    • Crosslinkable polyolefin composition comprising silane groups forming an acid or a base upon hydrolysation
    • 包含在水解时形成酸或碱的硅烷基团的可交联聚烯烃组合物
    • US08846844B2
    • 2014-09-30
    • US13265555
    • 2010-05-14
    • Kristian DahlenRoger Carlsson
    • Kristian DahlenRoger Carlsson
    • C08G77/08C08F255/02C08L51/06C08F255/00
    • C08F255/00C08F255/02C08L51/06C08L2666/04C08L2666/02
    • The present invention relates to a polyolefin composition comprising (A) a crosslinkable polyolefin with hydrolysable silane groups which upon hydrolysation form an acid or a base, characterised in that the acid or base generates a gel content of at least 40% after 40 hours in the 90° C. cross-linking test, wherein the acid or base is added in an amount of 4.5 mmol/kg to an ethylene/vinyltrimethoxysilane copolymer with a MFR2=2 g/10 min, a density of 923 g/cm3, and 2 wt. % of vinyltrimethoxysilane and then is cross-linked in a waterbath at 90° C., and to a polyolefin composition comprising (i) a crosslinkable polyolefin with hydrolysable silane groups, and (ii) a non-polymeric compound with hydrolysable silane groups which upon hydrolysation form an acid or a base, characterised in that the acid or base generates a gel content of at least 40% after 40 hours in the 90° C. cross-linking test, wherein the acid or base is added in an amount of 4.5 mmol/kg to an ethylene/vinyltrimethoxysilane copolymer with a MFR2=2 g/10 min, a density of 923 g/cm3, and 2 wt. % of vinyltrimethoxysilane and then is cross-linked in a waterbath at 90° C.
    • 本发明涉及一种聚烯烃组合物,其包含(A)具有可水解硅烷基团的可交联聚烯烃,其在水解形成酸或碱时,​​其特征在于所述酸或碱在40小时后产生至少40%的凝胶含量 90℃的交联试验,其中将酸或碱以4.5mmol / kg的量加入到MFR 2 = 2g / 10min,密度为923g / cm 3的乙烯/乙烯基三甲氧基硅烷共聚物中,和2 重量 %的乙烯基三甲氧基硅烷,然后在90℃的水浴中交联,以及包含(i)具有可水解硅烷基团的可交联聚烯烃的聚烯烃组合物,和(ii)具有可水解硅烷基团的非聚合化合物, 水解形成酸或碱,其特征在于酸或碱在90℃交联试验中40小时后产生至少40%的凝胶含量,其中酸或碱的加入量为4.5 mmol / kg,MFR 2 = 2g / 10min,密度为923g / cm 3,2重量%的乙烯/乙烯基三甲氧基硅烷共聚物。 %的乙烯基三甲氧基硅烷,然后在90℃的水浴中交联。
    • 2. 发明申请
    • CROSSLINKABLE POLYOLEFIN COMPOSITION COMPRISING SILANE GROUPS FORMING AN ACID OR A BASE UPON HYDROLYSATION
    • 可交联的聚烯烃组合物,包含形成酸或基于水解的硅烷基团
    • US20120071607A1
    • 2012-03-22
    • US13265555
    • 2010-05-14
    • Kristian DahlenRoger Carlsson
    • Kristian DahlenRoger Carlsson
    • C08L43/04C07F7/18C08F8/00C08F230/08C08L23/02
    • C08F255/00C08F255/02C08L51/06C08L2666/04C08L2666/02
    • The present invention relates to a polyolefin composition comprising (A) a crosslinkable polyolefin with hydrolysable silane groups which upon hydrolysation form an acid or a base, characterised in that the acid or base generates a gel content of at least 40% after 40 hours in the 90° C. cross-linking test, wherein the acid or base is added in an amount of 4.5 mmol/kg to an ethylene/vinyltrimethoxysilane copolymer with a MFR2=2 g/10 min, a density of 923 g/cm3, and 2 wt. % of vinyltrimethoxysilane and then is cross-linked in a waterbath at 90° C., and to a polyolefin composition comprising (i) a crosslinkable polyolefin with hydrolysable silane groups, and (ii) a non-polymeric compound with hydrolysable silane groups which upon hydrolysation form an acid or a base, characterised in that the acid or base generates a gel content of at least 40% after 40 hours in the 90° C. cross-linking test, wherein the acid or base is added in an amount of 4.5 mmol/kg to an ethylene/vinyltrimethoxysilane copolymer with a MFR2=2 g/10 min, a density of 923 g/cm3, and 2 wt. % of vinyltrimethoxysilane and then is cross-linked in a waterbath at 90° C.
    • 本发明涉及一种聚烯烃组合物,其包含(A)具有可水解硅烷基团的可交联聚烯烃,其在水解形成酸或碱时,​​其特征在于所述酸或碱在40小时后产生至少40%的凝胶含量 90℃的交联试验,其中将酸或碱以4.5mmol / kg的量加入到MFR 2 = 2g / 10min,密度为923g / cm 3的乙烯/乙烯基三甲氧基硅烷共聚物中,和2 重量 %的乙烯基三甲氧基硅烷,然后在90℃的水浴中交联,以及包含(i)具有可水解硅烷基团的可交联聚烯烃的聚烯烃组合物,和(ii)具有可水解硅烷基团的非聚合化合物, 水解形成酸或碱,其特征在于酸或碱在90℃交联试验中40小时后产生至少40%的凝胶含量,其中酸或碱的加入量为4.5 mmol / kg,MFR 2 = 2g / 10min,密度为923g / cm 3,2重量%的乙烯/乙烯基三甲氧基硅烷共聚物。 %的乙烯基三甲氧基硅烷,然后在90℃的水浴中交联。
    • 7. 发明申请
    • ADDITIVE MASTERBATCH WITH A C3-C5 ALPHA-OLEFIN HOMO- OR COPOLYMER IN THE CARRIER
    • 带载体的C3-C5阿尔法 - 烯烃共聚物的添加剂主板
    • US20150057407A1
    • 2015-02-26
    • US14387348
    • 2013-04-24
    • Kristian DahlenPerry NylanderOla Fagrell
    • Kristian DahlenPerry NylanderOla Fagrell
    • C08L23/08
    • C08L23/08C08J3/226C08J2343/04C08J2423/10C08J2423/20C08K5/0025C08K5/42C08K2003/2241C08L23/0892C08L23/12C08L2205/02C08L2310/00C08L2312/08C08L43/04
    • The present invention relates to a polyethylene composition comprising: a) a polyethylene having cross-linkable silicon-containing groups (A); and b) a masterbatch comprising—one or more additives; and—a carrier comprising a C3-C5 alpha-olefin homo or copolymer (B). The present invention further relates to a cross-linked polyethylene composition obtainable by treating the composition according to any one of the preceding claims under cross-linking conditions. The present invention also relates to the following uses: Use of a masterbatch comprising—an additive; and—a carrier comprising a C3-C5 alpha-olefin homo- or copolymer (B) for adding an additive to a polyethylene with cross-linkable silicon-containing groups. Use of C3-C5 alpha-olefin homo- or copolymer (B) as carrier for additive(s) to improve the performance of a silanol condensation catalyst when cross-linking a polyethylene composition further comprising a polyethylene with cross-linkable silicon-containing groups.
    • 本发明涉及一种聚乙烯组合物,其包含:a)具有可交联的含硅基团(A)的聚乙烯; 和b)包含一种或多种添加剂的母料; 和包含C 3 -C 5α-烯烃均聚物或共聚物(B)的载体。 本发明还涉及通过在交联条件下处理根据前述权利要求中任一项的组合物而获得的交联聚乙烯组合物。 本发明还涉及以下用途:使用包含添加剂的母料; 和包含用于向具有可交联的含硅基团的聚乙烯中添加添加剂的C 3 -C 5α-烯烃均聚物或共聚物(B)的载体。 当交联聚乙烯组合物进一步包含具有可交联的含硅基团的聚乙烯时,使用C 3 -C 5α-烯烃均聚物或共聚物(B)作为添加剂的载体来改善硅烷醇缩合催化剂的性能 。