aqueous suspension liquid of finely divided diamond particles, metallic film containing diamond particles and method of producing the same
    • 细碎金刚石颗粒的稳定含水悬浮液,含金刚石颗粒的金属膜及其制造方法
    • US20100069513A1
    • 2010-03-18
    • US12461135
    • 2009-08-03
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • C09K3/00
    • C25D15/02Y10S428/935Y10T428/12493Y10T428/12625Y10T428/25
    • An aqueous suspension liquid of finely divided diamond particles comprising 0.05 to 160 parts by weight of a finely divided diamond particles in 1000 parts of water, wherein; (i) the finely divided diamond particles have an element composition consisting mainly of 72 to 89.5% by weight of carbon, 0.8 to 1.5% of hydrogen, 1.5 to 2.5% of nitrogen, and 10.5 to 25.0% of oxygen; (ii) and, almost all of said diamond particles are in the range of 2 nm to 50 nm in diameters thereof (80% or more by number average, 70% or more by weight average), (iii) and, said finely divided diamond particles exhibit a strongest peak of the intensity of the Bragg angle at 43.9° (2θ±2°), strong and characteristic peaks at 73.5° (2θ±2°) and 95° (2θ±2°), a warped halo at 17° (2θ±2°), and no peak at 26.5°, by X-ray diffraction (XRD) spectrum analysis using Cu-Kα radiation when dried, (iv) and, specific surface area of said diamond particles when dry state powder is not smaller than 1.50×105 m2/kg, and substantially all the surface carbon atoms of said particles are bonded with hetero atoms, and the total absorption space of said powder is 0.5 m3/kg or more, when dried. The diamond particles are very active and dispersible in aqueous liquid in stable, and have essentially same mechanical properties as that of usual diamonds.
    • 一种细碎金刚石颗粒的水性悬浮液,其包含0.05至160重量份在1000份水中的细碎金刚石颗粒,其中: (i)细碎金刚石颗粒具有主要由碳原子数为72〜89.5重量%,氢为0.8〜1.5%,氮为1.5〜2.5%,氧为10.5〜25.0%的元素组成。 (ii),并且几乎所有的所述金刚石颗粒的直径在2nm至50nm的范围内(数均为80%或更多,平均为70%或更多),(iii),所述细分 金刚石颗粒在43.9°(2θ;±2°)处呈现出最强的布拉格角强度峰值,73.5°(2θ±2°)和95°(2°;±2°)的强和特征峰,a 通过在干燥时使用Cu-Kα辐射的X射线衍射(XRD)光谱分析,(iv)和所述金刚石颗粒的比表面积,在17°(2°和±2°)弯曲的光环,并且在26.5°没有峰 当干态粉末不小于1.50×10 5 m 2 / kg,并且所述颗粒的基本上所有的表面碳原子与杂原子键合时,干燥时所述粉末的总吸收空间为0.5m 3 / kg以上。 金刚石颗粒在水性液体中是非常活泼和可分散的,并且具有与通常的钻石基本上相同的机械性能。
    • 5. 发明授权
    • Stable aqueous suspension liquid of finely divided diamond particles, metallic film containing diamond particles and method of producing the same
    • 细碎金刚石颗粒的稳定含水悬浮液,含金刚石颗粒的金属膜及其制造方法
    • US07115325B2
    • 2006-10-03
    • US10231441
    • 2002-08-30
    • Tadamasa FujimuraMasato SoneValeri Yu. DolmatovShigeru Shiozaki
    • Tadamasa FujimuraMasato SoneValeri Yu. DolmatovShigeru Shiozaki
    • B32B15/00B32B5/00
    • C25D15/02Y10S428/935Y10T428/12493Y10T428/12625Y10T428/25
    • An aqueous suspension liquid of finely divided diamond particles comprising 0.05 to 160 parts by weight of a finely divided diamond particles in 1000 parts of water, wherein; (i) the finely divided diamond particles have an element composition consisting mainly of 72 to 89.5% by weight of carbon, 0.8 to 1.5% of hydrogen, 1.5 to 2.5% of nitrogen, and 10.5 to 25.0% of oxygen; (ii) and, almost all of said diamond particles are in the range of 2 nm to 50 nm in diameters thereof (80% or more by number average, 70% or more by weight average), (iii) and, said finely divided diamond particles exhibit a strongest peak of the intensity of the Bragg angle at 43.9° (2θ±2°), strong and characteristic peaks at 73.5° (2θ±2°)and 95° (2θ±2°), a warped halo at 17° (2θ±2°), and no peak at 26.5°, by X-ray diffraction (XRD) spectrum analysis using Cu-Kα radiation when dried, (iv) and, specific surface area of said diamond particles when dry state powder is not smaller than 1.50×105 m2/kg, and substantially all the surface carbon atoms of said particles are bonded with hetero atoms, and the total absorption space of said powder is 0.5m3/kg or more, when dried. The diamond particles are very active and dispersible in aqueous liquid in stable, and have essentially same mechanical properties as that of usual diamonds.
    • 一种细碎金刚石颗粒的水性悬浮液,其包含0.05至160重量份在1000份水中的细碎金刚石颗粒,其中: (i)细碎金刚石颗粒具有主要由碳原子数为72〜89.5重量%,氢为0.8〜1.5%,氮为1.5〜2.5%,氧为10.5〜25.0%的元素组成。 (ii),并且几乎所有的所述金刚石颗粒的直径在2nm至50nm的范围内(数均为80%或更多,平均为70%或更多),(iii),所述细分 金刚石颗粒在43.9°(2θ±2°)处呈现出最强的布拉格角强度峰值,73.5°(2θ±2°)和95°(2θ±2°)处的强和特征峰, 通过使用Cu-Kalpha辐射干燥时的X射线衍射(XRD)光谱分析,(iv)和当干态粉末时所述金刚石颗粒的比表面积,在17°(2θ±2°),26.5°没有峰 不小于1.50×10 5 / kg,并且所述颗粒的基本上所有的表面碳原子与杂原子键合,并且所述粉末的总吸收空间 干燥时为0.5m 3 / kg以上。 金刚石颗粒在水性液体中是非常活泼和可分散的,并且具有与通常的钻石基本上相同的机械性能。
    • 6. 发明申请
    • Stable aqueous suspension liquid of finely divided diamond particles, metallic film containing diamond particles and method of producing the same
    • 细碎金刚石颗粒的稳定含水悬浮液,含金刚石颗粒的金属膜及其制造方法
    • US20060147644A1
    • 2006-07-06
    • US11335734
    • 2006-01-20
    • Tadamasa FujimuraMasato SoneValeri DolmatovShigeru Shiozaki
    • Tadamasa FujimuraMasato SoneValeri DolmatovShigeru Shiozaki
    • C30B11/00B23K20/08B05D1/18B01J3/06
    • C25D15/02Y10S428/935Y10T428/12493Y10T428/12625Y10T428/25
    • An aqueous suspension liquid of finely divided diamond particles comprising 0.05 to 160 parts by weight of a finely divided diamond particles in 1000 parts of water, wherein; (i) the finely divided diamond particles have an element composition consisting mainly of 72 to 89.5% by weight of carbon, 0.8 to 1.5% of hydrogen, 1.5 to 2.5% of nitrogen, and 10.5 to 25.0% of oxygen; (ii) and, almost all of said diamond particles are in the range of 2 nm to 50 nm in diameters thereof (80% or more by number average, 70% or more by weight average), (iii) and, said finely divided diamond particles exhibit a strongest peak of the intensity of the Bragg angle at 43.9° (2θ±2°), strong and characteristic peaks at 73.5° (2θ±2°)and 95° (2θ±2°), a warped halo at 17° (2θ±2°), and no peak at 26.5°, by X-ray diffraction (XRD) spectrum analysis using Cu—Kα radiation when dried, (iv) and, specific surface area of said diamond particles when dry state powder is not smaller than 1.50×105 m2/kg, and substantially all the surface carbon atoms of said particles are bonded with hetero atoms, and the total absorption space of said powder is 0.5 m3/kg or more, when dried. The diamond particles are very active and dispersible in aqueous liquid in stable, and have essentially same mechanical properties as that of usual diamonds.
    • 一种细碎金刚石颗粒的水性悬浮液,其包含0.05至160重量份在1000份水中的细碎金刚石颗粒,其中: (i)细碎金刚石颗粒具有主要由碳原子数为72〜89.5重量%,氢为0.8〜1.5%,氮为1.5〜2.5%,氧为10.5〜25.0%的元素组成。 (ii),并且几乎所有的所述金刚石颗粒的直径在2nm至50nm的范围内(数均为80%或更多,平均为70%或更多),(iii),所述细分 金刚石颗粒在43.9°(2θ±2°)处呈现出最强的布拉格角强度峰值,73.5°(2θ±2°)和95°(2θ±2°)处的强和特征峰, 通过使用Cu-Kalpha辐射干燥时的X射线衍射(XRD)光谱分析,(iv)和当干态粉末时所述金刚石颗粒的比表面积,在17°(2θ±2°),26.5°没有峰 不小于1.50×10 5 / kg,并且所述颗粒的基本上所有的表面碳原子与杂原子键合,并且所述粉末的总吸收空间 干燥时为0.5m 3 / kg以上。 金刚石颗粒在水性液体中是非常活泼和可分散的,并且具有与通常的钻石基本上相同的机械性能。
    • 7. 发明授权
    • Stable aqueous suspension liquid of finely divided diamond particles, metallic film containing diamond particles and method of producing the same
    • 细碎金刚石颗粒的稳定含水悬浮液,含金刚石颗粒的金属膜及其制造方法
    • US07927390B2
    • 2011-04-19
    • US12461135
    • 2009-08-03
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • B24D3/02C09C1/68C09K3/14B01J3/06C25D15/00
    • C25D15/02Y10S428/935Y10T428/12493Y10T428/12625Y10T428/25
    • An aqueous suspension liquid of finely divided diamond particles comprising 0.05 to 160 parts by weight of a finely divided diamond particles in 1000 parts of water, wherein; (i) the finely divided diamond particles have an element composition consisting mainly of 72 to 89.5% by weight of carbon, 0.8 to 1.5% of hydrogen, 1.5 to 2.5% of nitrogen, and 10.5 to 25.0% of oxygen; (ii) and, almost all of said diamond particles are in the range of 2 nm to 50 nm in diameters thereof (80% or more by number average, 70% or more by weight average), (iii) and, said finely divided diamond particles exhibit a strongest peak of the intensity of the Bragg angle at 43.9° (2θ±2°), strong and characteristic peaks at 73.5° (2θ±2°) and 95° (2θ±2°), a warped halo at 17° (2θ±2°), and no peak at 26.5°, by X-ray diffraction (XRD) spectrum analysis using Cu—Kα radiation when dried, (iv) and, specific surface area of said diamond particles when dry state powder is not smaller than 1.50×105 m2/kg, and substantially all the surface carbon atoms of said particles are bonded with hetero atoms, and the total absorption space of said powder is 0.5 m3/kg or more, when dried. The diamond particles are very active and dispersible in aqueous liquid in stable, and have essentially same mechanical properties as that of usual diamonds.
    • 一种细碎金刚石颗粒的水性悬浮液,其包含0.05至160重量份在1000份水中的细碎金刚石颗粒,其中: (i)细碎金刚石颗粒具有主要由碳原子数为72〜89.5重量%,氢为0.8〜1.5%,氮为1.5〜2.5%,氧为10.5〜25.0%的元素组成。 (ii),并且几乎所有的所述金刚石颗粒的直径在2nm至50nm的范围内(数均为80%或更多,平均为70%或更多),(iii),所述细分 金刚石颗粒在43.9°(2θ;±2°)处呈现出最强的布拉格角强度峰值,在73.5°(2θ±2°)和95°(2°;±2°)的强和特征峰,a 通过在干燥时使用Cu-Kα辐射的X射线衍射(XRD)光谱分析,(iv)和所述金刚石颗粒的比表面积,在17°(2°和±2°)弯曲的光环,并且在26.5°处没有峰 当干态粉末不小于1.50×10 5 m 2 / kg,并且所述颗粒的基本上所有的表面碳原子与杂原子键合时,干燥时所述粉末的总吸收空间为0.5m 3 / kg以上。 金刚石颗粒在水性液体中是非常活泼和可分散的,并且具有与通常的钻石基本上相同的机械性能。
    • 8. 发明授权
    • Stable aqueous suspension liquid of finely divided diamond particles, metallic film containing diamond particles and method of producing the same
    • 细碎金刚石颗粒的稳定含水悬浮液,含金刚石颗粒的金属膜及其制造方法
    • US07585360B2
    • 2009-09-08
    • US11335734
    • 2006-01-20
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • Tadamasa FujimuraMasato SoneValeri Yu DolmatovShigeru Shiozaki
    • C09D5/00C01B31/06
    • C25D15/02Y10S428/935Y10T428/12493Y10T428/12625Y10T428/25
    • An aqueous suspension liquid of finely divided diamond particles comprising 0.05 to 160 parts by weight of a finely divided diamond particles in 1000 parts of water, wherein; (i) the finely divided diamond particles have an element composition consisting mainly of 72 to 89.5% by weight of carbon, 0.8 to 1.5% of hydrogen, 1.5 to 2.5% of nitrogen, and 10.5 to 25.0% of oxygen; (ii) and, almost all of said diamond particles are in the range of 2 nm to 50 nm in diameters thereof (80% or more by number average, 70% or more by weight average), (iii) and, said finely divided diamond particles exhibit a strongest peak of the intensity of the Bragg angle at 43.9° (2θ±2°), strong and characteristic peaks at 73.5° (2θ±2°)and 95° (2θ±2°), a warped halo at 17° (2θ±2°), and no peak at 26.5°, by X-ray diffraction (XRD) spectrum analysis using Cu—Kα radiation when dried, (iv) and, specific surface area of said diamond particles when dry state powder is not smaller than 1.50×105 m2/kg, and substantially all the surface carbon atoms of said particles are bonded with hetero atoms, and the total absorption space of said powder is 0.5 m3/kg or more, when dried. The diamond particles are very active and dispersible in aqueous liquid in stable, and have essentially same mechanical properties as that of usual diamonds.
    • 一种细碎金刚石颗粒的水性悬浮液,其包含0.05至160重量份在1000份水中的细碎金刚石颗粒,其中: (i)细碎金刚石颗粒具有主要由碳原子数为72〜89.5重量%,氢为0.8〜1.5%,氮为1.5〜2.5%,氧为10.5〜25.0%的元素组成。 (ii),并且几乎所有的所述金刚石颗粒的直径在2nm至50nm的范围内(数均为80%或更多,平均为70%或更多),(iii),所述细分 金刚石颗粒在43.9°(2θ±2°)处呈现出最强的布拉格角强度峰值,73.5°(2θ±2°)和95°(2θ±2°)处的强和特征峰, 通过使用Cu-Kalpha辐射干燥时的X射线衍射(XRD)光谱分析,(iv)和当干态粉末时所述金刚石颗粒的比表面积,在17°(2θ±2°),26.5°没有峰 不小于1.50×10 5 m 2 / kg,并且所述颗粒的基本上所有表面碳原子与杂原子键合,并且当干燥时,所述粉末的总吸收空间为0.5m 3 / kg以上。 金刚石颗粒在水性液体中是非常活泼和可分散的,并且具有与通常的钻石基本上相同的机械性能。
    • 9. 发明授权
    • Method for activating surface of base material and apparatus thereof
    • 激活基材表面的方法及其装置
    • US07300527B2
    • 2007-11-27
    • US10297878
    • 2002-11-06
    • Hideo YoshidaNobuyoshi SatoTakeshi SakoMasato SoneKentaro AbeKiyohito Sakon
    • Hideo YoshidaNobuyoshi SatoTakeshi SakoMasato SoneKentaro AbeKiyohito Sakon
    • B08B3/02
    • B08B3/04B08B3/02B08B7/02C25D5/34Y10S134/902
    • A method for activating the surface of a base material and an apparatus thereof, which is suited to be utilized for pretreatment in electrochemical treatment such as, for example, electroplating or the like, in which the surface of a base material such as metal can be subjected to degreasing treatment and oxide film removing treatment simultaneously, efficiently and rationally, in which productivity can be enhanced and the equipment cost can be reduced, and in which a waste solution can be rationalized so that the solution can be reutilized and the environmental pollution can be prevented. A method for activating the surface of a base material in which the surface of a member to be treated is subjected to degreasing treatment or oxide film removing treatment. Pressurized carbon dioxide is dissolved in a predetermined quantity of water, thereby preparing an oxide film removing solution having a predetermined acidic concentration.
    • 用于激活基材表面的方法及其装置,其适用于电化学处理例如电镀等中的预处理,其中诸如金属的基材的表面可以是 同时进行脱脂处理和氧化膜除去处理,能够高效合理地提高生产性,并且可以降低设备成本,并且其中废溶液可以合理化以使溶液可再利用并且环境污染可以 被阻止 一种激活基材的表面的方法,其中待处理部件的表面进行脱脂处理或氧化膜去除处理。 将加压的二氧化碳溶解在预定量的水中,从而制备具有预定酸性浓度的氧化膜去除溶液。