    • Polyolefin compositions particularly suitable for cast film, exhibiting heat sealability, retortability, low haze and stiffness, comprising: 1) 75-85% of a propylene homopolymer or copolymer of propylene with ethylene and/or one or more C4-C10 α-olefin(s), the homopolymer or copolymer having melting temperature equal to or higher than 150° C., 2) 15-25% of a copolymer of ethylene with one or more C4-C10 α-olefin(s) containing from 20 to 30% of said C4-C10 α-olefin(s); said composition having MFR (at 230° C., 2.16 kg) of from 5-10 g/10 min, the total content of ethylene of from 10 to 20%, the total content of C4-C10 α-olefin(s) of from 2 to 8%, the ratio XStot/XSm of the total fraction soluble in Xylene at room temperature to the fraction soluble in Xylene at room temperature of the matrix component (1) of from 5 to 15, and the value of the intrinsic viscosity of the total fraction soluble in Xylene at room temperature (XSIVtot) of 1.5 dl/g or less.
    • 特别适用于流延膜的聚烯烃组合物,具有热封性,蒸煮性,低雾度和刚度,包括:1)75-85%的丙烯均聚物或丙烯与乙烯和/或一种或多种C 4 -C 10α-烯烃的共聚物 s),熔融温度等于或高于150℃的均聚物或共聚物,2)乙烯与一种或多种含有20-30%(重量)的C 4 -C 10α-烯烃的共聚物的15-25% 的所述C 4 -C 10α-烯烃; 所述组合物的MFR(在230℃,2.16kg)为5-10g / 10min,乙烯的总含量为10至20%,C 4 -C 10α-烯烃的总含量为 2〜8%,室温下可溶于二甲苯的总馏分的比例XStot / XSm与基体成分(1)的室温下可溶于二甲苯的馏分的比例为5〜15,特性粘度 在室温下可溶于二甲苯的总馏分(XSIVtot)为1.5dl / g以下。
    • 2. 发明申请
    • Polyolefin Compositions
    • 聚烯烃组合物
    • US20120136121A1
    • 2012-05-31
    • US13378952
    • 2010-06-23
    • Monica GalvanMarco CiarafoniRoberto PantaleoniAngelo Ferraro
    • Monica GalvanMarco CiarafoniRoberto PantaleoniAngelo Ferraro
    • C08L23/04
    • C08J5/18C08J2323/10C08L23/0807C08L23/0815C08L23/10C08L2666/06
    • Polyolefin compositions particularly suitable for cast film, exhibiting heat sealability, retortability, low haze and stiffness, comprising: 1) 75-85% of a propylene homopolymer or copolymer of propylene with ethylene and/or one or more C4-C10 α-olefin(s), the homopolymer or copolymer having melting temperature equal to or higher than 150° C., 2) 15-25% of a copolymer of ethylene with one or more C4-C10 α-olefin(s) containing from 20 to 30% of said C4-C10 α-olefin(s); said composition having MFR (at 230° C., 2.16 kg) of from 5-10 g/10 min, the total content of ethylene of from 10 to 20%, the total content of C4-C10 α-olefin(s) of from 2 to 8%, the ratio XStot/XSm of the total fraction soluble in Xylene at room temperature to the fraction soluble in Xylene at room temperature of the matrix component (1) of from 5 to 15, and the value of the intrinsic viscosity of the total fraction soluble in Xylene at room temperature (XSIVtot) of 1.5 dl/g or less.
    • 特别适用于流延膜的聚烯烃组合物,具有热封性,蒸煮性,低雾度和刚度,包括:1)75-85%的丙烯均聚物或丙烯与乙烯和/或一种或多种C 4 -C 10α-烯烃的共聚物 s),熔融温度等于或高于150℃的均聚物或共聚物,2)乙烯与一种或多种含有20至30重量%的C 4 -C 10α-烯烃的共聚物的15-25% 的所述C 4 -C 10α-烯烃; 所述组合物的MFR(在230℃,2.16kg)为5-10g / 10min,乙烯的总含量为10至20%,C 4 -C 10α-烯烃的总含量为 2〜8%,室温下可溶于二甲苯的总馏分的比例XStot / XSm与基体成分(1)的室温下可溶于二甲苯的馏分的比例为5〜15,特性粘度 在室温下可溶于二甲苯的总馏分(XSIVtot)为1.5dl / g以下。
    • 4. 发明申请
    • Polyolefin compositions
    • 聚烯烃组合物
    • US20080182941A1
    • 2008-07-31
    • US11982705
    • 2007-11-01
    • Angelo FerraroTiziano Dall'OccoGiuliano Cecchin
    • Angelo FerraroTiziano Dall'OccoGiuliano Cecchin
    • C08F210/00C08L23/00
    • C08L23/0815C08F10/00C08F210/00C08F210/16C08F255/00C08F255/02C08L23/10C08L23/16C08L51/06C08L2314/02C08F4/6555C08F4/6494C08F4/651C08L2666/06C08L2666/02C08F210/08C08F2500/12C08F2500/08C08F2500/20C08F2500/11C08F210/06C08F2500/17C08F2500/04
    • A polyolefin composition, comprising: (A) from 5 to 95 parts by weight of a crystalline propylene polymer having an isotactic index greater than 80, selected from polypropylene homopolymer and propylene copolymers containing 0.5 to 15 mol % of ethylene and/or an α-olefin having 4 to 10 carbon atoms, and (B) from 5 to 95 parts by weight of an ethylene/α-olefin copolymer containing from 35 to 70% by weight of ethylene, from 30 to 65% by weight of an olefin CH2═CHR, in which R a hydrocarbyl radical with 1-12 carbon atoms, and from 0 to 10% of a polyene characterized by (i) a Molecular Weight Distribution expressed by Mw/Mn of higher than 3, (ii) a content of 2-1 regioinvertions of the α-olefin units of lower than 5% and (iii) a value of Shore A and content by weight of ethylenic units, calculated on the basis of the whole polymer, such that the point defined by such values falls below the curve defined by the following equation: Y=0.0438X2-4.1332X+A where Y is the value of the Shore A, X is the weight percentage of ethylene units in the polymer calculated by NMR and A is 145.
    • 一种聚烯烃组合物,其包含:(A)5至95重量份的全同立构指数大于80的结晶丙烯聚合物,其选自聚丙烯均聚物和含有0.5至15摩尔%乙烯和/或α-烯烃的丙烯共聚物, 具有4至10个碳原子的烯烃,和(B)5至95重量份的含有35至70重量%乙烯的乙烯/α-烯烃共聚物,30至65重量%的烯烃CH 2, 其中R 1具有1-12个碳原子的烃基和0至10%的多烯,其特征在于(i)由Mw / Mn表示的分子量分布高于3 ,(ii)α-烯烃单元的2-1区域转换的含量低于5%,(iii)肖氏A值和基于整个聚合物计算的烯属单元的重量含量,使得 由这些值定义的点低于由以下等式定义的曲线:<?in-line-formula description =“In-li “公式”end =“lead”?> Y = 0.0438X <2> -4.1332X + A <?in-line-formula description =“In-line Formulas”end =“tail”?> where Y是肖氏A的值,X是通过NMR计算的聚合物中乙烯单元的重量百分比,A是145。
    • 6. 发明授权
    • Process for the preparation of porous polymers and polymers obtainable thereof
    • 制备可获得的多孔聚合物和聚合物的方法
    • US07183332B2
    • 2007-02-27
    • US10450603
    • 2001-12-21
    • Angelo FerraroGiovanni BaruzziConstantine A. StewartOfelia Fusco
    • Angelo FerraroGiovanni BaruzziConstantine A. StewartOfelia Fusco
    • C08F10/06C08F4/02C08L23/10
    • C08F10/00C08F10/06C08F110/06Y10S526/943C08F4/027C08F2/001C08F2500/17C08F2500/18C08F2500/24
    • A process for preparing porous olefin polymers comprising bringing into contact in a polymerization reactor, at a temperature T1, one or more olefins of the formula (I) CH2═CHR1, R1 being hydrogen, a C1–C20-alkyl or a C6–C12-aryl group, with a catalyst obtained by reacting a solid catalyst component in the form of spheroidal particles comprising a compound of Ti or V not containing metal-π bonds and a Mg halide, optionally containing one or more electron donor compounds, with an aluminum-alkyl (Al-alkyl) compound, then raising the temperature up to the polymerization temperature, said process being characterized in that: a) if the temperature T1 is lower than 40° C., the temperature is raised up to the polymerization temperature is such a way that, for a time of at least one minute after the introduction temperature in such a way that, for a time of at least one minute after the introduction of the catalyst system into the reactor, the temperature of the reaction T2 fulfills the following condition of formula (II) wherein m is the time expressed in minutes employed for reaching the temperature T2; or b) if temperature T1 is 40° C. or higher, the reactor is maintained for a time of at least one minute at a temperature of at least 40° C.
    • 一种制备多孔烯烃聚合物的方法,包括在聚合反应器中,在温度T 1下接触一种或多种式(I)CH 2 -CHR的烯烃 R 1是氢,C 1 -C 20 - 烷基或C 6 - 与通过使包含不含金属-Ip键的Ti或V的化合物的球形颗粒形式的固体催化剂组分与Mg的反应获得的催化剂与Mg 卤化物,任选地含有一个或多个电子给体化合物与烷基铝(Al-烷基)化合物,然后将温度升高到聚合温度,所述方法的特征在于:a)如果温度T 1 低于40℃,温度升高到聚合温度是这样一种方式,使得在引入温度之后至少1分钟的时间,使得在 在介绍后至少一分钟 催化剂体系进入反应器中,反应温度T 2满足以下条件(II),其中m是达到温度T 2的分钟所用的时间 ; 或b)如果温度T≥0.4℃或更高,则反应器在至少40℃的温度下保持至少1分钟的时间。