    • 6. 发明申请
    • Method for producing ultra thin wall metallic tube with cold working process
    • 冷加工工艺制造超薄壁金属管的方法
    • US20090038360A1
    • 2009-02-12
    • US12285253
    • 2008-10-01
    • Chihiro Hayashi
    • Chihiro Hayashi
    • B21B17/10
    • B21C1/24B21B21/005B21B25/00B21C1/26B21C3/04B21C3/08
    • An exemplary embodiment of the invention provides a method for producing an ultra thin wall metallic tube by cold working method with significant wall thickness reduction. In a method for producing the metallic tube with a cold pilger mill according to the invention, cold rolling is performed while tube diameters are being expanded using rolls having tapered groove dies whose calibers increase from an engaging entry side toward a finishing exit side. In a method for producing the metallic tube with a drawing machine according to the invention, cold drawing is performed while the tube diameters are being expanded using a solid die whose calibers increase from an engaging entry side toward a finishing exit side and a plug of a tapered mandrel bar whose diameters increase from an entry side of the die toward an exit side. In the metallic tube producing method, a maximum diameter of the plug or tapered mandrel bar may be larger than an outside diameter of the mother tube.
    • 本发明的一个示例性实施例提供了一种通过冷加工方法制造超薄壁金属管的方法,其具有显着的壁厚减小。 在根据本发明的用于制造具有冷冲切机的金属管的方法中,使用具有锥形槽模的辊,使其卷边从接合入口侧朝向精加工出口侧增大,进行冷却。 在根据本发明的具有拉丝机的金属管的制造方法中,在使用从接合入口侧朝向精加工出口侧增加口径的固体模具扩大管直径的同时进行冷拉拔, 锥形芯棒的直径从模具的入口侧朝向出口侧增加。 在金属管制造方法中,塞子或锥形芯棒的最大直径可以大于母管的外径。
    • 9. 发明授权
    • Piercing-rolling method and piercing/rolling apparatus for seamless
steel tube
    • 无缝钢管穿孔轧制方法及穿孔/轧制设备
    • US5636542A
    • 1997-06-10
    • US435871
    • 1995-05-05
    • Tomio YamakawaChihiro HayashiKazuhiro Shimoda
    • Tomio YamakawaChihiro HayashiKazuhiro Shimoda
    • B21B19/04B21B37/00B21B37/78
    • B21B19/04
    • A method for manufacturing seamless steel tubes by the Mannnesmann tube making process wherein a billet is passed through a piercer and the center of the billet is pierced through to obtain a hollow shell. A pair of disk rolls are disposed to incline by a skew angle .delta. with respect to a pass line toward cone-type main roll located at the entry side, where a material to be rolled enters into the disk roll sliding face, thereby to become unparallel with the outlet face angle of the main roll, while the skew angle .delta. is set to satisfy the following conditions related to the skew angle .delta., the inlet face angle .theta.1 and the outlet face angle .theta.2 of the main roll, thereby to obtain expansion ratio of outer diameter of 1.15 or higher value..theta.2+2.degree.
    • 通过Mannnesmann管制造方法制造无缝钢管的方法,其中坯料穿过穿孔机,并且将坯料的中心穿透以获得中空壳体。 一对盘卷被设置成相对于位于入口侧的锥形主辊相对于通过线的斜角δ倾斜,其中待轧制的材料进入盘辊滑动面,从而变得不平行 与主辊的出口面角度相同,而偏斜角度设定为满足与主辊的倾斜角度δ,入口面角度θ1和出口面角θ2有关的以下条件,由此获得 外径膨胀比为1.15以上。 θ2 + 2°<δ<9°,δ+θ1 <12°外径膨胀比高的穿孔/滚压操作稳定地进行,不会发生从主辊未完全释放的故障, 外表和未完成的参与。