    • COLD-ROLLED STEEL SHEET AND PROCESS FOR PRODUCING THE SAME
    • 冷轧钢板及其制造方法
    • US20090300902A1
    • 2009-12-10
    • US12519539
    • 2006-12-20
    • Nobuko MinejiReiko SugiharaTadashi Inoue
    • Nobuko MinejiReiko SugiharaTadashi Inoue
    • H01M6/00C21D8/04C22C38/04
    • C21D9/46C22C38/004C22C38/04Y10T29/49108
    • A cold-rolled steel sheet that is suitable for battery cases and has low anisotropy is composed of, by mass %, C: ≦0.0030%, Si: ≦0.02%, Mn: 0.15 to 0.19%, P: ≦0.020%, S: ≦0.015%, N: ≦0.0040%, Al: 0.020 to 0.070%, Nb: 1.00≦Nb/C (atomic equivalent ratio)≦5.0, B: 1 ppm≦B-(11/14)N≦15 ppm (in the expression, B and N denote the contents of the respective elements), and the balance: being Fe and inevitable impurities, and has a planar anisotropy Δr of the r-value in the range of −0.10≦Δr≦0.10. In a process for producing the steel sheet, the cold rolling is performed at a rolling ratio of 70 to 87%, and then annealing is performed on a continuous annealing line at an annealing temperature of from the recrystallization temperature to 830° C.
    • 适用于电池壳体并且各向异性低的冷轧钢板以质量%计含有C:<= 0.0030%,Si:<= 0.02%,Mn:0.15〜0.19%,P:<0.020 %,S:<= 0.015%,N:<= 0.0040%,Al:0.020〜0.070%,Nb:1.00 <= Nb / C(原子当量比)<= 5.0,B:1ppm <= B- / 14)N <= 15ppm(在表达式中,B和N表示各元素的含量),余量为Fe和不可避免的杂质,并且在r值范围内具有平面各向异性Deltar -0.10 <= Deltar <= 0.10。 在钢板的制造方法中,以轧制率为70〜87%进行冷轧,然后在从再结晶温度至830℃的退火温度下在连续退火生产线上进行退火。