    • 1. 发明授权
    • White polymide film and manufacture thereof
    • 白色聚酰亚胺薄膜及其制造
    • US08461257B2
    • 2013-06-11
    • US13599550
    • 2012-08-30
    • Sheng-Yu HuangChung-Yi Chen
    • Sheng-Yu HuangChung-Yi Chen
    • C08L79/08
    • C08G73/1039C08J5/18C08J2379/08C08L79/08
    • A process of manufacturing a white polyimide film comprising performing condensation polymerization of monomers comprising diamine and dianhydride components to obtain a solution; adding a dehydrant, a catalyst and a coloration filler into the solution to obtain a precursor solution; coating a layer of the precursor solution on a support; and baking the coated layer of the precursor solution to form a white polyimide film. The diamine component can include 2,2′-bis(trifluoromethyl)benzidine, and the dianhydride component can include 3,3′,4,4′-biphenyltetracarboxylic dianhydride and 2,2-bis[4-(3,4-dicarboxyphenoxy)phenyl]propane dianhydride. The coloration filler can include TiO2, Al2O3, CaCO3, CaSO4, SiO2, BN, AlN and clay.
    • 一种制造白色聚酰亚胺膜的方法,包括进行包含二胺和二酐组分的单体的缩聚以获得溶液; 向溶液中加入脱水剂,催化剂和着色填料,得到前体溶液; 将一层前体溶液涂覆在载体上; 并烘烤前体溶液的涂层以形成白色聚酰亚胺膜。 二胺组分可包括2,2'-双(三氟甲基)联苯胺,二酐组分可包括3,3',4,4'-联苯四羧酸二酐和2,2-双[4-(3,4-二羧基苯氧基) 苯基]丙烷二酐。 着色填料可以包括TiO2,Al2O3,CaCO3,CaSO4,SiO2,BN,AlN和粘土。
    • 4. 发明申请
    • WHITE POLYMIDE FILM AND MANUFACTURE THEREOF
    • 白色聚氯乙烯薄膜及其制造方法
    • US20130032970A1
    • 2013-02-07
    • US13599550
    • 2012-08-30
    • Sheng-Yu HuangChung-Yi Chen
    • Sheng-Yu HuangChung-Yi Chen
    • B29D7/01
    • C08G73/1039C08J5/18C08J2379/08C08L79/08
    • A process of manufacturing a white polyimide film comprising performing condensation polymerization of monomers comprising diamine and dianhydride components to obtain a solution; adding a dehydrant, a catalyst and a coloration filler into the solution to obtain a precursor solution; coating a layer of the precursor solution on a support; and baking the coated layer of the precursor solution to form a white polyimide film. The diamine component can include 2,2′-bis(trifluoromethyl)benzidine, and the dianhydride component can include 3,3′,4,4′-biphenyltetracarboxylic dianhydride and 2,2-bis[4-(3,4-dicarboxyphenoxy) phenyl]propane dianhydride. The coloration filler can include TiO2, Al2O3, CaCO3, CaSO4, SiO2, BN, AlN and clay.
    • 一种制造白色聚酰亚胺膜的方法,包括进行包含二胺和二酐组分的单体的缩聚以获得溶液; 向溶液中加入脱水剂,催化剂和着色填料,得到前体溶液; 将一层前体溶液涂覆在载体上; 并烘烤前体溶液的涂层以形成白色聚酰亚胺膜。 二胺组分可包括2,2'-双(三氟甲基)联苯胺,二酐组分可包括3,3',4,4'-联苯四羧酸二酐和2,2-双[4-(3,4-二羧基苯氧基) 苯基]丙烷二酐。 着色填料可以包括TiO2,Al2O3,CaCO3,CaSO4,SiO2,BN,AlN和粘土。
    • 5. 发明授权
    • White polyimide film and manufacture thereof
    • 白色聚酰亚胺薄膜及其制造
    • US08288471B2
    • 2012-10-16
    • US12906951
    • 2010-10-18
    • Sheng-Yu HuangChung-Yi Chen
    • Sheng-Yu HuangChung-Yi Chen
    • C08L79/08
    • C08G73/1039C08J5/18C08J2379/08C08L79/08
    • A white polyimide film comprises a polyimide base polymer and a coloration filler homogeneously distributed in the white polyimide film by reacting a diamine component with a dianhydride component and a coloration filter. The diamine component can include 2,2′-bis(trifluoromethyl)benzidine, and the dianhydride component can include 3,3′,4,4′-biphenyltetracarboxylic dianhydride and 2,2-bis[4-(3,4-dicarboxyphenoxy)phenyl]propane dianhydride. The coloration filler can include TiO2, Al2O3, CaCO3, CaSO4, SiO2, BN, AlN and clay. The white polyimide film has a coefficient of thermal expansion (CTE) less than about 60 ppm/° C. in a temperature range between about 100° C. and about 200° C. , an elongation rate between about 5% and about 60%, and a b*-value between about 0 and about 15. In some embodiments, a method of manufacturing the white polyimide film is also described.
    • 白色聚酰亚胺膜包括通过使二胺组分与二酸酐组分和着色过滤器反应而均匀分布在白色聚酰亚胺膜中的聚酰亚胺基聚合物和着色填料。 二胺组分可包括2,2'-双(三氟甲基)联苯胺,二酐组分可包括3,3',4,4'-联苯四羧酸二酐和2,2-双[4-(3,4-二羧基苯氧基) 苯基]丙烷二酐。 着色填料可以包括TiO2,Al2O3,CaCO3,CaSO4,SiO2,BN,AlN和粘土。 白色聚酰亚胺膜在约100℃至约200℃的温度范围内具有小于约60ppm /℃的热膨胀系数(CTE),约5%至约60%的伸长率 ,并且ab *值在约0和约15之间。在一些实施例中,还描述了制造白色聚酰亚胺膜的方法。
    • 6. 发明申请
    • WHITE POLYIMIDE FILM AND MANUFACTURE THEREOF
    • 白色聚酰亚胺薄膜及其制造方法
    • US20120095147A1
    • 2012-04-19
    • US12906951
    • 2010-10-18
    • Sheng-Yu HuangChung-Yi Chen
    • Sheng-Yu HuangChung-Yi Chen
    • C08K3/38C08K3/28B05D3/02C08K3/22C08K3/26C08K3/30C08L79/08C08K3/34
    • C08G73/1039C08J5/18C08J2379/08C08L79/08
    • A white polyimide film comprises a polyimide base polymer and a coloration filler homogeneously distributed in the white polyimide film by reacting a diamine component with a dianhydride component and a coloration filter. The diamine component can include 2,2′-bis(trifluoromethyl)benzidine, and the dianhydride component can include 3,3′,4,4′-biphenyltetracarboxylic dianhydride and 2,2-bis[4-(3,4-dicarboxyphenoxy)phenyl]propane dianhydride. The coloration filler can include TiO2, Al2O3, CaCO3, CaSO4, SiO2, BN, AlN and clay. The white polyimide film has a coefficient of thermal expansion (CTE) less than about 60 ppm/° C. in a temperature range between about 100° C. and about 200° C. , an elongation rate between about 5% and about 60%, and a b*-value between about 0 and about 15. In some embodiments, a method of manufacturing the white polyimide film is also described.
    • 白色聚酰亚胺膜包括通过使二胺组分与二酸酐组分和着色过滤器反应而均匀分布在白色聚酰亚胺膜中的聚酰亚胺基聚合物和着色填料。 二胺组分可包括2,2'-双(三氟甲基)联苯胺,二酐组分可包括3,3',4,4'-联苯四羧酸二酐和2,2-双[4-(3,4-二羧基苯氧基) 苯基]丙烷二酐。 着色填料可以包括TiO2,Al2O3,CaCO3,CaSO4,SiO2,BN,AlN和粘土。 白色聚酰亚胺膜在约100℃至约200℃的温度范围内具有小于约60ppm /℃的热膨胀系数(CTE),约5%至约60%的伸长率 ,并且ab *值在约0和约15之间。在一些实施例中,还描述了制造白色聚酰亚胺膜的方法。
    • 8. 发明授权
    • Image processing circuit and associated method
    • 图像处理电路及相关方法
    • US08582665B2
    • 2013-11-12
    • US12480126
    • 2009-06-08
    • Chung-Yi ChenSu-Chun Wang
    • Chung-Yi ChenSu-Chun Wang
    • H04N11/02
    • H04N19/436H04N19/43
    • An image processing circuit includes a compression circuit, a plurality of first line buffers, a decompression circuit, and a motion estimation/compensation circuit. The compression circuit receives source image data and compresses the received source image data to generate a compressed image data. The first line buffers, coupled to the compression circuit, sequentially receive the compressed image data and buffer the compressed image data. The decompression circuit, coupled to the first line buffers, decompresses the compressed image data to generate a decompressed image data. The motion estimation/compression circuit, coupled to the decompression circuit, performs motion estimation/compensation according to the decompressed image data.
    • 图像处理电路包括压缩电路,多个第一行缓冲器,解压缩电路和运动估计/补偿电路。 压缩电路接收源图像数据并压缩接收到的源图像数据以产生压缩图像数据。 耦合到压缩电路的第一行缓冲器顺序地接收压缩的图像数据并缓冲压缩的图像数据。 耦合到第一行缓冲器的解压缩电路解压缩压缩的图像数据以产生解压缩的图像数据。 耦合到解压缩电路的运动估计/压缩电路根据解压缩的图像数据执行运动估计/补偿。